Effects of cooling rate on microstructure, mechanical properties, and residual stress of Fe-2.1B (wt%) alloy
Source abstract
Abstract
Abstract The continuous cooling transformation (CCT) curve of an Fe-2.1B (wt%) alloy is obtained using a Gleeble 1500D thermomechanical simulator. The microstructure, mechanical properties, and residual stress of alloy specimens with various cooling rates are examined. The results reveal that the cooling rate has a great influence on the matrix microstructure of the Fe-2.1B (wt%) alloy. Pearlite is formed at the cooling rate of 0.1 K/s, pearlite and martensite are formed in the cooling rate range of 0.2–0.5 K/s, and only martensite remains in the matrix when the cooling rate exceeds 0.5 K/s. In addition, as the cooling rate increases, the dislocation density in the matrix increases, and this, in turn, leads to an increase in the volume fraction of the M23(B, C)6 phase. The precipitation of M23(B, C)6 causes the decrease in the (B + C) contents of the matrix, which, in turn, reduces the microhardness of the matrix to some extent. Meanwhile, the large residual compressive stress of the alloy increases with increasing cooling rate. The maximum residual compressive stresses induced by the cooling rates of 0.5 and 30 K/s are approximately 18% and 36%, respectively, higher than that induced by the cooling rate of 0.1 K/s. Moreover, when the cooling rate increases from 0.1 K/s to 0.5 K/s, the macrohardness and bending stress increase significantly owing to an increase in Vm/Vpr (where Vm represents volume fraction of martensite, Vpr is the volume fractions of pearlite and austenite). When the cooling rate exceeds 0.5 K/s, the macrohardness and bending stress decrease gradually because of the decrease in the (B + C) contents of the matrix and an increase in the residual stress. The critical cooling rate (0.5 K/s) may be the optimal cooling rate of Fe-B alloys.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Effects of microstructures on the abrasive wear behaviour of spheroidal cast iron10.1016/0043-1648(94)06499-7 ↗
2. Abrasive wear of locomotive diesel engines and contaminant control10.1080/10402009808983789 ↗
3. Wear and friction characteristics of a selected stainless steel10.1080/10402004.2011.606960 ↗
4. Effect of molybdenum and chromium contents in sliding wear of high-chromium white cast iron: the relationship between microstructure and wear10.1016/j.wear.2008.12.095 ↗
5. Effect of impingement angle on slurry erosion behaviour and mechanisms of 1017 steel and high-chromium white cast iron10.1016/j.wear.2006.11.018 ↗
6. Sliding wear of spray-formed high-chromium white cast iron alloys10.1016/j.wear.2005.01.021 ↗
7. Wear resistance of Ni-hard 4 and high-chromium cast iron re-evaluated10.1016/0043-1648(93)90276-R ↗
8. Heat treatment and two-body abrasion of Ni-Hard 410.1016/j.wear.2014.01.013 ↗
9. Effect of Cu on microstructure, crystallography and mechanical properties in Fe-B-C-Cu alloys10.1016/j.msea.2017.09.135 ↗
10. Effect of casting thickness on microstructure, mechanical properties and abrasion resistance of Fe-B cast alloy10.1016/j.triboint.2018.02.031 ↗
11. Microstructure and hardening behavior of Al-modified Fe-1.5 wt% B-0.4 wt% C high-speed steel during heat treatment10.1016/j.matchar.2017.08.001 ↗
12. Stability, electronic and mechanical properties of Fe2B10.1016/j.physb.2007.10.014 ↗
13. Effect of boron concentration on microstructures and properties of Fe-B-C alloy steel10.1557/jmr.2017.304 ↗
14. Investigations on microstructures and two-body abrasive wear behavior of Fe-B cast alloy10.1007/s11249-011-9900-9 ↗
15. Effect of normal load on two-body abrasive wear of an Fe-B-Cr-C based alloy with minor Cu and Ni additions10.1016/j.wear.2018.05.014 ↗
