journal article·2019-09

Damage tolerant design by microstructural gradation – Influence of processing parameters and build orientation on crack growth within additively processed 316L

F. Brenne, T. Niendorf

Publisher page

Abstract

Abstract Powder bed based additive manufacturing techniques, such as selective laser melting (SLM) and selective electron beam melting (EBM), attract a lot of interest due to the possibility of producing geometrically complex and individualized components. Additionally, the dependency of the resulting microstructure on the processing parameters applied enables for fabrication of graded structures having locally different mechanical properties. In this study, the effect of different types of gradation on the crack growth behavior of 316L stainless steel processed by SLM was investigated. Using an approach combining mechanical testing, local strain analysis by means of digital image correlation (DIC) and electron backscatter diffraction (EBSD), insights into the relationships between the local microstructure, the crack growth rate (CGR) and the crack deflection on macroscopic and microscopic scale were obtained. The results show clear dependencies of the CGR on the local microstructure, which can be rationalized based on effects stemming from intercrystalline and transcrystalline crack growth. In graded structures, arrest of priorly growing cracks was observed upon reaching a coarse grained area, when the growth direction was perpendicular to the building direction during processing. This highlights the capability of achieving damage tolerant structures without substantially sacrificing strength.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (60)

Show source-provided references
1. Wohlers · 2015
2. Additive layered manufacturing: sectors of industrial application shown through case studies10.1080/00207540903479786 ↗
3. Metal additive manufacturing: a review10.1007/s11665-014-0958-z ↗
4. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
5. Microstructure and mechanical behavior of Ti-6Al-4V produced by rapid-layer manufacturing, for biomedical applications10.1016/j.jmbbm.2008.05.004 ↗
6. On the impact of additive manufacturing on microstructural and mechanical properties of stainless steel and Ni-base alloys10.1007/s00501-017-0590-y ↗
7. Mechanical properties of AlSi10Mg produced by selective laser melting10.1016/j.phpro.2012.10.059 ↗
8. Helmer · 2014
9. Microstructures and mechanical behavior of Inconel 718 fabricated by selective laser melting10.1016/j.actamat.2011.12.032 ↗
10. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
11. Additive manufacturing of 316L stainless steel by electron beam melting for nuclear fusion applications10.1016/j.jnucmat.2016.12.042 ↗
12. Microstructural characterization and mechanical performance of hot work tool steel processed by selective laser melting10.1007/s11663-014-0267-9 ↗
13. Strong morphological and crystallographic texture and resulting yield strength anisotropy in selective laser melted tantalum10.1016/j.actamat.2013.04.036 ↗
14. Effect of heat treatment of 316L stainless steel produced by selective laser melting (SLM)
15. Fatigue performance evaluation of selective laser melted Ti–6Al–4V10.1016/j.msea.2014.01.041 ↗
16. High cycle fatigue (HCF) performance of Ti-6Al-4V alloy processed by selective laser melting10.4028/www.scientific.net/AMR.816-817.134 ↗
17. On the fatigue crack growth behavior in 316L stainless steel manufactured by selective laser melting10.1016/j.engfracmech.2014.03.008 ↗
18. Inconel 939 processed by selective laser melting: effect of microstructure and temperature on the mechanical properties under static and cyclic loading10.1016/j.msea.2013.09.025 ↗
19. On the microstructural and mechanical properties of post-treated additively manufactured Inconel 718 superalloy under quasi-static and cyclic loading10.1016/j.msea.2016.05.089 ↗
20. Additive manufactured AlSi10Mg samples using Selective Laser Melting (SLM) - microstructure, high cycle fatigue, and fracture behavior10.1016/j.matdes.2011.07.067 ↗
21. Comparison of microstructure and mechanical properties of Scalmalloy® produced by selective laser melting and laser metal deposition10.3390/ma11010017 ↗
22. On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: fatigue resistance and crack growth performance10.1016/j.ijfatigue.2012.11.011 ↗
23. Fatigue crack growth mechanisms at the microstructure scale in as-fabricated and heat treated Ti-6Al-4V ELI manufactured by electron beam melting (EBM)10.1016/j.engfracmech.2017.03.024 ↗
24. Characterization of fatigue crack growth behavior in LENS fabricated Ti-6Al-4V using high-energy synchrotron x-ray microtomography
