Abstract In this study, the effect of different microstructures resulting from thermochemical processes of X65 pipeline steel on mechanical properties of welding in the presence of hydrogen was investigated. According to studies conducted, due to the charge of hydrogen, the hardness of base metal (BM) increased by 10%, the hardness of heat affected zone (HAZ) samples increased by about 13%, the yield strength of base metal increased by an average of 5% and the yield strength of HAZ increased by about 7%, indicating hardening. Elongation was reduced by 32–70% and the percentage of ductile fracture decreased by an average 46% which shows that the fracture of samples in the presence of hydrogen is brittle. In the study of hydrogen defect and concentration of hydrogen permeated to the material it was determined that, the ferrite-pearlite banded microstructure of base metal has a higher hydrogen defect sensitivity than HAZ with an acicular ferrite microstructure and hard phase. In base metal samples under various rolling conditions, the two-pass rolled and the final rolling temperature of 800 °C sample (2BM800), with a smaller grain microstructure and higher interface, had the most diffusive hydrogen content and therefore had the highest hydrogen defects. In the case of HAZ samples, the effect of hydrogen on the increase in hardness and strength properties is greater than that of the base metal samples due to the different microstructure (of the acicular ferrite) and the variable grain size (i.e. the presence of two coarse-grained and fine grained areas). Overall, the results of this study showed that the microstructure has a significant effect on mechanical properties, the amount of diffusive hydrogen and hydrogen defects in welds.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Welding Techniques and Residual Stresses · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Effect of microstructure on the hydrogen trapping efficiency and hydrogen induced cracking of linepipe steel10.1016/j.corsci.2008.03.007 ↗
2. R. API, 571–Damage Mechanisms Affecting Fixed Equipment in the Refining Industry, Am. Pet. Inst., 2003.
3. Effect of environmental and metallurgical factors on hydrogen induced cracking of HSLA steels10.1016/j.corsci.2008.09.030 ↗
4. Effects of hydrogen-charging on the susceptibility of X100 pipeline steel to hydrogen-induced cracking10.1016/j.ijhydene.2009.09.090 ↗
5. Hydrogen embrittlement of high strength pipeline steels10.1016/j.corsci.2006.02.011 ↗
6. Investigation on the H2S-resistant behaviors of acicular ferrite and ultrafine ferrite10.1016/S0167-577X(02)00720-6 ↗
7. Hydrogen effect on a low carbon ferritic-bainitic pipeline steel10.1016/j.ijhydene.2014.09.029 ↗
8. Effect of microstructures and inclusions on hydrogen-induced cracking and blistering of A537 steel10.1016/j.msea.2015.06.085 ↗
9. Effect of microstructure and inclusions on hydrogen induced cracking susceptibility and hydrogen trapping efficiency of X120 pipeline steel10.1016/j.msea.2010.07.022 ↗
10. A possible explanation for the contradictory results of hydrogen effects on macroscopic deformation10.1016/j.ijpvp.2012.08.001 ↗
11. The mutual effects of hydrogen and microstructure on hardness and impact energy of SMA welds in X65 steel10.1016/j.msea.2016.09.103 ↗
12. Effect of bainitic microstructure on the susceptibility of pipeline steels to hydrogen induced cracking10.1016/j.msea.2011.03.036 ↗
13. Effect of manganese content and microstructure on the susceptibility of X70 pipeline steel to hydrogen cracking10.1016/j.msea.2012.04.076 ↗
14. Investigation of role of alloy microstructure in hydrogen-assisted fracture of AISI 4340 steel using circumferentially notched cylindrical specimens10.1016/j.msea.2017.05.056 ↗
15. Effect of hydrogen on room-temperature hardness of B2 FeAl alloys10.1016/j.scriptamat.2008.07.002 ↗
16. Bridgman · 1952
17. R.S. Treseder, Guarding Against Hydrogen Embrittlement, 1981.
18. I.D. Ballesteros, A.F. Ponciano, J.A.D.C Bott, Study of the Susceptibility of API 5L X80 Girth welds to sulfide stress corrosion cracking and hydrogen embrittlement, in: Int. Pipeline Conf., American Society of Mechanical Engineers, 2010, pp. 375–380.10.1115/IPC2010-31243 ↗
19. Comparison of microfractographic behaviour of acicular ferrite and bainite and hydrogen cracking resistance
20. Challenge of mechanical properties of an acicular ferrite pipeline steel10.1016/j.msea.2006.05.029 ↗
21. Production of ultra-fine grain microstructures in Al-Mg alloys by conventional rolling10.1016/S1359-6454(02)00253-7 ↗
22. Microstructural evolution in Al deformed to strains of 60 at 400 °C10.1016/0036-9748(85)90268-6 ↗
23. Effects of deformation parameters on the final microstructure and mechanical properties in warm rolling of a low-carbon steel10.1007/s00170-006-0594-3 ↗
24. The influence of hot rolling parameters on the microstructure and mechanical properties of an ultra-high strength steel10.1016/S0924-0136(00)00474-X ↗
25. Effect of the Zener-Hollomon parameter on the microstructures and mechanical properties of copper subjected to plastic deformation10.1016/j.actamat.2008.10.021 ↗
26. Influence of Mo content on microstructure and mechanical properties of high strength pipeline steel10.1016/j.matdes.2004.03.009 ↗
27. Fatigue crack growth acceleration caused by irreversible hydrogen desorption in high-strength steel and its mechanical condition10.1016/j.msea.2011.07.003 ↗
28. The role of hydrogen in hardening/softening steel: influence of the charging process10.1016/j.scriptamat.2015.05.017 ↗
29. Hydrogen diffusion and trapping in a precipitation-hardened nickel-copper-aluminum alloy Monel K-500 (UNS N05500)10.1016/j.actamat.2013.02.007 ↗
30. Investigation of the effect of electrolytic hydrogen charging of X70 steel: I. The effect of microstructure on hydrogen-induced cold cracking and blistering10.1016/j.ijhydene.2016.04.114 ↗
31. Effect of hot-rolling conditions on the physical properties of a carbon steel
32. Ductility enhancement in AZ31 magnesium alloy by controlling its grain structure10.1016/S1359-6462(01)00996-4 ↗
33. Effect of nickel and molybdenum additions on weld metal toughness in a submerged arc welded HSLA line-pipe steel10.1016/j.jmatprotec.2005.10.028 ↗
34. Microstructure and mechanical properties of TWIP steel joints10.1016/S1006-706X(14)60137-0 ↗
35. The effect of hydrogen on stress corrosion behavior of X65 steel welded joint in simulated deep sea environment10.1016/j.oceaneng.2016.01.020 ↗
36. The effect of hydrogen on the mechanical properties of high purity iron II. Effect of quenched-in hydrogen below room temperature10.1016/0025-5416(79)90192-7 ↗
37. Solid solution softening and hardening by mobile solute atoms with special focus on hydrogen10.1016/j.scriptamat.2012.07.022 ↗
38. Hydrogen-induced hardening and softening of Ni-Nb-Zr amorphous alloys: dependence on the Zr content10.1016/j.scriptamat.2014.08.029 ↗
39. Resolving the hydrogen effect on dislocation nucleation and mobility by electrochemical nanoindentation10.1016/j.scriptamat.2011.12.004 ↗