journal article·2017-08

Microstructure – Toughness relationships in sub-zero treated and tempered Vanadis 6 steel compared to conventional treatment

Jana Ptačinová, Viktória Sedlická, Mária Hudáková, Ivo Dlouhý, Peter Jurči

Publisher page

Abstract

Abstract The influence of sub-zero treatment and tempering on the microstructure, flexural strength, and fracture toughness of Cr-V ledeburitic steel was examined with reference to the same material processed without the sub-zero period. The experimental results lead to the following findings: (i) Sub-zero treatment induces a considerable reduction of the amount of retained austenite, refinement of newly formed martensite, and increase in population density of small globular carbides. (ii) The hardness is improved by the sub-zero treatment in the prior-to-tempering state as well as in the state after low-temperature tempering; after high-temperature tempering, the situation is changed in favour of conventionally quenched specimens, whereas the secondary hardening peak disappears in sub-zero treated steel. This is due to combined effect of the population density decrease of small globular carbides, accelerated decomposition rate of retained austenite, coarsening of cementitic precipitates, and retardation of precipitation of stable M 7 C 3 carbide. (iii) There is almost no effect of sub-zero treatment on the flexural strength in the low-temperature tempering range but this property is improved after tempering into the secondary hardening range. Sub-zero treatment causes a worsening of fracture toughness after low-temperature tempering but a slight improvement after tempering in the secondary hardening temperature range.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal Alloys Wear and Properties · Advanced materials and composites · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (71)

