The T23 and T24 steels were designed for welding membrane water walls without preheating and without post-weld heat treatment (PWHT). Results presented demonstrate that non-tempered weld joints of low-alloy creep-resistant steels T23 and T24 undergo a process of secondary hardening during long-term exposure at elevated temperatures. This process is accompanied by degradation of plastic properties, especially in the heat affected zone (HAZ). Therefore, PWHT of T23 and T24 welds is necessary to achieve suitable hardness and plastic properties of welds.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · High Temperature Alloys and Creep · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (10)

Show source-provided references
1. V. Foldyna, J. Purmenský, Z. Kuboň, Acta Metallurgica Slovaca, No. 13, Hutnícka fakulta - TU Košice, 2007, Košice, pp. 556–562, ISSN 1335–1532.
2. Foldyna · 2001 · 150
3. Purmenský · 1999 · 419
4. P. Mohyla, Changes of mechanical properties of CrMoV steel welds during long term heat exposure in sub-creep range, Ph.D. thesis, VŠB–TU Ostrava, 2001.
5. Ashby · 1969 · 113
6. EN ISO 15614-1. Specification and qualification of welding procedures for metallic materials—welding procedure test. Part 1: arc and gas welding of steels and arc welding of nickel and nickel alloys, European Committee for Standardization, 2004.
7. Karlsson · 2000 · 171–174
8. Wortel · 2004 · 21
9. Purmenský · Japan Society for the Promotion of Science · 2003 · 44 · 315
10. Foldyna · 2002 · 1477