Effect of pre-strain and quench rate on stress corrosion cracking resistance of a low-Cu containing Al–Zn–Mg–Cu alloy
Source abstract
Abstract
Abstract The synergy effect of quench rate and pre-strain prior to artificial aging heat treatment on microstructure, stress corrosion cracking (SCC) resistance, and mechanical property of a low-Cu containing Al–Zn–Mg–Cu alloy have been investigated using SCC and room temperature tensile tests, combined with X-ray diffraction, scanning electron microscopy (SEM), and high-angle angular dark-field scanning transmission electron microscopy (HAADF-STEM) microstructural examinations. The results showed that the SCC resistance was significantly improved by pre-strain and slow quench-rate owing to discontinuous distribution, large inter-space, and high Cu content of grain boundary precipitates. Moreover, the pre-strain was more effective for fast-quenched samples on improving SCC resistance compared with slowly quenched samples. The SCC mechanisms have been discussed in detail.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (61)
Show source-provided references
1. Progress in structural materials for aerospace systems10.1016/j.actamat.2003.08.023 ↗
2. Relationship between alloy composition, microstructure and exfoliation corrosion in alloys10.1016/j.corsci.2011.05.057 ↗
3. Mechanical properties of solution heat treated Al-Zn-Mg-Cu (7075) alloy under different cooling conditions: analysis with full field measurement and finite element modeling10.1016/j.jallcom.2020.158180 ↗
4. EASA · 2018
5. Environmental cracking performance of new generation thick plate 7000-T7x series alloys in humid air10.1016/j.corsci.2020.108701 ↗
6. Effect of Cr, Yb and Zr additions on localized corrosion of Al–Zn–Mg–Cu alloy10.1016/j.corsci.2009.08.001 ↗
7. Effect of trace Er on the microstructure and properties of Al–Zn–Mg–Cu–Zr alloys during heat treatments10.1016/j.msea.2020.139807 ↗
8. The effect of quench rate and overageing temper on the corrosion behaviour of AA705010.1016/j.corsci.2013.10.010 ↗
9. Effect of quenching rate on microstructure and stress corrosion cracking of 7085 aluminum alloy10.1016/S1003-6326(11)61138-2 ↗
10. Effect of retrogression treatments on microstructure, hardness and corrosion behaviors of aluminum alloy 708510.1016/j.jallcom.2019.152264 ↗
11. Stress-corrosion cracking of high-strength aluminum alloys
12. Enhancing the stress corrosion cracking resistance of low-Cu containing Al–Zn–Mg–Cu aluminum alloy by step-quench and aging heat treatment10.1016/j.corsci.2019.108184 ↗
13. Some effects of alloy composition on stress corrosion cracking in Al–Zn–Mg–Cu alloys10.1016/j.corsci.2015.05.016 ↗
14. Influence of grain structure on quench sensitivity relative to localized corrosion of high strength aluminum alloy10.1016/j.matchemphys.2015.10.051 ↗
15. Enhancing stress corrosion cracking resistance of low Cu-containing Al–Zn–Mg–Cu alloys by slow quench rate10.1016/j.matdes.2018.107558 ↗
16. Effects of pre-strain on the surface residual stress and corrosion behavior of an Al–Zn–Mg–Cu alloy plate10.1016/j.matchar.2020.110129 ↗
17. Influence of pre-stretching and aging processes on comprehensive performance of aluminum alloy10.1080/10426914.2016.1221087 ↗
18. Effect of pre-strain on microstructure and stress corrosion cracking of over-aged 7050 aluminum alloy10.1016/j.jallcom.2008.01.137 ↗
19. Effect of pre-strain on precipitation and exfoliation corrosion resistance in an Al–Zn–Mg–Cu alloy10.1088/1757-899X/274/1/012007 ↗
20. Effect of pre-stretching and ageing on the strength and fracture toughness of aluminum alloy 705010.1016/j.msea.2011.01.068 ↗
21. Influence of dislocations on hydrogen diffusion and trapping in an Al–Zn–Mg–Cu aluminium alloy10.1016/j.matdes.2019.107901 ↗
22. Effect of tensile deformation and heat treatment on the stress corrosion susceptibility of an Al–Zn–Mg–Cu alloy10.1179/030716974803288347 ↗
23. Effect of pre-deformation on quench-induced inhomogeneity of microstructure and hardness in 7050 aluminum alloy10.1016/j.matchar.2019.110005 ↗
24. Grain structure and quench-rate effects on strength and toughness of AA7050 Al–Zn–Mg–Cu–Zr alloy plate10.1007/BF02671263 ↗
25. GB12445. 1-90, National Standard of China. High Strength Alloys-Method of Stress Corrosion Test for Double Cantilever Beam (DCB) Specimens.