16. Effect of heat treatment on microstructure and mechanical properties of high boron white cast iron10.1016/j.msea.2010.09.092 ↗
17. Effects of mn addition on the two-body abrasive wear behavior of fe-3.0wt% B alloy10.1016/j.triboint.2016.07.008 ↗
18. Investigation on two-body abrasive wear behavior and mechanism of Fe–3.0 wt% B cast alloy with different chromium content10.1016/j.wear.2016.04.029 ↗
19. Effects of cooling rate on microstructure of Fe-Cr-B alloy
20. Effect of quenching cooling ways on microstructure and high temperature wear performance of high boron medium carbon alloy
21. Continuous cooling transformation behavior in the weld coarse grained heat affected zone and mechanical properties of Nb-microalloyed and HY85 steels10.1016/j.matdes.2015.10.071 ↗
22. Continuous cooling transformation behaviour and bainite formation kinetics of new bainitic steel
23. Phase transformation behavior and kinetics of high Nb–TiAl alloy during continuous cooling10.1016/j.jallcom.2016.01.205 ↗
24. The determining impact of coiling temperature on the microstructure and mechanical properties of a titanium-niobium ultrahigh strength microalloyed steel: Competing effects of precipitation and bainite10.1016/j.msea.2016.04.007 ↗
25. Hard iron boride (Fe 2 B) on 99.97 wt% pure iron10.1016/j.vacuum.2006.01.022 ↗
26. Valence electron structure of Fe2B phase and its eigen-brittleness
27. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
28. Effect of boron concentration on microstructure and properties of high-boron low-carbon ferro-matrix alloy
29. Effect of chromium concentration on microstructure and properties of Fe–3.5B alloy10.1016/j.msea.2010.07.066 ↗
30. First principles study on the structural properties and electronic structure of X2B (X=Cr, Mn, Fe, Co, Ni, Mo and W) compounds10.1016/j.commatsci.2008.07.035 ↗
31. The elasticity, bond hardness and thermodynamic properties of X2B (X=Cr, Mn, Fe, Co, Ni, Mo, W) investigated by DFT theory10.1016/j.physb.2009.11.064 ↗
32. The effect of copper on passivity and corrosion behaviour of ferritic and ferritic–austenitic stainless steels10.1016/S0921-5093(99)00530-4 ↗
33. Microstructure and crystallography of borides and secondary precipitation in 18 wt.% Cr–4 wt.% Ni–1 wt.% Mo–3.5 wt.% B–0.27 wt.% C steel10.1016/j.actamat.2011.11.004 ↗
34. Effect of orientation and lamellar spacing of Fe2B on interfaces and corrosion behavior of Fe-B alloy in hot-dip galvanization10.1016/j.actamat.2016.06.016 ↗
35. The effect of the addition of alloying elements on carbide precipitation and mechanical properties in 5% chromium martensitic steels10.1016/j.actamat.2007.05.004 ↗
36. On the contribution of carbides and micrograin boundaries to the creep strength of tempered martensite ferritic steels10.1016/j.actamat.2006.08.046 ↗
37. Effect of carbide distribution on the fracture toughness in the transition temperature region of an SA 508 steel10.1016/S1359-6454(02)00313-0 ↗
38. Orientation gradients and geometrically necessary dislocations in ultrafine grained dual-phase steels studied by 2D and 3D EBSD10.1016/j.msea.2010.01.004 ↗
39. Investigation of zeolite frameworks by vibrational properties. 2. The double-six-ring in group 4 zeolites10.1021/j100488a015 ↗
40. Numerical analysis of cooling rate dependence on dislocation density in multicrystalline silicon for solar cells10.1016/j.jcrysgro.2010.11.009 ↗
41. Influence of quenching cooling rate on residual stress and tensile properties of 2A14 aluminum alloy forgings10.1016/j.msea.2016.08.017 ↗
42. Investigations on microstructure, mechanical properties and abrasion resistance of 4wt%Cr-2wt%Mn-2wt%Cu-Fe-B alloy10.1016/j.matchar.2018.01.038 ↗
43. Effects of chromium on the morphology and mechanical properties of Fe 2 B intermetallic in Fe-3.0B alloy10.1007/s10853-017-1936-2 ↗