journal article·2015-01

Lamellar microstructure alignment and fracture toughness in Ti–47Al alloy by electromagnetic confinement and directional solidification

Yujun Du, Jun Shen, Yilong Xiong, Zhao Shang, Lei Wang, Hengzhi Fu

Publisher page

Abstract

Abstract Large-scale Ti–47Al sample without contamination is shaped by electromagnetic confinement and directional solidification. Controlled by a Ti–43Al–3Si seed, numerous columnar grains grow directionally in transition region and the lamellar microstructure within those grains is aligned parallel to the growth direction. Because the solid/liquid interface is convex towards the liquid and its h / r value is 0.25, one of the columnar grains in sample center grows divergently and then a near single (NS) crystal forms with crystal growth. Fracture toughness of the NS crystal with the desired lamellae is detected and the value is measured 34.7 MPa m 1/2 . The crack propagation path is checked after the fracture toughness testing and a schematic model is used to illustrate the relevant toughness mechanism.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · Solidification and crystal growth phenomena · Metallic Glasses and Amorphous Alloys

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Yamaguchi · Acta Mater. · 2000 · 48 · 30710.1016/S1359-6454(99)00301-8 ↗
2. Wu · Intermetallics · 2006 · 14 · 111410.1016/j.intermet.2005.10.019 ↗
3. Lin · Intermetallics · 2011 · 19 · 13110.1016/j.intermet.2010.08.029 ↗
4. Ding · Trans. Nonferr. Met. Soc. · 2012 · 22 · 74710.1016/S1003-6326(11)61240-5 ↗
5. Lee · Acta Mater. · 2000 · 48 · 322110.1016/S1359-6454(00)00123-3 ↗
6. Takeyama · Mater. Sci. Eng. A · 2002 · 329 · 710.1016/S0921-5093(01)01493-9 ↗
7. Coriell · J. Cryst. Growth · 1977 · 42 · 46610.1016/0022-0248(77)90232-9 ↗
8. Lan · J. Cryst. Growth · 1992 · 119 · 28110.1016/0022-0248(92)90680-H ↗
9. Kim · Intermetallics · 2007 · 15 · 97610.1016/j.intermet.2006.12.004 ↗
10. Shen · J. Mater. Process. Technol. · 2000 · 102 · 10910.1016/S0924-0136(00)00479-9 ↗
11. Fu · J. Mater. Process. Technol. · 2004 · 148 · 2510.1016/j.jmatprotec.2003.11.039 ↗
12. Du · JOM · 2014 · 66 · 191410.1007/s11837-014-1051-7 ↗
13. Zheng · Mater. Rev. · 2005 · 19 · 118
14. Kim · Mater. Sci. Eng. A · 1997 · 239 · 57010.1016/S0921-5093(97)00632-1 ↗
15. Li · Acta Metall. Sin. (Engl. Lett.) · 2009 · 45 · 1479
16. Yamaguchi · Intermetallics · 2000 · 8 · 51110.1016/S0966-9795(99)00157-0 ↗
17. Yokoshima · Acta Mater. · 1996 · 44 · 87310.1016/1359-6454(95)00255-3 ↗
18. Kim · Intermetallics · 2000 · 8 · 39910.1016/S0966-9795(99)00122-3 ↗
19. Chen · Intermetallics · 2011 · 19 · 140510.1016/j.intermet.2011.05.006 ↗
20. Oehring · Mater. Sci. Forum · 2007 · 539–543 · 147510.4028/www.scientific.net/MSF.539-543.1475 ↗
21. Su · Intermetallics · 2005 · 13 · 26710.1016/j.intermet.2004.07.010 ↗
22. Johnson · Acta Mater. · 1998 · 46 · 652910.1016/S1359-6454(98)00310-3 ↗
23. Johnson · Acta Mater. · 2006 · 54 · 107710.1016/j.actamat.2005.10.040 ↗
24. Kitamura · J. Cryst. Growth · 1982 · 57 · 47510.1016/0022-0248(82)90061-6 ↗
25. Abdur Razzaque Sarker · J. Cryst. Growth · 2010 · 312 · 200810.1016/j.jcrysgro.2010.03.028 ↗
26. Song · J. Mater. Process. Technol. · 2006 · 180 · 17910.1016/j.jmatprotec.2006.06.002 ↗
27. Kimura · J. Cryst. Growth · 1983 · 65 · 54310.1016/0022-0248(83)90100-8 ↗
28. Chan · Mater. Sci. Eng. A · 1993 · 167 · 5710.1016/0921-5093(93)90337-E ↗
29. Zambaldi · Acta Mater. · 2010 · 58 · 351610.1016/j.actamat.2010.02.025 ↗