Achieving an ultra-high strength in a low alloyed Al alloy via a special structural design
Source abstract
Abstract
Abstract An ultrafine-grained (UFGed) low alloyed aluminum alloy (6061 Al alloy) with a special nano-sized spherical precipitate structure was achieved by friction stir processing (FSP) and post-FSP aging. The evolution of the grains and precipitates during post-FSP aging and their contribution to mechanical properties were investigated. Under a low rotation rate (200 rpm) with water cooling, the average grain size of the FSP sample was only 200 nm. The ultimate tensile strength of the UFG 6061Al alloy aged at 100 °C for 20 min achieved 573 MP with a high elongation of 17%. This strength was nearly 90% higher than that of 6061 Al-T6 alloy (∼300 MPa), and was equivalent to that of commercial 7075Al-T651 alloy (∼572 MPa, the typical high alloyed Al alloy). Such a good mechanical property was attributed to the good thermal stability and the accelerated precipitation of the FSP UFGed structure under the low-temperature and short-time aging conditions. Further, the contribution of various strengthening mechanisms to the total strength in post-FSP aged Al alloys was quantitatively evaluated. This work provides an effective strategy for obtaining low alloyed high-strength Al alloys, which is beneficial for reducing environmental burdens and improving long-term sustainability.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Advanced Welding Techniques Analysis · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Warming trends in Asia amplified by brown cloud solar absorption10.1038/nature06019 ↗
2. Impacts of vehicle weight reduction via material substitution on life-cycle greenhouse gas emissions10.1021/acs.est.5b03192 ↗
3. High-strength aluminum-based light-weight materials for safety components – recent progress by microstructural refinement and particle reinforcement10.3139/146.110631 ↗
4. Machining of high strength light weight Alloys for engine applications10.1016/j.cirp.2007.05.027 ↗
5. Microstructural and corrosion characteristics of iron-silicon alloyed layer on 5083 Al alloy by electrical discharge alloying processing10.2320/matertrans.M2010363 ↗
6. Playing with defects in metals10.1038/nmat4929 ↗
7. X. Li, L. Yang, K. Lu, Making materials plain: concept, principle and applications, Acta Metall. Sin.
8. Cai · 2016 · 1
9. Modeling of precipitation hardening for the naturally aged Al-Mg-Si-Cu alloy AA611110.1016/S1359-6454(03)00167-8 ↗
10. Microstructural evolution and age hardening in aluminium alloys10.1016/S1044-5803(99)00051-0 ↗
11. Plastic strain-induced grain refinement at the nanometer scale in copper10.1016/j.actamat.2006.07.013 ↗
12. Microstructural evolution and wear characteristics of equal channel angular pressing processed semi-solid-cast hypoeutectic aluminum alloys10.1016/j.matdes.2014.11.054 ↗
13. Aging behavior of Al 6061 alloy processed by high-pressure torsion and subsequent aging10.1007/s11661-015-2840-5 ↗
14. Formation of nano-laminated structure in nickel by means of surface mechanical grinding treatment10.1016/j.actamat.2015.06.014 ↗
15. Characterization of plastic deformation and material flow in ultrasonic vibration enhanced friction stir welding10.1016/j.scriptamat.2015.02.022 ↗
16. Thermal stability of nanocrystallized surface produced by surface mechanical attrition treatment in aluminum alloys10.1016/j.surfcoat.2012.03.069 ↗
17. Effects of ARB and aging processes on mechanical properties and microstructure of 6061 aluminum alloy10.1016/j.jmatprotec.2011.01.023 ↗
18. Fabrication of high-quality Ti joint with ultrafine grains using submerged friction stirring technology and its microstructural evolution mechanism10.1016/j.actamat.2018.12.059 ↗
19. Improvement of mechanical properties of aluminum die casting alloy by multi-pass friction stir processing10.1016/j.msea.2006.07.150 ↗
