Effect of mean stresses on mode of failures and fatigue life of selective laser melted stainless steel
Source abstract
Abstract
Abstract In today's era of modern manufacturing, selective laser melting is getting increasingly popular due to its capability of producing geometrically complex parts directly from CAD model in a single step. Few papers have reported the fatigue behaviour of selective laser sintered stainless steel specimens. In the present study, effect of tensile, zero and compressive mean stresses on mode of failures and fatigue strength of laser sintered 15-5 precipitation hardened stainless steel specimens have been investigated. Presence of compressive mean stress is found to improve the fatigue life while tensile mean stress is found to be detrimental. For tensile and compressive mean stresses, fracture surfaces show four distinct regions: crack initiation site, stable crack growth region, unstable crack growth region and fracture region. However, under zero mean stress fracture surfaces do not show any unstable crack growth region. Unstable crack growth region could be attributed to presence of mean stresses. Predominant mode of failure for compressive mean stress is brittle. Presence of tensile mean stress leads to fracture surface having brittle and mixed-rupture characteristics of quasi-cleavage and dimples respectively; whereas under zero mean stress fracture surface shows ductile-brittle mixed mode of failure.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. An overview of Direct Laser Deposition for additive manufacturing; Part II: mechanical behavior, process parameter optimization and control10.1016/j.addma.2015.07.002 ↗
2. Anisotropic high cycle fatigue behavior of Ti–6Al–4V obtained by powder bed laser fusion10.1016/j.ijfatigue.2016.04.032 ↗
3. On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: fatigue resistance and crack growth performance10.1016/j.ijfatigue.2012.11.011 ↗
4. Fatigue performance evaluation of selective laser melted Ti–6Al–4V10.1016/j.msea.2014.01.041 ↗
5. Improving the fatigue performance of porous metallic biomaterials produced by Selective Laser Melting10.1016/j.actbio.2016.10.005 ↗
6. Fatigue performance of additive manufactured TiAl6V4 using electron and laser beam melting10.1016/j.ijfatigue.2016.05.001 ↗
7. Comparison of the microstructures and mechanical properties of Ti–6Al–4V fabricated by selective laser melting and electron beam melting10.1016/j.matdes.2015.12.135 ↗
8. Critical assessment of the fatigue performance of additively manufactured Ti–6Al–4V and perspective for future research10.1016/j.ijfatigue.2015.12.003 ↗
9. Corrosion of bio implants10.1007/BF02706450 ↗
10. Biomedical implants: corrosion and its prevention - A review10.2174/1877610801002010040 ↗
11. Fatigue failures of austenitic stainless steel orthopedic fixation devices10.1007/BF02719191 ↗
12. On the fatigue crack growth behavior in 316L stainless steel manufactured by selective laser melting10.1016/j.engfracmech.2014.03.008 ↗
13. Fatigue performance of additive manufactured metallic parts10.1108/13552541311302932 ↗
14. Effects of building orientation and heat treatment on fatigue behavior of selective laser melted 17-4 PH stainless steel10.1016/j.ijfatigue.2016.03.014 ↗
15. Influence of the build orientation on the fatigue strength of EOS maraging steel produced by additive metal machine10.1111/ffe.12395 ↗
16. The fatigue of additive manufacturing metal parts
17. A comparison of the tensile, fatigue, and fracture behavior of Ti–6Al–4V and 15-5 PH stainless steel parts made by selective laser melting10.1007/s00170-013-5106-7 ↗
18. Fatigue strength of Co–Cr–Mo alloy clasps prepared by selective laser melting10.1016/j.jmbbm.2016.02.032 ↗
19. Additive manufactured AlSi10Mg samples using Selective Laser Melting (SLM): microstructure, high cycle fatigue, and fracture behavior10.1016/j.matdes.2011.07.067 ↗
20. Oxides, porosity and fatigue performance of AlSi10Mg parts produced by selective laser melting10.1016/j.ijfatigue.2016.06.002 ↗
21. A comparison of fatigue strength sensitivity to defects for materials manufactured by AM or traditional processes10.1016/j.ijfatigue.2016.06.020 ↗
22. Long fatigue crack growth in Inconel 718 produced by selective laser melting10.1016/j.ijfatigue.2016.03.012 ↗
23. Bending fatigue life characterisation of direct metal laser sintering nickel alloy 71810.1111/ffe.12286 ↗
24. Low cycle fatigue behavior of direct metal laser sintered Inconel alloy 71810.1016/j.ijfatigue.2016.08.019 ↗
25. Fatigue behavior of IN718 microtrusses produced via additive manufacturing10.1016/j.matdes.2016.05.032 ↗
26. Powder bed binder jet printed alloy 625: densification, microstructure and mechanical properties10.1016/j.matdes.2016.06.067 ↗
27. 〈http://www.eos.info/material-m〉.
28. Strain ratio effects on low-cycle fatigue behavior and deformation microstructure of 2124-T851 aluminum alloy10.1016/j.msea.2014.03.040 ↗