Effect of Cu addition on the microstructure and mechanical properties of In–Sn-based low-temperature alloy
Source abstract
Abstract
Abstract The In–48Sn eutectic alloy has emerged as a favorable solder for flexible electronic devices, owing to its low operating temperature. However, the low strength of In–48Sn eutectic alloy compared with that of other commercial solders affects the product life and limits its use in the device applications. Herein, we studied the effects of xCu addition (x = 1.0, 2.0, and 8.0 wt %) on melting temperature, phase segregation, and mechanical properties of In–Sn alloy. The results revealed that the melting temperatures of the In–Sn–Cu (ISC) alloys were close to that of eutectic In–Sn alloy (115 °C) due to the ternary reaction in the ISC alloys. In addition, the initial solidification temperature of the η-(Cu,In,Sn) compound took place below 400 °C, and partial solid-transformation to ternary τ-Cu2In3Sn occurred in the temperature range 83–78 °C, owing to the diffusion of Cu-atoms and consumption of the β-In3Sn phase in the new ISC alloys. The phase segregation affected the phase fraction in the ISC matrix and the mechanical properties of ISC alloys. Furthermore, the In–Sn-1.0Cu alloy exhibited the highest elongation of 74%, which was more than twice that of In–48Sn alloy. Simultaneously, the In–Sn-8.0Cu alloy presented the highest tensile strength of approximately 17.0 MPa, which was 1.5 times that of the In–48Sn alloy.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Semiconductor materials and interfaces · Silicon and Solar Cell Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Recent progress in SLID bonding in novel 3D-IC technologies10.1016/j.jallcom.2019.152825 ↗
2. Flexible electronic devices based on polymers
3. Tuller · 2009
4. Substrates for flexible electronics: a practical investigation on the electrical, film flexibility, optical, temperature, and solvent resistance properties10.1002/polb.22227 ↗
5. Microstructure and mechanical properties of the In–48Sn–xAg low-temperature alloy10.1007/s10853-020-04691-7 ↗
6. Fine microstructured In−Sn−Bi solder for adhesion on a flexible PET substrate: its effect on superplasticity and toughness
7. Characterization of eutectic Sn-Bi solder joints10.1007/BF02655427 ↗
8. Sn-3.0Ag-0.5Cu/Sn-58Bi composite solder joint assembled using a low-temperature reflow process for PoP technology10.1016/j.matdes.2019.108144 ↗
9. Recent progress on the development of Sn–Bi based low-temperature Pb-free solders10.1007/s10854-019-00701-w ↗
10. The effect of substrate on the microstructure and mechanical behavior of eutectic Indium-Tin
11. Lead-free solders in microelectronics10.1016/S0927-796X(00)00010-3 ↗
12. Kim · 2005 · vol. 386 · 151
13. Phase identification and growth kinetics of the intermetallic compounds formed during In-49Sn/Cu soldering reactions10.1007/s11664-002-0136-1 ↗
14. Microstructure and mechanical properties of Pb-free solder alloys for low-cost electronic assembly: a review10.1007/BF02651361 ↗
15. Effect of Zinc addition on the microstructure, thermal and mechanical properties of Indium-Tin-xZinc alloys10.1007/s11664-018-6768-6 ↗
16. The solidification behavior and microstructure of in-Sn-Cu solder alloys with low Cu
17. Improvement of mechanical properties of In-48mass%Sn solder by Ag and Cu addition
18. Experimental determination and thermodynamic calculation of the phase equilibria in the Cu-In-Sn system10.1007/s11664-001-0135-7 ↗
19. Liquidus projection and solidification of the Sn-In-Cu ternary alloys10.1007/s11664-008-0380-0 ↗
20. Phase equilibria in the In–Sn-rich part of the Cu–In–Sn ternary system10.1016/j.jallcom.2009.07.129 ↗
21. Improved mechanical properties induced by in and in & Zn double additions to eutectic Sn58Bi alloy10.1007/s10854-019-01056-y ↗
22. Very long-term aging of 52In-48Sn (at.%) solder joints on Cu-plated stainless steel substrates10.1007/s10853-008-3083-2 ↗
23. Effect of Zinc addition on the microstructure, thermal and mechanical properties of Indium-Tin-xZinc alloys10.1007/s11664-018-6768-6 ↗
24. Suppressing interfacial voids in Cu/In/Cu microbump with Sn and Cu addition10.1016/j.matlet.2019.126855 ↗
25. 250 °C isothermal section of ternary Sn-In-Cu phase equilibria10.1557/jmr.2009.0317 ↗
26. Improvement in the mechanical properties of eutectic Sn58Bi alloy by 0.5 and 1 wt% Zn addition before and after thermal aging10.1016/j.jallcom.2018.06.121 ↗
27. Sayyadi · 2019 · vol. 3 · 1
28. Microstructure and mechanical properties of Sn–xBi solder alloy10.1007/s10854-015-2880-z ↗
29. Undercooling and nucleation during solidification10.2355/isijinternational.35.580 ↗