journal article·2016-04

Microstructure and mechanical properties of Al-Fe-V-Si aluminum alloy produced by electron beam melting

Shaobo Sun, Lijing Zheng, Hui Peng, Hu Zhang

Publisher page

Abstract

Abstract Atomized, pre-alloyed Al-8.5Fe-1.3V-1.7Si (wt%) powder was used to fabricate solid components by electron beam melting (EBM). The residual porosity, chemical composition, microstructure and mechanical properties have been investigated. Results show that the relative density of as-built alloy under the optimized processing parameters was 98.2%. Compare to the initial alloy powder, the EBM parts demonstrated a restricted aluminum loss (~1 wt%) and a quite low oxygen pickup. The microstructure of the deposits was non-uniform. The fusion zone and heat affected zone exhibited a large number of fine spherical Al12(Fe,V)3Si particles (30–110 nm) distributed uniformly in the α-Al matrix. Some coarser Fe- and V-riched rectangle-like AlmFe phase (m=4.0–4.4) with 100–400 nm in size was precipitated in the melting boundary zone. The microhardness of the EBM samples was 153 HV in average. The average ultimate tensile strength (UTS) reached 438 MPa with the elongation of 12%. A ductile fracture mode of the tensile specimens was also revealed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High-Temperature Coating Behaviors · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Dispersion strengthened Al-Fe-V-Si alloys10.1016/0036-9748(86)90456-4 ↗
2. Skinner · 1988
3. Microstructure and properties of rapidly solidified powder metallurgy Al-Fe-Mo-Si alloys10.1016/S1359-6462(03)00483-4 ↗
4. An investigation on the microstructure and mechanical properties of spray-deposited Al-8.5Fe-1.1V-1.9Si alloy10.1016/j.jmatprotec.2006.10.033 ↗
5. Texture stability of a rapidly solidified dispersion strengthened Al-Fe-V-Si material10.1016/S1359-6462(98)00039-6 ↗
6. Influence of silicon content on phase development in Al-Fe-V-Si alloys10.1016/j.msea.2009.02.026 ↗
7. Preparation of Al-Fe-V-Si alloy by spray co-deposition with added its over-sprayed powders10.1016/j.jallcom.2006.08.233 ↗
8. Tensile deformation behavior of spray-deposited FVS0812 heat-resistant aluminum alloy sheet at elevated temperatures10.1016/j.matchar.2006.06.024 ↗
9. Effects of processing on microstructure and mechanical properties of a titanium alloy (Ti–6Al–4V) fabricated using electron beam melting (EBM), Part 1: distance from build plate and part size10.1016/j.msea.2013.02.064 ↗
10. Novel powder/solid composites possessing low young's modulus and tunable energy absorption capacity, fabricated by electron beam melting, for biomedical applications10.1016/j.jallcom.2015.03.141 ↗
11. Graded microstructure and mechanical properties of additive manufactured Ti–6Al–4V via electron beam melting10.1016/j.actamat.2015.06.036 ↗
12. Novel microstructural growth in the surface of Inconel 625 by the addition of SiC under electron beam melting10.1016/j.apsusc.2011.02.067 ↗
13. Process development for the manufacturing of 99.94% pure copper via selective electron beam melting10.1016/j.matlet.2014.12.105 ↗
14. Microstructures and mechanical properties of dispersion-strengthened high-temperature AL-8.5Fe-1.2V-1.7Si alloys produced by atomized melt deposition process10.1007/BF02656507 ↗
15. Microstructure and mechanical properties of RSP/M Al-Fe-V-Si and Al-Fe-Ce alloys10.1023/A:1004700830936 ↗
16. Processing window and evaporation phenomena for Ti–6Al–4V produced by selective electron beam melting10.1016/j.actamat.2014.05.037 ↗
17. Selective laser melting of aluminium components10.1016/j.jmatprotec.2010.09.019 ↗
18. Electron beam melting of Tie48Ale2Cre2Nb alloy: microstructure and mechanical properties investigation10.1016/j.intermet.2010.11.017 ↗
19. Characterization of titanium aluminide alloy components fabricated by additive manufacturing using electron beam melting10.1016/j.actamat.2009.11.032 ↗
20. Residual stresses in selective laser sintering and selective laser melting10.1108/13552540610707013 ↗
21. A new iron-rich intermetallic-AlmFe phase in Al-4.6Cu-0.5Fe cast alloy10.1007/s11661-011-1004-5 ↗
22. The microstructure of CO2 laser welds in an Al-Fe-V-Si alloy10.1016/0921-5093(94)09720-8 ↗
23. Fine-structured aluminium products with controllable texture by selective laser melting of pre-alloyed AlSi10Mg powder10.1016/j.actamat.2012.11.052 ↗
24. Iron intermetallic phases in the Al corner of the Al-Si-Fe system10.1007/s11661-003-0116-y ↗
25. Solidification characteristics of the Al-8.3Fe-0.8V-0.9Si alloy10.1007/s11661-000-0170-7 ↗
26. Ambient temperature mechanical properties of Al–8.5Fe–1.3V–1.7Si/SiC P composite10.1016/j.msea.2007.02.105 ↗
27. Structure development in rapidly solidified Al-Fe-V-Si ribbons10.1016/j.msea.2003.12.034 ↗
28. Thermostability of monolithic and reinforced Al-Fe-V-Si materials10.1163/156855109X434775 ↗
29. Characterization of microstructure and thermal stability of rapidly solidified Al-8.5Fe-1.3V-1.7Si alloy during prolonged exposure at 625°C10.1179/174328406X131064 ↗
30. Microstructural characterization of squeeze-cast Al-8Fe-1.4V-8Si10.1016/j.msea.2007.07.065 ↗
31. Solidification behaviour, microstructure and mechanical properties of high Fe-containing Al-Si-V alloys10.1016/j.jmatprotec.2008.02.043 ↗