26. X-ray line broadening from filed aluminium and wolfram10.1016/0001-6160(53)90006-6 ↗
27. Precipitation strengthening at ambient and elevated temperatures of heat-treatable Al (Sc) alloys10.1016/S1359-6454(02)00201-X ↗
28. The contrast factors of dislocations in cubic crystals: the dislocation mode of strain anisotropy in practice10.1107/S0021889899009334 ↗
29. Characterization of nanocrystalline materials by X-ray line profile analysis10.1007/s10853-006-0696-1 ↗
30. Enhancing creep formability and comprehensive property in Al–Mg–Si alloy by combinatorial pre-ageing and large pre-deformation10.1016/j.msea.2021.141967 ↗
31. Synergy effect of Si addition and pre-straining on microstructure and properties of Al–Cu–Mg alloys with a medium Cu/Mg ratio10.1016/j.msea.2019.138429 ↗
32. The influence of Cu addition and pre-straining on the natural aging and bake hardening response of Al–Mg–Si alloys10.1016/j.jallcom.2016.07.066 ↗
33. Residual stress, stress relief, and inhomogeneity in aluminum plate10.1016/S1359-6462(01)01201-5 ↗
34. A modeling of residual stress in stretched aluminum alloy plate10.1016/j.jmatprotec.2012.06.019 ↗
35. Effect of microstructure on the quench sensitivity of AlZnMgCu alloys10.1016/j.jallcom.2010.07.124 ↗
36. Microstructural effects on hydrogen enbrittlement in a high purity 7075 aluminum alloy10.1016/0001-6160(87)90139-8 ↗
37. Investigation of precipitation behavior and related hardening in AA7055 aluminum alloy10.1016/j.msea.2008.09.065 ↗
38. Precipitation kinetics, mechanical strength and electrical conductivity of AlZnMgCu alloys10.1016/S1359-6454(96)00033-X ↗
39. Aging behavior and precipitate characterization of a high Zn-containing Al–Zn–Mg–Cu alloy with various tempers10.1016/j.matdes.2016.03.150 ↗
40. Analysis of age hardening precipitates of Al–Zn–Mg–Cu alloys in a wide range of quenching rates using small angle X-ray scattering10.1016/j.matdes.2018.01.037 ↗
41. Synchrotron-based holotomography and X-ray fluorescence study on the stress corrosion cracking behavior of the peak-aged 7075 aluminum alloy10.1016/j.jallcom.2019.152722 ↗
42. Hydrogen partitioning behavior and related hydrogen embrittlement in Al–Zn–Mg alloys10.1016/j.engfracmech.2019.106503 ↗
43. Effect of solution pH on electrochemical and stress corrosion cracking behaviour of a 7150 Al–Zn–Mg–Cu alloy10.1016/j.msea.2014.02.036 ↗
44. Stress corrosion cracking in Al–Zn–Mg–Cu aluminum alloys in saline environments10.1007/s11661-012-1528-3 ↗
45. The influence of temperature on the hydrogen environmentally assisted cracking of AA7449-T7651 in moist air10.1016/j.corsci.2020.109199 ↗
46. Hydrogen-induced delayed fracture under mode II loading10.1007/BF02643993 ↗
47. Stress corrosion cracking in high strength steel under mode III loading10.1007/BF02643992 ↗
48. Investigation of stress corrosion cracking of the cost and forged steel in water10.1007/BF02646842 ↗
49. A quantitative analysis of hydrogen trapping10.1007/BF02661939 ↗
50. Effect of precipitate state on the stress corrosion behavior of 7050 aluminum alloy10.1016/j.matchar.2016.01.022 ↗
51. Discontinuous propagation of stress corrosion cracks in Al–Zn–Mg alloys10.1016/0036-9748(79)90305-3 ↗
52. Grain boundary segregation and hydrogen-induced fracture in 7050 aluminium alloy10.1016/1359-6454(95)00406-8 ↗
53. Grain boundary segregation in Al–Zn–Mg alloys-Implications to stress corrosion cracking10.1007/BF02700441 ↗
54. Theoretical predictions of structure and related properties of intermetallics10.1179/mst.1992.8.4.345 ↗
55. The elastic behaviour of a crystalline aggregate10.1088/0370-1298/65/5/307 ↗
56. First-principles calculations of elastic and thermodynamic properties of the four main intermetallic phases in Al–Zn–Mg–Cu alloys10.1016/j.commatsci.2014.06.031 ↗
57. The solution composition and electrode potential in pits, crevices and cracks10.1016/0010-938X(83)90014-8 ↗
58. Effect of prior deformation and heat treatment on the corrosion-induced hydrogen trapping in aluminium alloy 202410.1016/j.corsci.2013.11.021 ↗
59. The diffusion and trapping of hydrogen in high purity aluminum
60. Gibala · 1984 · 271
61. Combined microtomography, thermal desorption spectroscopy, X-ray diffraction study of hydrogen trapping behavior in 7XXX aluminum alloys10.1016/j.msea.2015.12.092 ↗