Anisotropy of stress rupture properties of a Ni base single crystal superalloy at two temperatures
Source abstract
Abstract
The stress rupture properties of a single crystal superalloy in three orientations were tested under 871 degrees C/552MPa and 1010 degrees C/248MPa. The [0 0 1] orientation shows the longest life and good elongation at 871 degrees C, the [111] orientation exhibits the best elongation, while the life and elongation of [0 11] orientation are both poor at this test condition. At 10 10 degrees C, the anisotropy between [001] and [011] orientation is evidently reduced, however the [111] orientation shows the longest life at the same condition. In [0 0 1] orientation, the N type rafts are formed under two test conditions. In [111] orientation, the gamma' keep cuboidal shape under 871 degrees C/552 MPa, while rafts with direction varying with local position are formed under 10 10 degrees C/248 MPa. In [011] orientation, lots of stacking faults appears in gamma' under 871 degrees C/55 2 MPa, while many twins are formed under 1010 degrees C/248 MPa, which are both related to the activation of {111} (112) slip system. The influence of orientation and test condition on the deformation mechanisms and stress rupture properties is discussed. (C) 2007 Elsevier B.V. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High Temperature Alloys and Creep · Fatigue and fracture mechanics · Metallurgy and Material Forming
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Svetlov · Probl. Prochn. · 1987 · 19 · 51
2. Kakehi · Trans. JIM · 1999 · 40 · 15910.2320/matertrans1989.40.159 ↗
3. Caron · 1988 · 215
4. MacLachlan · Comput. Mater. Sci. · 2002 · 25 · 12910.1016/S0927-0256(02)00257-4 ↗
5. Leverant · Metall. Trans. · 1970 · 1 · 49110.1007/BF02811560 ↗
6. Sass · Acta Mater. · 1996 · 44 · 196710.1016/1359-6454(95)00315-0 ↗
7. Shah · 2000 · 295
8. Fredholm · 1984 · 211
9. Link · Mater. Sci. Eng. A · 2006 · 425 · 4710.1016/j.msea.2006.03.005 ↗
10. Feller-Kniepmeier · Acta Metall. Mater. · 1994 · 42 · 316710.1016/0956-7151(94)90415-4 ↗
11. Kuttner · Mater. Sci. Eng. · 1994 · A188 · 14710.1016/0921-5093(94)90366-2 ↗
12. Sass · 1996 · 283
13. Hopgood · Mater. Sci. Eng. · 1986 · 82 · 2710.1016/0025-5416(86)90092-3 ↗
14. Crompton · Metall. Trans. A · 1984 · 15 · 171110.1007/BF02666354 ↗
15. Sherry · Mater. Sci. Eng. · 1993 · A172 · 5110.1016/0921-5093(93)90425-E ↗
16. Chan · Acta Metall. · 1987 · 35 · 98110.1016/0001-6160(87)90177-5 ↗
17. Tanaka · Acta Metall. · 1984 · 32 · 173110.1016/0001-6160(84)90229-3 ↗
18. Epishin · Acta Mater. · 2001 · 49 · 401710.1016/S1359-6454(01)00290-7 ↗
19. Zhang · Acta Mater. · 2003 · 51 · 507310.1016/S1359-6454(03)00355-0 ↗
20. Zhang · Scr. Mater. · 2003 · 48 · 28710.1016/S1359-6462(02)00379-2 ↗
21. Zhang · Acta Mater. · 2005 · 53 · 462310.1016/j.actamat.2005.06.013 ↗
22. Knowles · Mater. Sci. Eng. A · 2002 · 328 · 22310.1016/S0921-5093(01)01688-4 ↗
23. Knowles · Mater. Sci. Eng. A · 2003 · 340 · 8810.1016/S0921-5093(02)00172-7 ↗
24. Golubovskii · Strength Mater. · 2002 · 34 · 10910.1023/A:1015365723962 ↗
25. Epishin · 2004 · 137
26. Liu · Acta Metall. Sinica · 2001 · 37 · 1233