Characterization of fatigue properties of powder metallurgy titanium alloy
Source abstract
Abstract
Abstract The fatigue characteristics of powder metallurgy (P/M) Ti6Al4V (wt%) alloys prepared by powder sintering and hot rolling were studied under tension–tension loading conditions at R =0.1 and 25 Hz in air, where R = σ min / σ max ( σ min and σ max are the applied minimum and maximum stresses, respectively). The results show that for the as-sintered Ti6Al4V alloy the fatigue limit is about 325 MPa, and the fatigue cracks initiate from the residual pores open to the surface of the gauge area and propagate along the α/β interfaces. Hot rolling markedly enhances the fatigue properties, and the fatigue limit increases to about 430 MPa. The reducing of porosity and refining of grain size through hot rolling are the dominant mechanisms for the improvement of fatigue properties. In addition, the microstructure of α/β interfaces//RD and the texture of α//RD formed during hot rolling act as barriers for the fatigue crack propagation, which partly attributes to the improvement of the fatigue properties.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Powder Metallurgy Techniques and Materials · Titanium Alloys Microstructure and Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. Plastic deformation and fracture behavior of Ti–6Al–4V alloy loaded with high strain rate under various temperatures10.1016/S0921-5093(97)00471-1 ↗
2. Effect of heat treatment on mechanical properties of Ti–6Al–4V ELI alloy10.1016/j.msea.2008.11.018 ↗
3. Correlation of microstructure and high temperature oxidation resistance of plasma sprayed NiCrAl, NiCrAlY, and TiAlO composite coatings on Ti–6Al–4V10.1007/BF03027500 ↗
4. Boyer · 1994
5. Titanium in the family automobile: the cost challenge10.1007/s11837-004-0144-0 ↗
6. Titanium for automotive applications: challenges and opportunities in materials and processing10.1007/s11837-012-0310-8 ↗
7. Effect of density and pore morphology on fatigue properties of sintered Ti–6Al–4V10.1016/j.ijfatigue.2013.05.015 ↗
8. Variability in room temperature fatigue life of alpha+beta processed Ti–6Al–4V10.1016/j.ijfatigue.2009.01.005 ↗
9. Slip and fatigue crack formation processes in an α/β titanium alloy in relation to crystallographic texture on different scales10.1016/j.actamat.2008.04.036 ↗
10. The effect of microstructure on the mechanical properties of TC4 titanium alloys10.1016/j.msea.2012.11.033 ↗
11. Microstructure and fatigue crack growth mechanisms in high temperature titanium alloys10.1016/j.ijfatigue.2010.02.001 ↗
12. Effect of microstexture on fatigue cracking in Ti–6Al–4V10.1016/j.actamat.2007.06.034 ↗
13. Recent advances in the deformation processing of titanium alloys10.1361/105994903322692466 ↗
14. Thermomechanical characterization of P/M Ti–Fe–Mo–Y alloy with a fine lamellar microstructure10.1016/j.msea.2010.12.055 ↗
15. Mechanism of fatigue crack initiation and propagation in the very high cycle fatigue regime of high-strength steels10.1016/j.scriptamat.2012.07.049 ↗
16. Effect of microstructure on ultra-high cycle fatigue behavior of Ti–6Al–4V10.1016/j.msea.2007.04.062 ↗
17. Effect of residual surface stress on the fatigue behavior of a low-alloy powder metallurgy steel10.1016/j.ijfatigue.2007.01.008 ↗
18. Improvements in the fatigue strength of Ti6Al4V through microstructure control10.1007/BF00570387 ↗
19. High-cycle fatigue of nickel-base superalloy René 104: interaction of microstructurally small cracks with grain boundaries of known character10.1016/j.actamat.2007.01.033 ↗
20. Fatigue behavior of ultrafine-grained Ti–6Al–4V ‘ELI’ alloy for medical applications10.1016/j.msea.2008.04.082 ↗
21. Influence of crystallographic orientation upon microscopic indentation shape on pure titanium10.2472/jsms.57.249 ↗
22. The effect of grain orientation on fracture morphology during high-cycle fatigue of Ti–6Al–4V10.1016/j.actamat.2009.04.018 ↗
23. The role of microtexture on the faceted fracture morphology in Ti–6Al–4V subjected to high-cycle fatigue10.1016/j.actamat.2010.03.036 ↗