Overcoming the strength-ductility trade-off by the combination of static recrystallization and low-temperature heat-treatment in Co-Cr-W-Ni alloy for stent application

Kosuke Ueki, Soh Yanagihara, Kyosuke Ueda, Masaaki Nakai, Takayoshi Nakano, Takayuki Narushima

Abstract

A process combining swaging, static recrystallization, and heat treatment at 873 K (low-temperature heat-treatment, LTHT) was developed for achieving both high ultimate strength and high ductility in Co-20Cr-15W-10Ni (mass%, CCWN) alloy for stent application. The alloys swaged to a sectional area reduction rate of 58.3% were annealed at 1373–1473 K for 30–300 s. Under annealing at 1373 K for 300 s, a fine grain structure with an average grain size of ~6 μm formed, while under annealing at 1473 K, a structure with an average grain size of 12 μm formed after 120 s. In the alloys annealed at 1373–1448 K, the formation of η-phase precipitates (M6X-M12X type, M: metallic elements, X: C and/or N) was observed, while no precipitates were observed in the alloys annealed at 1473 K. The improvement in ultimate strength by grain refinement was confirmed. Alloys annealed at 1473 K showed higher ductility compared to those annealed at 1373–1448 K even if the grain size was similar. It is considered that the η-phase precipitates deteriorated the ductility of the annealed alloys. LTHT suppressed the strain-induced martensitic γ-to-ε transformation to improve the ductility of the fine-grained as well as coarse-grained alloys. Thus, regardless of the grain size, it is newly evidenced that LTHT effectively improves ductility in CCWN alloy. By combining high-temperature short-time annealing and LTHT, both the ultimate strength and ductility of Co-20Cr-15W-10Ni (mass%) alloy improved, and it was possible to provide properties suitable for next-generation balloon-expandable stents with Co-20Cr-15W-10Ni (mass%) alloy.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · High Temperature Alloys and Creep · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Deformation behavior and dynamic recrystallization of biomedical Co-Cr-W-Ni (L-605) alloy10.1007/s11661-012-1602-x ↗
2. “Stent tubing: understanding the desired attributes”, med. Device mater
3. Cobalt alloys as implants in humans
4. Fatigue and life prediction for cobalt-chromium stents: a fracture mechanics analysis10.1016/j.biomaterials.2005.10.012 ↗
5. Precipitates in biomedical Co-Cr alloys10.1007/s11837-013-0567-6 ↗
6. Microstructure and mechanical properties of heat-treated Co-20Cr-15W-10Ni alloy for biomedical application10.1007/s11661-016-3488-5 ↗
7. Microstructural changes during plastic deformation and corrosion properties of biomedical Co-20Cr-15W-10Ni alloy heat-treated at 873 K10.1007/s11661-018-4597-0 ↗
8. Synchronous improvement in strength and ductility of biomedical Co-Cr-Mo alloys by unique low-temperature heat treatment10.1016/j.msea.2018.10.016 ↗
9. High strength and high ductility in the Co-20Cr-15W-10Ni alloy having a bimodal grain structure achieved by static recrystallization10.1016/j.msea.2018.06.104 ↗
10. Bimodal grain-structure formation in a Co-Cr-based superalloy during ultrahigh-homologous temperature annealing without severe plastic deformation10.1016/j.jallcom.2018.12.320 ↗
11. Grain growth and static recrystallization kinetics in Co-20Cr-15W-10Ni(L-605) cobalt-base superalloy10.1080/14786435.2014.903342 ↗
12. Mineta · Metall. Mater. Trans. A · 2012 · 43 · 335110.1007/s11661-012-1142-4 ↗
13. Carbide formation and dissolution in biomedical Co-Cr-Mo alloys with different carbon contents during solution treatment10.1007/s11661-010-0227-1 ↗
14. Changes in microstructure of biomedical Co-Cr-Mo alloys during aging at 973 to 1373 K10.2320/matertrans.MI201507 ↗
15. Combined effects of strain and grain size on carbide precipitation and sensitization in 304 stainless steel10.1016/0956-716X(94)90548-7 ↗
16. Effects of strain and grain size on carbide precipitation and corrosion sensitization behavior in 304 stainless steel10.1016/S1359-6454(97)00106-7 ↗
17. Correlation of the M23C6 precipitation morphology with grain boundary characteristics in austenitic stainless steel10.1016/S0921-5093(01)01254-0 ↗
18. A TEM investigation of M23C6 carbide precipitation behaviour on varying grain boundary misorientations in 304 stainless steels10.1023/A:1004390029071 ↗
19. Interaction between recrystallization and precipitation during the high temperature deformation of HSLA steels
20. Effect of carbon content on static recrystallization behavior of work-hardened austenite in low alloy steel and its mechanism10.2320/matertrans.M2016344 ↗
21. Metall. Mater. Trans. A, “Tensile properties and microstructure of Haynes25 alloy after aging at elevated temperatures for extended times”10.1007/s11661-004-0223-4 ↗
22. Effect of microstructure on mechanical properties of refractory Co-Cr-W-Ni alloy10.1007/s11041-008-9031-6 ↗
23. Twinning and strain-induced f.c.c.→h.c.p. transformation on the mechanical properties of Co Ni Cr Mo alloys10.1016/0025-5416(76)90234-2 ↗
24. Méthode d'analyse quantitative des variétés allotropiques du cobalt par les rayons X10.1051/metal/195047020139 ↗
25. Smaller is less stable: size effects on twinning vs. transformation of reverted austenite in TRIP-maraging steels10.1016/j.actamat.2014.07.020 ↗
26. Effects of austenite grain size on ε martensitic transformation in Fe-15mass%Mn alloy10.2320/matertrans1989.34.489 ↗
27. Computational simulation of the dependence of the austenitic grain size on the deformation behavior of TRIP steels10.1016/S0749-6419(99)00079-0 ↗
28. Strain induced ε-martensite in a Co-Cr-Mo alloy: grain size effects10.1016/S0167-577X(99)00021-X ↗
29. Driving force for γ→ε martensitic transformation and stacking fault energy of γ in Fe-Mn binary system10.1007/s11661-000-0271-3 ↗
30. Influence of specimen dimensions on the tensile behavior of ultrafine-grained Cu10.1016/j.scriptamat.2008.05.031 ↗
31. Effects of specimen thickness in tensile tests on elongation and deformation energy for industrially pure iron10.2355/isijinternational.ISIJINT-2016-555 ↗
32. The effect of grain size and grain orientation on deformation twinning in a Fe-22wt.%Mn-0.6wt.%C TWIP steel10.1016/j.msea.2010.02.041 ↗