journal article·2007-03Open access

Formation of ductile ultrafine eutectic structure in Ti–Fe–Sn alloy

J. Das, K.B. Kim, W. Xu, W. Löser, J. Eckert

Abstract

Abstract A Ti67.79Fe28.36Sn3.85 (at.%) alloy has been prepared through arc-melting and solidification at a cooling rate of 40–10 K/s. The as-prepared microstructure exhibits a two-phase ultrafine eutectic consisting of FeTi (B2) and β-Ti (A2) phases. The mechanical properties (maximum strength, σmax = 1939 MPa; strain to fracture, ɛf = 13.5%) are considerably improved if compared with the model Ti70.5Fe29.5 eutectic alloy (σmax = 1733 MPa, ɛf = 3.4%). The improvement of plastic deformability is assessed in terms of a detailed investigation of the microstructure and fractographic studies. The presence of Sn is believed to boost the ease of slip transfer across the interface between the A2/B2 phases due a higher lattice mismatch between the structures.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · Microstructure and mechanical properties · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. Koch · J. Metast. Nanocryst. Mater. · 2003 · 18 · 910.4028/www.scientific.net/JMNM.18.9 ↗
2. Bruck · Scripta Metall. Mater. · 1994 · 30 · 42910.1016/0956-716X(94)90598-3 ↗
3. Schroers · Phys. Rev. Lett. · 2004 · 93 · 25550610.1103/PhysRevLett.93.255506 ↗
4. Das · Phys. Rev. Lett. · 2005 · 94 · 20550110.1103/PhysRevLett.94.205501 ↗
5. Hays · Phys. Rev. Lett. · 2000 · 84 · 290110.1103/PhysRevLett.84.2901 ↗
6. Kühn · Appl. Phys. Lett. · 2002 · 80 · 247810.1063/1.1467707 ↗
7. Wang · Nature · 2002 · 419 · 91210.1038/nature01133 ↗
8. Das · Appl. Phys. Lett. · 2003 · 82 · 469010.1063/1.1587254 ↗
9. Das · Scripta Mater. · 2003 · 49 · 118910.1016/j.scriptamat.2003.08.015 ↗
10. He · Nat. Mater. · 2003 · 2 · 3310.1038/nmat792 ↗
11. He · Acta Mater. · 2003 · 51 · 522310.1016/S1359-6454(03)00386-0 ↗
12. Louzguine · Acta Mater. · 2005 · 53 · 200910.1016/j.actamat.2005.01.012 ↗
13. Louzguine · J. Mater. Res. · 2004 · 19 · 360010.1557/JMR.2004.0462 ↗
14. Kurz · 1998
15. Lütjering · 2003
16. Brandes · 1992
17. Zhang · Mater. Trans. JIM · 1998 · 39 · 100110.2320/matertrans1989.39.1001 ↗
18. Massalski · 1992
19. Young · 1993
20. Das · Appl. Phys. Lett. · 2005 · 87 · 16190710.1063/1.2105998 ↗
21. Misra · Intermetallics · 2000 · 8 · 102510.1016/S0966-9795(00)00079-0 ↗