Effect of temperature on microstructure and texture evolutions during uniaxial compression of commercially pure titanium
Source abstract
Abstract
Abstract Commercially pure (CP) titanium samples were subjected to uniaxial compression of 3%, 10%, 20%, 30%, 40% and 50% reductions at room temperature (298 K), 673 K and 873 K respectively. {10 1 ¯ 2} type tensile twins were observed during the deformation at temperatures of 298 K and 673 K only. Volume fraction of these twins was increased up to 20% reduction beyond which it was decreased on further increasing the % reduction. The non-basal orientations had higher Taylor factor values and were prone to twinning. On the other hand near-basal orientations were observed to be the possible twinning products. It was further observed that the volume fraction of dynamically recrystallized grains was increased with increase in % reductions at high temperatures. The initial non-basal texture of the samples was found to be transformed to dominant basal texture after deformation irrespective of the temperature of deformation. An abrupt transition of texture from non-basal to basal at a true strain of 0.22 of the samples deformed at a temperature of 873 K was observed and this may be attributed to the nucleation and growth of tensile twinning.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and mechanical properties · Titanium Alloys Microstructure and Properties · Magnesium Alloys: Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. An overview on the use of titanium in the aerospace industry10.1016/0921-5093(96)10233-1 ↗
2. An overview on the development of titanium alloys for non-aerospace application in Japan10.1016/0921-5093(96)10241-0 ↗
3. 1984
4. 2015
5. Misorientations induced by deformation twinning in titanium10.1107/S0021889810008228 ↗
6. Effect of twinning on microstructure and texture evolutions of pure Ti during dynamic plastic deformation10.1016/j.msea.2012.11.097 ↗
7. Determination of near-coincident cells for hexagonal crystals, Related DSC Lattices10.1107/S0567739481000466 ↗
8. Role of twinning in texture development and in plastic deformation of hexagonal materials10.1155/TSM.7.265 ↗
9. Bishoyi · Mater. Sci. Eng. A · 2017 · 703 · 39910.1016/j.msea.2017.07.081 ↗
10. Effect of deformation twinning on microstructure and texture evolution during cold rolling of CP-titanium10.1016/j.msea.2005.03.019 ↗
11. Texture and microstructure evolution of commercially pure titanium during hot rolling: role of strain-paths10.1016/j.matdes.2015.11.073 ↗
12. Microstructure and microtexture of highly cold-rolled commercially pure titanium10.1007/s10853-006-1302-2 ↗
13. Microstructural and textural evolution of pure titanium during differential speed rolling and subsequent annealing10.1007/s10853-014-8019-4 ↗
14. Texture evolution of commercial pure Ti during cold rolling and recrystallization annealing10.1007/s12613-012-0591-5 ↗
15. Effect of twinning on microstructure and texture evolutions of pure Ti during dynamic plastic deformation10.1016/j.msea.2012.11.097 ↗
16. Microstructure evolution of commercial pure titanium during equal channel angular pressing10.1016/j.msea.2009.09.005 ↗
17. Texture evolution in commercially pure titanium after warm equal channel angular extrusion10.1016/j.actamat.2010.10.045 ↗
18. Microstructural and textural evolution of high-purity titanium under dynamic loading10.1016/j.matdes.2017.04.042 ↗
19. Microstructure and texture evolution of commercial pure titanium deformed at elevated temperatures10.1016/j.msea.2009.01.065 ↗
20. Hot rolling textures in Ti10.1515/ijmr-1990-810411 ↗
21. Role of deformation twin on texture evolution in cold rolled commercial-purity Ti10.1557/JMR.2008.0354 ↗
22. Texture formation and transition in cold rolled titanium10.1016/0025-5416(88)90245-5 ↗
23. Improvement in mechanical properties of commercially pure Ti through reverse rolling10.1080/09500839.2017.1341647 ↗
24. Effect of orientation and temperature on the mechanical properties of commercially pure titanium
25. Effect of pre-annealing strains on annealing texture developments in commercially pure (CP) titanium10.1080/14786435.2015.1020905 ↗
26. Microstructure evolution of titanium after tensile test10.1016/j.msea.2015.12.041 ↗
27. Orientation dependent mechanical properties of commercially pure (cp) titanium10.1016/j.matchar.2014.10.011 ↗
28. Deformation twinning in Zircaloy 210.1179/174328408X393396 ↗
29. Growth mechanism of extension twin variants during annealing of pure magnesium: an 'ex situ' electron back scattered diffraction investigation10.1016/j.matchar.2017.02.008 ↗
30. Hatherly · 1990
31. An 'ex situ' electron back scattered diffraction study of nucleation and grain growth in pure magnesium10.1016/j.matdes.2016.11.091 ↗
32. A constitutive model of twin nucleation, propagation and growth in magnesium crystals10.1016/j.msea.2014.11.096 ↗
33. Formability and metallurgical structure
34. Physics and phenomenology of strain hardening: the FCC case10.1016/S0079-6425(02)00003-8 ↗
35. Constitutive relation based on Taylor slip analysis to replicate work-hardening evolution10.1016/j.actamat.2010.09.065 ↗