journal article·2004-10

An investigation of the embrittlement in X20CrMoV12.1 power plant steel after long-term service exposure at elevated temperature

Zheng-Fei Hu, Zhen-Guo Yang

Publisher page

Abstract

Abstract X20CrMoV12.1 alloy steel used as main steam pipes in power plants exhibits embrittlement at room temperature after long-term service exposure at 550 °C and the embrittlement can be partly removed by retempering. Microstructural observation shows that the carbides in the exposed pipe coarsened heavily with enriching alloying elements of Cr and Mo from the matrix during long-term service exposure, so the coarsened carbides reduce both precipitation and solid solution strengthening mechanisms. The degradation of the material is mainly related to carbide coarsening. AES investigations show that the embrittlement is mostly due to the segregation of phosphorus to the prior austenite grain boundaries, and plenty of coarsened carbides residing on the grain boundaries result in this embrittlement tendency as well.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High Temperature Alloys and Creep · Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (10)

Show source-provided references
1. K. Borggreen, P.B. Mortensen, Long-term Properties of Fracture of X20CrMoV12.1, The Danish Corrosion Center, November 1989.
2. Hahn · VGB Kraftwerks Technik · 2000 · 11 · 85
3. Murphy · JISI · 1968 · 206 · 266
4. Vodarek · Scripta Mat. · 1998 · 38 · 10110.1016/S1359-6462(97)00440-5 ↗
5. P.J. Ennis, A. Zielinska-Lipiec, A. Filemonowicz, Quantitative comparison of the microstructure of high chromium steels for advanced power stations. In: A. Strang, J. Cawley, G.W. Greenwood (Eds.), Microstructure of High Temperature Materials, No.2, The Institute of Materials, 1998, p. 135.
6. Eggeler · Acta Metall. · 1989 · 37 · 322510.1016/0001-6160(89)90194-6 ↗
7. P. Battaini, D. Dangelo, G. Marino, J. Hald, Interparticle distance evolution on steam pipes’ 12% Cr steel during power plants’ service time. In: B. Wilshire, R.W. Evans (Eds.), Proceedings of the 4th International Conference on Creep and Fracture of Engineering Materials and Structures, The Institute of Metals, 1–6 April 1990, p. 1039.
8. Zheng-Fei · J. Mater. Eng. Perf. · 2003 · 12 · 10610.1361/105994903770343556 ↗
9. A. Strang, V. Vodarek, Microstructural stability of creep resistant martensitic 12% Cr steels. In: A. Strang, J. Cawley, G.W. Greenwood (Eds.), Microstructure of High Temperature Materials, No. 2, The Institute of Materials, 1998, p. 117.
10. Viswanathan · Metall. Trans. A · 1971 · 2 · 80910.1007/BF02662740 ↗