Effect of heat treatment on the microstructure, microhardness and impact toughness of TC11 and TC17 linear friction welded joint
Source abstract
Abstract
Abstract The service life of whole blisks for the aero-engine compressor is sharply decreased due to the dissimilar linear friction welded (LFWed) joint of Ti–6.5Al–3.5Mo–1.5Zr–0.3Si (TC11) and Ti–4Mo–4Cr–5Al–2Sn–2Zr (TC17) alloys, which have the different microstructure and mechanical properties. To optimize the microstructure and performance of the joint, and improve service life of the whole blisks, the post-weld heat treatment (PWHT) with annealing, solution plus aging were adopted for the welded joint. The results show that the nucleation rate of primary α P phase increases obviously, which are spheres, rods and strips, and orthorhombic martensite α s phases transform into hexagonal martensite α s phases interlaced evenly on the β phase matrix on the WZ of TC17 side; meanwhile, acicular hexagonal martensite α s phases transform into lamellar α s phases on the WZ of TC11 side after solid solution and dual aging. The difference of the microhardness on both sides of the joint is narrowed significantly. The impact toughness of the joint is improved sharply from 9.3 J/cm2 after welding to 27.6 J/cm2 with an increase of 200%. In addition, the dissolution and growth model of primary α p phases were established, which can reasonably predict the nucleation and grow process of α phase. Furthermore, the narrowed discrepancy of the microhardness and increased impact toughness can be attributed to the decreased slice thickness of martensite α s phase, based on the dislocation slip mechanism and distorted discordant model.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Metal and Thin Film Mechanics · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. The role of microtexture on the faceted fracture morphology in Ti-6Al-4V subjected to high-cycle fatigue10.1016/j.actamat.2010.03.036 ↗
2. Microstructural evolution, mechanical properties and fracture toughness of near beta titanium alloy during different solution plus aging heat treatments10.1016/j.jallcom.2019.07.134 ↗
3. Microstructure and deformation behavior of Ti-6Al-4V alloy by high-power laser solid forming10.1016/j.actamat.2017.04.026 ↗
4. Strain-controlled fatigue properties of linear friction welded dissimilar joints between Ti-6Al-4V and Ti-6.5Al-3.5Mo-1.5Zr-0.3Si alloys10.1016/j.msea.2014.06.010 ↗
5. Strain hardening behavior of linear friction welded joints between TC11 and TC17 dissimilar titanium alloys10.1016/j.msea.2014.10.044 ↗
6. Effect of the forging pressure on the microstructure and residual stress development in Ti-6Al-4V linear friction welds10.1016/j.actamat.2009.07.055 ↗
7. Numerical simulation of transient temperature and axial deformation during linear friction welding between TC11 and TC17 titanium alloys10.1016/j.commatsci.2014.05.062 ↗
8. A computational modeling of fully friction contact-interaction in linear friction welding of Ni-based superalloys10.1016/j.matdes.2019.108244 ↗
9. Solid state joining of metals by linear friction welding: a literature review10.1179/026708310X520510 ↗
10. Linear friction welding of Ti-6Al-4V: processing, microstructure, and mechanical-property inter-relationships10.1007/s11661-005-0335-5 ↗
11. The effect of grain orientation on fracture morphology during high-cycle fatigue of Ti-6Al-4V10.1016/j.actamat.2009.04.018 ↗
12. Microstructural evolution of a TC11 titanium alloy during linear friction welding10.1007/s10853-010-4716-9 ↗
13. Hot working of Ti-6Al-3Mo-2Zr-0.3Si alloy with lamellar alpha plus beta starting structure using processing map10.1016/j.matdes.2008.07.031 ↗
14. Microstructural evolution and mechanical properties of a linear friction welded two-phase Ti-6.5Al-3.5Mo-1.5Zr-0.3Si titanium alloy joint10.1016/j.msea.2018.11.059 ↗
15. Hot deformation mechanism and microstructure evolution of TC11 titanium alloy in β field10.1016/S1003-6326(08)60175-2 ↗
16. Effect of solution treatment and aging on microstructure and tensile properties of high strength β titanium alloy, Ti–5Al–5V–5Mo–3Cr10.1016/j.matdes.2014.04.015 ↗
17. Linear friction welding of Ti–5Al–2Sn–2Zr–4Mo–4Cr alloy with dissimilar microstructure10.1016/j.jmatprotec.2013.11.006 ↗
18. Effect of post-weld heat treatment on microstructure and property of linear friction welded Ti17 titanium alloy joint10.1179/1362171811Y.0000000079 ↗
19. Microstructure and mechanical property correlation and property optimization of a near β titanium alloy Ti-733310.1016/j.jallcom.2016.04.303 ↗
20. Microstructure evolution and mechanical properties of linear friction welded Ti-5Al-2Sn-2Zr-4Mo-4Cr (Ti17) titanium alloy joints10.1002/adem.200900185 ↗
21. Strain-controlled fatigue properties of dissimilar welded joints between Ti–6Al–4V and Ti17 alloys10.1016/j.matdes.2013.02.034 ↗
22. Evaluation of titanium alloys fabricated using rapid prototyping technologies—electron beam melting and laser beam melting10.3390/ma4101776 ↗
23. Low cycle fatigue properties of linear friction welded joint of TC11 and TC17 titanium alloys10.1016/j.jallcom.2016.03.113 ↗
24. Biocompatibility of β-stabilizing elements of titanium alloys
25. Effects of Sn and Zr on the microstructure and mechanical properties of Ti-Ta-based shape memory alloys10.1007/s11665-010-9817-8 ↗
26. omega-Assisted nucleation and growth of alpha precipitates in the Ti-5Al-5Mo-5V-3Cr-0.5Fe beta titanium alloy10.1016/j.actamat.2009.01.007 ↗
27. Static globularization mechanism of Ti-17 alloy during heat treatment10.1016/j.jallcom.2017.11.117 ↗
28. Microstructure and microhardness of Ti6246 linear friction weld10.1016/j.msea.2012.10.089 ↗
29. Precipitation of secondary alpha in competition with epitaxial growth of primary alpha in two-phase titanium alloys10.1016/j.jallcom.2017.04.209 ↗
30. Influence of solution treatment on microstructure and mechanical properties of a near β titanium alloy Ti-733310.1016/j.matdes.2015.06.015 ↗
31. Effect of thermomechanical processing on evolution of various phases in Ti-Nb alloys10.1007/s12034-011-0338-3 ↗
32. The search for novel, superhard materials10.1116/1.581977 ↗
33. Hall-petch relationships in gamma titanium aluminides10.1016/1359-6462(96)00097-8 ↗