Show source-provided references
1. Optimising nano-carbide precipitation in tool steels10.1016/j.msea.2006.01.162 ↗
2. Cr-V Ledeburitic cold-work tool steels
3. Fracture of hot formed ledeburitic chromium steels10.1016/S0013-7944(97)00118-5 ↗
4. Using chevron notched specimens for determining fracture toughness of bearing steels
5. Influence of sub-zero treatments on fracture toughness of AISI D2 steel10.1016/j.msea.2010.09.057 ↗
6. The effect of sub-zero treatment on microstructure, fracture toughness, and wear resistance of Vanadis 6 tool steel10.1016/j.msea.2015.11.078 ↗
7. Sintering behaviour and fracture toughness characterization of D2 matrix tool steel, comparison with wrought and PM D210.1016/S1359-6462(01)01253-2 ↗
8. Cryogenic treatment of tool steels
9. Deep cryogenic treatment of a D2 cold-work tool steel
10. Effect of retained austenite on the fracture toughness of tempered tool steel
11. Fracture toughness of a high carbon and high silicon steel10.1016/S0921-5093(00)01272-7 ↗
12. Evaluation of structural isotropy of Cr-V ledeburitic steel made by powder metallurgy of rapidly solidified particles
13. Microstructure and hardness of sub-zero treated and no tempered P/M Vanadis 6 ledeburitic tool steel10.1016/j.vacuum.2014.10.004 ↗
14. Evaluation of the microstructural changes in Cr-V ledeburitic tool steel depending on the austenitization temperature
15. ISO, 12137. Metallic Materials – Determination of Plane Strain Fracture Toughness, 2010.
16. Study of phase transformations in Cr-V tool steel
17. ASTM E975-13 · 2004 · 3.01
18. Sub-zero treatment of cold work tool steels – metallurgical background and the effect on microstructure and properties10.3139/105.110301 ↗
19. Low-temperature martensitic transformation and deep cryogenic treatment of a tool steel10.1016/j.msea.2010.07.056 ↗
20. Sub-zero treatments of AISI D2 steel: Part I. Microstructure and hardness10.1016/j.msea.2009.10.070 ↗
21. Structure-property correlation of sub-zero treated AISI D2 steel10.1016/j.msea.2012.01.130 ↗
22. Restaustenit in ledeburitischen Chromstählen und seine Umwandlung durch Kaltumformen, Tiefkühlen und Anlassen10.1515/htm-1974-290402 ↗
23. On the enhancement of wear resistance of tool steels by cryogenic treatment10.1080/09500830802380788 ↗
24. Low-temperature martensitic transformation in tool steels in relation to their deep cryogenic treatment10.1016/j.actamat.2012.11.045 ↗
25. Isothermal martensite formation at sub-zero temperatures10.1520/JAI103459 ↗
26. Investigating the effect of holding duration on the microstructure of 1.2080 tool steel during the deep cryogenic treatment10.1016/j.vacuum.2012.02.013 ↗
27. Effects of applying an external magnetic field during the deep cryogenic heat treatment on the corrosion resistance and wear behaviour of 1.2080 tool steel10.1016/j.matdes.2012.03.045 ↗
28. Investigating the effect of electric current flow on the wear behaviour of 1.2080 tool steel during the deep cryogenic heat treatment10.1016/j.matdes.2012.08.012 ↗
29. Investigating the effect of ball milling during the deep cryogenic heat treatment of the 1.2080 tool steel10.1016/j.vacuum.2012.09.023 ↗
30. Investigating the effect of the quench environment on the final microstructure and wear behaviour of 1.2080 tool steel after deep cryogenic heat treatment10.1016/j.matdes.2012.08.006 ↗
31. Effect of simultaneous magnetic field and deep cryogenic heat treatment on the microstructure of 1.2080 tool steel10.1016/j.matdes.2011.09.015 ↗
32. Long-term sub-zero treatment of P/M Vanadis 6 ledeburitic tool steel – a preliminary study
33. Evolution of compressive strains in retained austenite during sub-zero Celsius martensite formation and tempering10.1016/j.actamat.2013.11.007 ↗
34. On the stabilization of retained austenite: mechanism and kinetics10.1016/0921-5107(95)03017-4 ↗
35. Influence of deep cryogenic treatment on the thermal decomposition of Fe-C martensite10.1007/s10853-014-8527-2 ↗
36. Strength of initially virgin martensite at –196 °C after aging and tempering
37. Carbide precipitation during tempering of a tool steel subjected to deep cryogenic treatment10.1007/s11661-014-2202-8 ↗
38. Role of eta-carbide precipitation′s in the wear resistance improvements of Fe-12Cr-Mo-V-1.4C tool steel by cryogenic treatment10.2355/isijinternational.34.205 ↗
39. The source of martensite strength
40. Effects of the aging of martensite on its deformation characteristics and on fracture in Fe–Ni–Si–C steel
41. Experimental verification of segregation of carbon and precipitation of carbides due to deep cryogenic treatment for tool steel by internal friction method
42. Influence of deep cryogenic treatment on microstructure and evaluation by internal friction of a tool steel10.1016/j.cryogenics.2010.09.002 ↗
43. Influence of deep cryogenic treatment on internal friction behaviour in the process of tempering
44. M. Villa, K. Pantleon, M.A.J. Somers, Enhanced carbide precipitation during tempering of sub-zero Celsius treated AISI 52100 bearing steel, in: Proceedings of the Heat Treat & Surface Engineering Conference Exposition 2013, Chennai, India, May 16–18, 2013.
45. Saturation of the Cr-V ledeburitic steel with nitrogen
46. Fracture toughness of carbides in tool steels evaluated by nanoindentation10.1016/j.actamat.2007.03.028 ↗
47. A thermodynamic evaluation of the Fe-C-Cr system10.1007/BF02649276 ↗
48. Beitrag zum Tiefkuehlen von Schnellarbeitsstaehlen10.1515/htm-1992-470510 ↗
49. Carbide reactions (M3C→M7C3→M23C6→M6C) during tempering of rapidly solidified high carbon Cr-W and Cr-Mo steels10.1007/BF02661203 ↗
50. In situ transformation of cementite to M7C3 and internal defects of M7C3 in high carbon-chromium steel by tempering10.2320/matertrans1960.19.11 ↗
51. Deep cryogenic treatment of tool steels – a review
52. Effects of cryogenic treatment on wear behaviour of D6 tool steel10.1016/j.matdes.2008.11.016 ↗
53. Chemical composition and morphology of M7C3 eutectic carbide in high chromium white cast iron alloyed with vanadium10.2355/isijinternational.52.2200 ↗
54. Sub-zero treatments of AISI D2 steel: Part II. Wear behaviour10.1016/j.msea.2009.10.071 ↗
55. Hardness, toughness and cracking systems of primary (Cr, Fe)23C6 and (Cr, Fe)7C3 carbides in high-carbon Cr-based alloys by indentation10.1016/j.msea.2010.04.073 ↗
56. Influence of varied cryotreatment on the wear behaviour of AISI D2 steel10.1016/j.wear.2008.07.001 ↗
57. Influence of temperature of sub-zero treatments on the wear behaviour of die steel10.1016/j.wear.2008.11.029 ↗
58. Effect of deep cryogenic treatment on the carbide precipitation and tribological behavior of D2 steel10.1080/10426910701235934 ↗
59. Investigating the effect of as-quenched vacancies in the final microstructure of 1.2080 tool steel during the deep cryogenic heat treatment10.1016/j.matlet.2012.11.081 ↗
60. Effects of austenitizing time on wear behaviour of D6 tool steel after deep cryogenic treatment10.1016/S1006-706X(10)60023-4 ↗
61. Fracture characteristics of the Cr-V ledeburitic steel Vanadis 6
62. P. Jurči, M. Kusý, M. Dománková, L. Čaplovič, J. Sobotová, P. Salabová, O. Prikner, D. Jenko, Tempering response of sub-zero processed Cr-V ledeburitic steel Vanadis 6, in: TANGER s.r.o. (Ed.), in: Proceedings of the 22nd International Conference on Metallurgy and Materials (METAL) Brno, Czech Republic, 15–17 May 2013, pp. 651–656.
63. Hall-Petch relation in nanocrystalline solids10.1016/0956-716X(91)90256-Z ↗
64. Optimization of the duration of cryogenic processing to maximize wear resistance of AISI D2 steel10.1016/j.cryogenics.2009.01.002 ↗
65. Acoustic emission methodology to evaluate the fracture toughness in heat treated AISI D2 tool steel10.1007/s11665-011-0119-6 ↗
66. J.R. Shant, R.K. Goyal, G. Chauhan, T.S. Khatayat, Failure investigation of tools used in LSAN pipe expansion process, in: H. Leitner (Ed.), Proceedings of the 9th International Tooling Conference, Leoben, Austria, 11–14 Sept. 2012, Montanuniversitat Leoben, pp. 163–171.
67. Optimizing fracture toughness and abrasion resistance in white cast irons10.1007/BF02670698 ↗
68. The behaviour of the carbides of ledeburitic AISI D2 tool steel during multiple hot deformation cycles10.1016/j.matchar.2013.06.008 ↗
69. Microstructural effects on the fatigue crack nucleation in cold work tool steels10.1016/j.proeng.2010.03.191 ↗
70. Fractographic evaluation of gigacycle fatigue crack nucleation and propagation of a high Cr alloyed cold work tool steel10.1016/j.ijfatigue.2008.05.013 ↗
71. Fatigue of cold-work tool steels: effect of heat treatment and carbide morphology on fatigue crack formation, life, and fracture surface observations10.1007/s11661-004-0303-5 ↗