Selective laser melting of Fe–Al alloys with simultaneous gradients in composition and microstructure
Source abstract
Abstract
Abstract Selective laser melting technique was employed to fabricate a step-wise compositionally graded Fe–Al alloy coupon using the in-situ alloying of blended powders. Microstructural characterization of the fabricated coupons shows a columnar to equiaxed grain structure transition with increasing Al content along the building direction, along which the laser scan speed is increased. In the low Al content regions, the absence of constitutional undercooling (CUC) allows columnar grain growth against the macroscopic thermal gradients, whereas dominance of CUC in high Al regions leads to fully equiaxed and refined microstructures. Nanoindentation studies show a linear increase in hardness and reduction in elastic modulus for Al content up to ~20 at.%; no significant anisotropy in these properties could be seen.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Resolving the porosity-unmelted inclusion dilemma during in-situ alloying of Ti34Nb via laser powder bed fusion10.1016/j.actamat.2020.116522 ↗
2. Functionally graded material of 304L stainless steel and inconel 625 fabricated by directed energy deposition: characterization and thermodynamic modeling10.1016/j.actamat.2016.02.019 ↗
3. Laser powder bed fusion of compositionally graded CoCrMo-Inconel 718
4. Fabrication of functionally graded TiC/Ti composites by laser engineered net shaping10.1016/S1359-6462(03)00020-4 ↗
5. Structure and mechanical properties of iron-aluminium alloys10.1016/0001-6160(68)90107-7 ↗
6. Relationship between atomic ordering and fracture in Fe-Al alloys10.1007/BF00543684 ↗
7. Iron aluminides10.1146/annurev-matsci-070218-125911 ↗
8. Deformation behaviour of iron-rich iron-aluminum alloys at low temperatures10.1016/S1359-6454(03)00089-2 ↗
9. Fabrication and microstructure characterization of selective laser‐melted FeAl intermetallic parts10.1016/j.surfcoat.2012.05.072 ↗
10. Material transitions within multi-material laser deposited intermetallic iron aluminides
11. Direct synthesis of Fe-Al alloys from elemental powders using laser engineered net shaping10.3390/ma13030531 ↗
12. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
13. Neutron diffraction residual stress determinations in Fe3Al based iron aluminide components fabricated using wire-arc additive manufacturing (WAAM), Addit
14. Graded microstructure and mechanical properties of additive manufactured Ti–6Al–4V via electron beam melting10.1016/j.actamat.2015.06.036 ↗
15. Fabrication of Fe-FeAl functionally graded material using the wire-arc additive manufacturing process10.1007/s11663-015-0509-5 ↗
16. Wear behavior and microstructure of hypereutectic Al-Si alloys prepared by selective laser melting10.1016/j.apsusc.2016.03.221 ↗
17. Re-determination of transition temperatures in the Fe–Al system by differential thermal analysis10.3139/146.101512 ↗
18. Physical measurements of iron-aluminum alloys with 10 to 50 at.-% Al. IV. Young's modulus of the alloys
19. Physical aspects of process control in selective laser sintering of metals10.1002/adem.200310099 ↗
20. Micro-and meso-structures and their influence on mechanical properties of selectively laser melted Ti-6Al-4V10.1016/j.actamat.2018.05.044 ↗
21. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
22. The redistribution of solute atoms during the solidification of metals10.1016/0001-6160(53)90126-6 ↗
23. Kou · 2003 · 431
24. Single-crystal laser deposition of superalloys: processing–microstructure maps10.1016/S1359-6454(00)00367-0 ↗
25. Theory of microstructural development during rapid solidification10.1016/0001-6160(86)90056-8 ↗
26. Origin of grain orientation during solidification of an aluminum alloy10.1016/j.actamat.2016.05.057 ↗
27. Additive manufacturing of ultrafine-grained high-strength titanium alloys10.1038/s41586-019-1783-1 ↗
28. Determination of the growth restriction factor and grain size for aluminum alloys by a quasi-binary equivalent method10.1016/j.msea.2012.01.072 ↗
29. Microstructures and grain refinement of additive-manufactured Ti-x W alloys10.1007/s11661-017-4117-7 ↗
30. Solidification behavior and grain morphology of laser additive manufacturing titanium alloys10.1016/j.jallcom.2018.11.055 ↗
31. Kurz · 1989
32. Facile route to bulk ultrafine-grain steels for high strength and ductility10.1038/s41586-021-03246-3 ↗
33. Evaluation of elastic modulus and hardness of Fe–Al base intermetallics by nano-indentation techniques10.1016/j.intermet.2013.02.012 ↗