Nitride coatings improve Ti-6Al-4V alloy behavior in creep tests

V.M.C.A. Oliveira, A.M. Vazquez, C. Aguiar, A. Robin, M.J.R. Barboza

Publisher page

Abstract

Abstract This study aimed to evaluate the effect of plasma-assisted PVD TiN and TiAlN/TiAlCrN coatings on the Ti-6Al-4V alloy under creep conditions at 600 °C. Microstructural and surface coating analysis were investigated using XRD, optical and scanning microscopy and isothermal oxidation. The results showed that the TiN coated sample showed the lowest secondary creep rate values for stresses greater than 222 MPa. Below 222 MPa, the TiAlN/TiAlCrN coated sample presented a secondary creep rate value higher than the TiN coated sample. This behavior was due to TiAlN/TiAlCrN oxidation resistance that, according to isothermal oxidation tests, did not suffer oxidation at 600 °C. The stress exponent analysis indicated that the main creep mechanism was controlled by climbing dislocations. The fracture mode is similar for all conditions studied and displayed transgranular fracture with decohesion of intergranular regions. Finally, the coated samples contribute to improved oxidation resistance, reduced damage tolerance parameter (λ) and increased lifetime of Ti-6Al-4V alloy.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Titanium Alloys Microstructure and Properties · Boron and Carbon Nanomaterials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. Titanium alloy production technology, market prospects and industry development10.1016/j.matdes.2010.09.011 ↗
2. Texture and microstructure evolution of commercially pure titanium during hot rolling: role of strain-paths10.1016/j.matdes.2015.11.073 ↗
3. Enhancing the microstructure and properties of titanium alloys through nitriding and other surface engineering methods10.1016/j.surfcoat.2004.07.115 ↗
4. Tribological oxidation behavior of PVD hard coatings10.1016/j.triboint.2009.04.026 ↗
5. Comparative study of titanium carbide and nitride coatings grown by cathodic vacuum arc technique10.1016/j.apsusc.2011.09.061 ↗
6. Investigating the fretting fatigue life of thin film titanium nitride coated aerospace Al7075-T6 alloy10.1016/j.msea.2012.08.123 ↗
7. Fatigue fracture behavior of Ti-6Al-4V PVD coated10.1016/j.proeng.2010.03.200 ↗
8. Erosion resistant titanium based PVD coatings on CFRP10.1016/j.wear.2013.01.045 ↗
9. Short-term creep properties of Ti-6Al-4V alloy subjected to surface plasma carburizing process10.1016/j.jmrt.2015.05.006 ↗
10. Fatigue property improvements of Ti-6Al-4V by thin film coatings of metallic glass and TiN: a comparison study10.1016/j.tsf.2013.08.027 ↗
11. Assessment of fatigue and corrosion fatigue behaviours of the nitrogen íon implanted CpTi10.1016/j.ijfatigue.2013.11.010 ↗
12. Comparison for mechanical properties between TiN and TiAlN coatings layers by AIP technique10.1016/S0924-0136(02)00746-X ↗
13. Multilayered TiAlN films on Ti6Al4V alloy for biomedical applications by closed field unbalanced magnetron sputter ion plating process10.1016/j.msec.2015.10.071 ↗
14. Effect of coating on the creep behavior of the Ti-6Al-4V alloy10.1016/j.msea.2007.09.024 ↗
15. Improving corrosion resistance of Ti-6Al-4V alloy through plasma-assisted PVD deposited nitride coatings10.1016/j.corsci.2014.07.047 ↗
16. Effects of Ti/TiN multilayer on corrosion resistance of nickel–titanium orthodontic brackets in artificial saliva10.1016/j.corsci.2007.03.041 ↗
17. TiAlN based wear resistant coatings modified by molybdenum addition10.1016/j.vacuum.2015.08.027 ↗