25. Evaluation of orientation dependence of fracture toughness and fatigue crack propagation behavior of as-deposited ARCAM EBM Ti-6Al-4V10.1007/s11837-015-1298-7 ↗
26. Crack path selection at the interface of wrought and wire+arc additive manufactured Ti–6Al–4V10.1016/j.matdes.2016.05.027 ↗
27. Fatigue crack propagation behaviour in wire+arc additive manufactured Ti‐6Al‐4V: effects of microstructure and residual stress10.1016/j.matdes.2015.10.141 ↗
28. Fatigue and fracture toughness characteristics of laser rapid manufactured Inconel 625 structures10.1016/j.msea.2010.08.034 ↗
29. Fatigue crack growth behavior and mechanical properties of additively processed EN AW-7075 aluminium alloy10.1016/j.prostr.2016.06.380 ↗
30. Steel showing twinning-induced plasticity processed by selective laser melting - an additively manufactured high performance material10.1016/j.matchar.2013.08.010 ↗
31. On the effect of internal channels and surface roughness on the high-cycle fatigue performance of Ti-6Al-4V processed by SLM10.1016/j.matdes.2018.01.042 ↗
32. Design of novel materials for additive manufacturing - isotropic microstructure and high defect tolerance10.1038/s41598-018-19376-0 ↗
33. Fine-structured aluminium products with controllable texture by selective laser melting of pre-alloyed AlSi10Mg powder10.1016/j.actamat.2012.11.052 ↗
34. Epitaxial laser metal forming: analysis of microstructure formation10.1016/S0921-5093(99)00202-6 ↗
35. Highly anisotropic steel processed by selective laser melting10.1007/s11663-013-9875-z ↗
36. Grain orientation effects on the growth of short fatigue cracks in austenitic stainless steel10.1016/j.msea.2008.04.050 ↗
37. Plastic strain amplitude dependent surface path of microstructurally short fatigue cracks in face-centered cubic metals10.1016/S0921-5093(99)00060-X ↗
38. Effect of grain size and misorientation angle on fatigue crack growth of nanocrystalline materials10.1016/j.msea.2016.03.105 ↗
39. Microstructure and fatigue crack growth in a γ-Fe-Ni-Al alloy10.1016/0001-6160(76)90104-8 ↗
40. Microstructural influences on fatigue crack growth in Ti-6Al-4V10.1016/0025-5416(74)90104-9 ↗
41. Influence of grain structure and slip planarity on fatigue crack growth in low alloying artificially aged 2xxx aluminium alloys10.1016/j.ijfatigue.2006.08.005 ↗
42. An EBSD based comparison of the fatigue crack initiation mechanisms of nickel and nitrogen-stabilized cold-worked austenitic stainless steels10.1016/j.msea.2013.08.027 ↗
43. Microstructure dependent fatigue cracking resistance of Ti–6.5Al–3.5Mo–1.5Zr–0.3Si alloy10.1016/S1005-0302(12)60106-6 ↗
44. Crack deflection: implications for the growth of long and short fatigue cracks10.1007/BF02663313 ↗
45. Functionally graded alloys obtained by additive manufacturing10.1002/adem.201300579 ↗
46. Maier · 2011
47. ASTM International · 2015
48. Application of the electrical potential method to crack length measurements using johnson's formula10.1520/JTE11560J ↗
49. Labelling additively manufactured parts by microstructural gradation – advanced copy-proof design10.1108/RPJ-12-2014-0183 ↗
50. Lattice structures manufactured by SLM: on the effect of geometrical dimensions on microstructure evolution during processing10.1007/s11663-014-0086-z ↗
51. Microstructure and fracture behavior of 316L austenitic stainless steel produced by selective laser melting10.1016/j.jmst.2016.06.016 ↗
52. On the fatigue properties of metals manufactured by selective laser melting – the role of ductility10.1557/jmr.2014.157 ↗
53. Correlation between process parameters, microstructure and properties of 316 L stainless steel processed by selective laser melting10.1016/j.msea.2018.01.103 ↗
54. Origin of stray grain formation in single-crystal superalloy weld pools from heat transfer and fluid flow modeling10.1016/j.actamat.2009.10.051 ↗
55. On the size of plastic zone ahead of crack tip10.1016/0013-7944(86)90219-5 ↗
56. Selektives Laserschmelzen metallischer Materialien - einfluss von Prozessparametern und Miniaturisierung auf Mikrostruktur und mechanisches Verhalten geometrisch komplexer Strukturen
57. Modeling fatigue crack growth in a bimaterial specimen with the configurational forces concept10.1016/j.msea.2009.04.059 ↗
58. Improvement of fatigue life by compliant and soft interlayers10.1016/j.scriptamat.2015.10.021 ↗
59. Fatigue crack propagation behavior in the vicinity of an interface between materials with different yield stresses10.1016/S0921-5093(00)00703-6 ↗
60. Theoretical, experimental and numerical investigations on crack growth in fracture mechanical graded structures10.1016/j.engfracmech.2016.05.003 ↗