journal article·2019-03

Variation of phase composition of Mo-Si-B alloys induced by boron and their mechanical properties and oxidation resistance

Rui Li, Bin Li, Xuan Chen, Juan Wang, Tao Wang, Yichao Gong, Shuai Ren, Guojun Zhang

Publisher page

Abstract

Abstract Mo-12Si-xB (x = 5, 8.5, 17 at%) alloys, doped with 0.9 wt% nanometer La2O3, were fabricated via a powder metallurgical process. The distribution of the α-Mo, Mo3Si and Mo5SiB2 phases existed in these alloys was dependent on the volume fractions of the individual phases. The Mo-12Si-5B (~52 vol% of α-Mo) and Mo-12Si-8.5B (~46 vol% of α-Mo) alloys possessed a continuous α-Mo matrix where Mo3Si/Mo5SiB2 particles distributed dispersedly and the former exhibited the highest fracture toughness. Our theoretical analysis demonstrated that the crucial contribution of crack trapping mechanism to the toughness and the α-Mo volume fraction increasing effectively promoted this mechanism. Besides, the α-Mo/intermetallic interface debonding and the formation of intragranular microcracks induced by La2O3 provided extra contributions to toughness. The Mo-12Si-17B alloy (~65 vol% of intermetallic) formed an intermetallic matrix with embedded semi-continuous α-Mo colonies and other isolated α-Mo islands, having the highest compression strengths at 800–1300 °C. Especially at 1200–1300 °C, the intermetallic matrix with low plastic deformation played a significant role in reinforcing alloy. Besides, the intragranular La2O3 particles strengthened alloy by pinning down and accumulating dislocations in the grain interior. The Mo-12Si-17B was also found to have the excellent oxidation resistance at 1000 °C owing to exhibiting the shortest duration and minimal mass loss in the transient oxidation stage. Moreover, higher B content decreased the viscosity of the borosilicate and thereby formed a dense and protective glassy borosilicate scale quickly, which substantially reduced the growth of inner oxide layers in the steady oxidation stage. In addition, the La2O3 as a blocking phase could impede the permeation of MoO3 bubbles/clusters through the flowing SiO2 glass scale.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Intermetallics and Advanced Alloy Properties · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Mo-Si-B alloys for ultrahigh-temperature structural applications10.1002/adma.201200764 ↗
2. Effect of Zr addition on the high-temperature oxidation behavior of Mo-Si-B alloys10.1007/s11085-009-9175-9 ↗
3. Ambient-to elevated-temperature fracture and fatigue properties of Mo-Si-B alloys: role of microstructure10.1007/s11661-005-0112-5 ↗
4. Boron-doped molybdenum silicides for structural applications10.1016/S0921-5093(98)01045-4 ↗
5. Oxide scale formation and isothermal oxidation behavior of Mo-Si-B intermetallics at 600–1000 °C10.1016/S0966-9795(98)00058-2 ↗
6. Mechanical properties of Mo5SiB2 single crystals10.1016/S0921-5093(01)01575-1 ↗
7. Stoichiometry and mechanical properties of Mo3Si10.1016/S0966-9795(00)00058-3 ↗
8. Optimization of Mo-Si-B intermetallic alloys10.1007/s11661-005-0166-4 ↗
9. Physical and mechanical properties of single crystals of the T2 phase in the Mo-Si-B system10.1016/S0966-9795(01)00049-8 ↗
10. High-temperature compression behavior of Mo-Si-B alloys10.1016/j.actamat.2004.08.035 ↗
11. Transient oxidation of Mo-Si-B alloys: effect of the microstructure size scale10.1016/j.actamat.2009.06.036 ↗
12. Oxidation behavior of multiphase Mo-Si-B alloys10.1016/j.intermet.2004.02.011 ↗
13. Synthesis of oxidation resistant silicide coating on Mo-Si-B alloys10.1016/j.scriptamat.2005.05.015 ↗
14. Oxidation resistant coatings for ultrahigh temperature refractory Mo‐base alloys10.1002/adem.200900118 ↗
15. Fracture and fatigue resistance of Mo-Si-B alloys for ultrahigh-temperature structural applications10.1016/j.scriptamat.2003.11.002 ↗
16. Correlation between microstructure and properties of fine grained Mo-Mo3Si-Mo5SiB2 alloys10.1016/j.intermet.2013.10.025 ↗
17. Effect of Si/B ratio on the microstructure and mechanical properties of lanthanum oxide-doped Mo-Si-B alloys10.1016/j.jallcom.2013.04.116 ↗
18. Processing and properties of multiphase Mo-Si-B alloys10.4028/www.scientific.net/MSF.426-432.4301 ↗
19. High temperature compressive flow behavior of a Mo-Si-B solid solution alloy10.1016/j.scriptamat.2005.09.015 ↗
20. Nanostructured high-strength molybdenum alloys with unprecedented tensile ductility10.1038/nmat3544 ↗
21. Microstructure and mechanical properties of lanthanum oxide-doped Mo-12Si-8.5B (at%) alloys10.1016/j.jallcom.2013.04.116 ↗
22. Experiment and multiscale modeling of the coupled influence of constituents and precipitates on the ductile fracture of heat-treatable aluminum alloys10.1016/j.actamat.2005.04.002 ↗
23. Microstructure and mechanical behaviour of reaction hot pressed multiphase Mo-Si-B and Mo-Si-B-Al intermetallic alloys10.1016/j.intermet.2006.01.057 ↗
24. Processing and mechanical properties of a molybdenum silicide with the composition Mo-12Si-8.5B (at%)10.1016/S0966-9795(00)00093-5 ↗
25. Structural integrity in severe thermal environments10.1111/j.1151-2916.1977.tb16085.x ↗
26. Crack-profile shapes formed under a Vickers indent pyramid10.1007/BF01770938 ↗
27. Sintering characteristics of nanocrystalline TiO210.1557/JMR.1990.0609 ↗
28. A Mo-Si-Bintermetallic alloy with a continuous α-Mo matrix10.1016/S1359-6462(01)01227-1 ↗
29. Effects of lanthanum oxide content on mechanical properties of mechanical alloying Mo-12Si-8.5B (at%) alloys10.1016/j.ijrmhm.2013.07.011 ↗
30. Ductility of Mo-12Si-8.5B alloys doped with lanthanum oxide by the liquid-liquid doping method10.1016/j.jallcom.2015.04.047 ↗
31. A three-dimensional analysis of crack trapping and bridging by tough particles10.1016/0022-5096(91)90026-K ↗
32. The fracture resistance of directionally solidified dual-phase NiAl reinforced with refractory metals10.1016/0956-7151(93)90079-8 ↗
33. An investigation of fatigue and fracture in NiAl-Mo composites10.1016/S0921-5093(98)00503-6 ↗
34. Mechanisms of fatigue crack propagation in metals, ceramics and composites: role of crack tip shielding10.1016/0025-5416(88)90547-2 ↗
35. Perspective on the development of high-toughness ceramics10.1111/j.1151-2916.1990.tb06493.x ↗
36. Transient stage oxidation behavior of Mo76Si14B10 alloy at 1150 °C10.1016/j.corsci.2012.11.021 ↗
37. Characterization of oxidation kinetics of Mo-Si-B-based materials10.1007/s11085-016-9659-3 ↗