Influence of heat treatment and loading direction on compressive deformation behaviour of Ti–6Al–4V ELI fabricated by powder bed fusion additive manufacturing
Source abstract
Abstract
Abstract In this study, we have investigated the effects of heat treatment and loading direction on anisotropic compressive behaviour of additively manufactured (AM) Ti–6Al–4V ELI (extra low interstitials). AM samples were fabricated by powder bed fusion (PBF) processing, heat-treated between 800 °C and 950 °C, and compressed along two directions (i.e. parallel and perpendicular to the building direction) with a strain rate of 10−3 s−1 at room temperature. The heat treatment effectively leads to increasing ductility of as-built by decomposing the α′ phase to α and β phases. The heat-treated samples show a significantly lower yield strength than the as-built sample, which has a higher pre-existing dislocation density. As the annealing temperature increases, the yield strength decreased with a broadening of α lath thickness. Furthermore, perpendicular loaded samples have significantly higher strain hardening rate and ductility than parallel loaded samples. However, most of these anisotropic responses disappeared with indistinct morphologies. Anisotropic properties can be ascribed to the directional features of the microstructure resulting from the additive manufacturing process.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (70)
Show source-provided references
1. Titanium alloys in total joint replacement—a materials science perspective10.1016/S0142-9612(97)00146-4 ↗
2. Mechanical biocompatibilities of titanium alloys for biomedical applications10.1016/j.jmbbm.2007.07.001 ↗
3. Customised titanium implant fabricated in additive manufacturing for craniomaxillofacial surgery10.1080/17452759.2014.900857 ↗
4. Cranial reconstruction: 3D biomodel and custom-built implant created using additive manufacturing10.1016/j.jcms.2014.07.006 ↗
5. Patient-specific reconstruction with 3D modelling and DMLS additive manufacturing10.1108/13552541211218126 ↗
6. Application of additive manufacturing in customized titanium mandibular implants for patients with oral tumors
7. Effect of texture and temperature gradient on anisotropic plastic deformation of commercially pure titanium at room and low temperatures10.1016/j.matchar.2020.110834 ↗
8. Local deformation mechanisms of two-phase Ti alloy10.1016/j.msea.2015.09.016 ↗
9. Deformation induced anisotropic responses of Ti–6Al–4V alloy. Part I: Experiments10.1016/j.ijplas.2012.03.015 ↗
10. Local strain rate sensitivity of single α phase within a dual-phase Ti alloy10.1016/j.actamat.2016.01.057 ↗
11. Effects of building direction and heat treatment on the local mechanical properties of direct metal laser sintered 15-5 PH stainless steel10.1016/j.matchar.2020.110468 ↗
12. Fatigue crack growth behavior of Ti-6Al-4V alloy fabricated via laser metal deposition: effects of building orientation and heat treatment10.1016/j.jallcom.2021.159023 ↗
13. The positive effect of hot isostatic pressing on improving the anisotropies of bending and impact properties in selective laser melted Ti-6Al-4V alloy10.1016/j.msea.2016.02.023 ↗
14. Microstructure and tensile properties of selectively laser-melted and of HIPed laser-melted Ti–6Al–4V10.1016/j.msea.2013.04.099 ↗
15. Effect of heat-treatment on microstructure and mechanical properties of Ti alloys: an overview
16. Improvement of fatigue resistance and ductility of TiAl6V4 processed by selective laser melting10.1016/j.jmatprotec.2015.01.025 ↗
17. Ductility of a Ti‐6Al‐4V alloy produced by selective laser melting of prealloyed powders10.1108/13552541011083371 ↗
18. As-fabricated and heat-treated microstructures of the Ti-6Al-4V alloy processed by selective laser melting10.1007/s11661-011-0731-y ↗
19. Correlation between microstructures and mechanical properties under tensile and compression tests of heat-treated Ti-6Al–4V ELI alloy produced by additive manufacturing for biomedical applications10.1016/j.jmatprotec.2017.09.022 ↗
20. Heat treatment of Ti6Al4V produced by selective laser melting: microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
21. Microstructural evolution and microhardness of a selective-laser-melted Ti–6Al–4V alloy after post heat treatments10.1016/j.jallcom.2016.02.183 ↗
22. Anisotropic tensile behavior of Ti–6Al–4V components fabricated with directed energy deposition additive manufacturing10.1016/j.actamat.2014.12.054 ↗
23. Influence of energy density on metallurgy and properties in metal additive manufacturing10.1080/02670836.2017.1289444 ↗
24. Influence of energy density on energy demand and porosity of 316L stainless steel fabricated by selective laser melting10.1007/s40684-018-0006-9 ↗
25. An oxidation model for predicting the life of titanium alloy components in gas turbine engines10.1016/j.jallcom.2004.05.079 ↗
26. Local and global deformation behaviour in rolled pure magnesium sheets at room temperature under different strain rates10.1016/j.msea.2019.138110 ↗
27. X-ray diffraction analysis by Williamson-Hall, Halder-Wagner and size-strain plot methods of CdSe nanoparticles- a comparative study10.1016/j.matchemphys.2019.122021 ↗
28. X-ray line broadening from filed aluminium and wolfram10.1016/0001-6160(53)90006-6 ↗