20. Microstructure and mechanical properties of multi-pass friction stir processed aluminum alloy 606310.1016/j.matdes.2013.07.062 ↗
21. Optimization of electrical conductivity and strength combination by structure design at the nanoscale in Al–Mg–Si alloys10.1016/j.actamat.2015.07.039 ↗
22. Influence of severe plastic deformation on aging of Al–Mg–Si alloys10.1016/j.msea.2005.08.135 ↗
23. Precipitation kinetics in a severely plastically deformed 7075 aluminium alloy10.1016/j.actamat.2013.11.071 ↗
24. Effect of aging treatment on heavily deformed microstructure of a 6061 aluminum alloy after equal channel angular pressing10.1016/S1359-6462(01)01109-5 ↗
25. Enhanced mechanical properties and electrical conductivity in ultrafine-grained Al alloy processed via ECAP-PC10.1007/s10853-013-7279-8 ↗
26. Nanostructure and related mechanical properties of an Al–Mg–Si alloy processed by severe plastic deformation10.1080/09500830802186938 ↗
27. Intrinsic high cycle fatigue behavior of ultrafine grained pure Cu with stable structure10.1007/s40843-016-5068-6 ↗
28. Microstructure and low-cycle fatigue of a friction-stir-welded 6061 aluminum alloy10.1007/s11661-010-0279-2 ↗
29. Effects of stacking fault energy, strain rate and temperature on microstructure and strength of nanostructured Cu–Al alloys subjected to plastic deformation10.1016/j.actamat.2011.06.013 ↗
30. The limits of refinement by severe plastic deformation10.1002/adem.200600133 ↗
31. Effect of ECAP on microstructure and mechanical properties of a commercial 6061 Al alloy produced by powder metallurgy10.1016/S0925-8388(03)00008-2 ↗
32. Achieving friction stir welded pure copper joints with nearly equal strength to the parent metal via additional rapid cooling10.1016/j.scriptamat.2011.02.019 ↗
33. Effect of heat input conditions on microstructure and mechanical properties of friction-stir-welded pure copper10.1007/s11661-010-0254-y ↗
34. Enhanced mechanical properties of friction stir welded 5083Al-H19 joints with additional water cooling10.1016/j.jmst.2017.01.016 ↗
35. Effect of Ag and Cu additions on natural aging and precipitation hardening behavior in Al-Mg-Si alloys10.1016/j.jallcom.2016.11.140 ↗
36. Restoration of the bake hardening response in a naturally aged twin-roll cast AlMgSi automotive sheet10.1016/j.scriptamat.2006.03.022 ↗
37. Strain-induced ultrahard and ultrastable nanolaminated structure in nickel10.1126/science.1242578 ↗
38. Structure and thermal stability of nanocrystalline materials
39. Hall–Petch relationship in friction stir welds of equal channel angular-pressed aluminium alloys10.1016/S0921-5093(03)00008-X ↗
40. Friction stir welding and processing10.1016/j.mser.2005.07.001 ↗
41. High tensile ductility via enhanced strain hardening in ultrafine-grained Cu10.1016/j.msea.2011.10.070 ↗
42. Grain refinement of 1050 aluminum alloy by friction stir processing10.1023/A:1012882413401 ↗
43. Coupled precipitation and yield strength modelling for non-isothermal treatments of a 6061 aluminium alloy10.1016/j.actamat.2013.09.041 ↗
44. Modelling of the age hardening behaviour of Al–Mg–Si alloys10.1016/S1359-6454(00)00301-3 ↗
45. Influence of tool dimension and welding parameters on microstructure and mechanical properties of friction-stir-welded 6061-t651 aluminum alloy10.1007/s11661-008-9586-2 ↗
46. Mechanical properties at room temperature of an Al–Zn–Mg–Cu alloy processed by equal channel angular pressing10.1016/j.jallcom.2011.06.070 ↗
47. Effect of severe plastic deformation on the structure and mechanical properties of Al-Cu-Mg alloy10.1088/1757-899X/63/1/012081 ↗
48. Strength, grain refinement and solute nanostructures of an Al–Mg–Si alloy (AA6060) processed by high-pressure torsion10.1016/j.actamat.2013.10.022 ↗
49. Tensile properties and tensile fracture characteristics of cast Al–Zn–Mg alloys processed by equal channel angular pressing10.1007/s12666-017-1067-0 ↗