18. Microstructure and thermal stability of Ti1-xAlxN coatings deposited by reactive magnetron co-sputtering10.1016/j.phpro.2011.06.085 ↗
19. Comparison for mechanical properties between TiN and TiAlN coating layers by AIP technique10.1016/S0924-0136(02)00746-X ↗
20. Isothermal oxidation behavior of two-phase TiAl-Mn-Mo-C-Y alloys fabricated by different processes10.1016/j.intermet.2005.02.014 ↗
21. Microstructural changes during oxidation of titanium alloys10.1016/S0254-0584(03)00070-1 ↗
22. Influence of nitriding on the oxidation behaviour of titanium alloys at 700°C10.1016/j.surfcoat.2004.04.066 ↗
23. Comparison of microstructure and phase transformation for nanolayered CrN/AlN and TiN/AlN coatings at elevated temperatures in air environment10.1016/j.tsf.2006.07.162 ↗
24. Oxidation of Ti–6Al–4V alloy10.1016/j.jallcom.2008.04.024 ↗
25. Thermal stability of TiN thin films investigated by DTG/DTA10.1016/S0257-8972(01)01042-8 ↗
26. High temperature oxidation behavior of Ti0.5Al0.5N coating and Ti0.5Al0.4Si0.1N coating10.1016/j.vacuum.2012.04.013 ↗
27. Improved properties of Ti-Al-N coating by multilayer structure10.1016/j.ijrmhm.2011.05.001 ↗
28. Thermal oxidation of CP-Ti: evaluation of characteristics and corrosion resistance as a function of treatment time10.1016/j.msec.2009.03.007 ↗
29. Advances in the Wilshire extrapolation technique—full creep curve representation for the aerospace alloy Titanium 83410.1016/j.msea.2012.04.054 ↗
30. Effect of severe plastic deformation on creep behaviour of a Ti–6Al–4V alloy10.1007/s10853-013-7160-9 ↗
31. Investigation on high temperature short-term creep and stress relaxation of titanium alloy10.1016/j.msea.2014.10.015 ↗
32. Influence of heat treatment on microstructure and creep properties of hot continuous rolled Ti-6Al-4V alloy10.1016/j.msea.2012.08.116 ↗
33. Creep behavior study at 500°C of laser nitrided Ti-6Al-4V alloy10.1016/j.jmrt.2013.03.011 ↗
34. Steady state creep deformation of superalloy inconel 71810.1016/0025-5416(87)90246-1 ↗
35. Creep behavior of Ti-6Al-4V and a comparison with titanium matrix composites10.1016/j.msea.2006.05.089 ↗
36. Steady state creep behaviour of TiC particulate reinforced Ti–6Al–4V composite10.1016/S0921-5093(98)00617-0 ↗
37. Enhancement in creep resistance of Ti–6Al–4V alloy due to boron addition10.1016/j.msea.2013.12.078 ↗
38. Creep and high temperature fatigue resistance of Ti-6Al-4V modified by duplex plasma carburization/CrN coating10.4028/www.scientific.net/SSP.118.515 ↗
39. Creep behavior of Ti-6Al-4V from 450°C to 600°C
40. Mechanical behavior of crystalline solids at elevated temperature10.1016/0079-6425(68)90024-8 ↗
41. Evans · 1993
42. In situ TEM study of dislocation slip in a metastable β titanium alloy10.1016/j.scriptamat.2011.11.036 ↗
43. Structure and formation mechanism of α/α interface in laser melting deposited α+β titanium alloy10.1016/j.jallcom.2015.09.236 ↗
44. An empirical relationship between rupture life and minimum creep rate in creep-rupture tests
45. The relation between minimum creep rate and time to fracture10.1080/03063453.1976.11683560 ↗
46. The influence of temperature and strain rate on the deformation response and microstructural evolution during hot compression of a titanium alloy Ti–6Al–4V–0.1B10.1016/j.jallcom.2012.08.123 ↗
47. Creep deformation and rupture behaviour of P92 steel at 923K10.1016/j.proeng.2013.03.220 ↗
48. Improvement in creep damage tolerance of 14Cr-15Ni-Ti modified stainless steel by addition of minor elements10.1016/j.proeng.2013.03.219 ↗