29. X-ray peak profile analysis of solid-state sintered alumina doped zinc oxide ceramics by Williamson–Hall and size-strain plot methods10.1016/j.jascer.2017.02.001 ↗
30. The use of Fourier analysis in the interpretation of X-ray line broadening from cold-worked iron and molybdenum10.1107/S0365110X54001879 ↗
31. Stacking faults in face-centred cubic metals and alloys10.1080/14786435708242709 ↗
32. Correlation between dislocation-density-based strain hardening and microstructural evolution in dual phase TC6 titanium alloy10.1016/j.msea.2017.12.098 ↗
33. The role of β-titanium ligaments in the deformation of dual phase titanium alloys10.1016/j.msea.2019.01.032 ↗
34. Anisotropy in α′ martensite and compression behavior of Ti6Al4V prepared by selective laser melting10.1088/2053-1591/ab5741 ↗
35. Anisotropic response of Ti-6Al-4V alloy fabricated by 3D printing selective laser melting10.1016/j.msea.2016.11.061 ↗
36. Phase transformations during cooling in α+β titanium alloys10.1016/S0921-5093(97)00802-2 ↗
37. In-situ characterization of laser-powder interaction and cooling rates through high-speed imaging of powder bed fusion additive manufacturing10.1016/j.matdes.2017.09.044 ↗
38. Ferreira · 2012
39. An overview of the thermomechanical processing of α/β titanium alloys: current status and future research opportunities10.1007/s11661-020-05625-3 ↗
40. Ti-6Al-4V additively manufactured by selective laser melting with superior mechanical properties
41. Constitutive analysis of compressive deformation behavior of ELI-grade Ti–6Al–4V with different microstructures10.1007/s10853-011-6145-9 ↗
42. The martensitic transformation and mechanical properties of Ti6Al4V prepared via selective laser melting10.3390/ma12020321 ↗
43. Prediction of microstructure evolution for additive manufacturing of Ti-6Al-4V10.1016/j.promfg.2020.04.170 ↗
44. Quantifying the dislocation structures of additively manufactured Ti–6Al–4V alloys using X-ray diffraction line profile analysis
45. Dislocation network in additive manufactured steel breaks strength–ductility trade-off10.1016/j.mattod.2017.11.004 ↗
46. Microstructure evolution of sub-critical annealed laser deposited Ti–6Al–4V alloy10.1016/j.matdes.2011.12.016 ↗
47. Raghavan · 2016
48. Lütjering · 2007
49. The effect of microstructure on the mechanical properties of two-phase titanium alloys10.1016/S0924-0136(02)00248-0 ↗
50. Formation of α-Widmanstätten structure: effects of grain size and cooling rate on the Widmanstätten morphologies and on the mechanical properties in Ti6Al4V alloy10.1016/S0925-8388(01)01571-7 ↗
51. Deformation behavior of Ti-6Al-4V microstructures under uniaxial loading: equiaxed Vs. transformed-β microstructures10.1016/j.matchar.2020.110780 ↗
52. Tensile and creep properties improvement of Ti-6Al-4V alloy specimens produced by electron beam powder bed fusion additive manufacturing10.3390/met9111207 ↗
53. Effects of heat treatments on microstructure and properties of Ti-6Al-4V ELI alloy fabricated by electron beam melting (EBM)10.1016/j.msea.2017.01.019 ↗
54. Effect of subtransus heat treatment on the microstructure and mechanical properties of additively manufactured Ti-6Al-4V alloy10.1016/j.jallcom.2017.11.263 ↗
55. Additive manufacturing of strong and ductile Ti-6Al-4V by selective laser melting via in situ martensite decomposition10.1016/j.actamat.2014.11.028 ↗
56. As-fabricated and heat-treated microstructures of the Ti-6AI-4V alloy processed by selective laser melting10.1007/s11661-011-0731-y ↗
57. Effects of microstructure and internal defects on mechanical anisotropy and asymmetry of selective laser-melted 316L austenitic stainless steel10.1016/j.msea.2019.138152 ↗
58. Anisotropy and heterogeneity of microstructure and mechanical properties in metal additive manufacturing: a critical review10.1016/j.matdes.2017.11.021 ↗
59. Fabrication of large Ti-6Al-4V structures by direct laser deposition10.1016/j.jallcom.2014.12.234 ↗
60. Deformations of Ti-6Al-4V additive-manufacturing-induced isotropic and anisotropic columnar structures: insitu measurements and underlying mechanisms
61. Wang · 2017 · 87
62. Microstructural porosity in additive manufacturing: the formation and detection of pores in metal parts fabricated by powder bed fusion10.1002/amp2.10021 ↗
63. Effect of build geometry on the β-grain structure and texture in additive manufacture of Ti6Al4V by selective electron beam melting10.1016/j.matchar.2013.07.012 ↗
64. On the texture formation of selective laser melted Ti-6Al-4V10.1007/s11661-014-2218-0 ↗
65. The anisotropy of laser melting deposition additive manufacturing Ti–6.5Al–3.5Mo–1.5Zr–0.3Si titanium alloy10.1016/j.matdes.2014.11.001 ↗
66. The influence of process parameters and scanning strategy on the texture in Ti6A14V parts produced by selective laser melting
67. Anisotropic tensile behavior of Ti-6Al-4V components fabricated with directed energy deposition additive manufacturing10.1016/j.actamat.2014.12.054 ↗
68. The effect of loading direction on strain localisation in wire arc additively manufactured Ti–6Al–4V10.1016/j.msea.2020.139608 ↗
69. Characterizing the tensile behavior of additively manufactured Ti-6Al-4V using multiscale digital image correlation10.1016/j.msea.2018.03.091 ↗
70. Deformation and failure mechanisms of Ti–6Al–4V as built by selective laser melting10.1016/j.msea.2019.138456 ↗