The mechanism of elevated temperature intergranular cracking in heat-resistant alloys
Source abstract
Abstract
Abstract Reheat or stress relief cracking phenomena have been reassessed in 2.25Cr1.5W heat-resistant alloys. During rupture test, time to intergranular failure increases with decreasing temperature and tensile stress and is shorter in the alloy containing a higher bulk content of phosphorus. Also the time to intergranular failure can be expressed by t = t 0 · σ − n ·exp( Q /RT) where t 0 is the proportional constant, n the stress exponent and Q the activation enthalpy. Matrix softening is accelerated under tensile stress and an active carbide growth occurs at grain boundaries oriented normal to the tensile stress direction. Because impurities segregate actively to dimples frequently observed at reheat intergranular fracture surfaces, the dimples are not micro-ductile fracture areas but the grain boundary carbide interfaces. The segregation concentration of the impurities is much higher at the grain boundary carbide interfaces than the carbide-free grain boundaries. The phosphorus segregation at the carbide interfaces of the alloy containing the higher bulk content of phosphorus is mainly replaced by the segregation of nitrogen, tin and tellurium in the alloy containing a lower bulk content of phosphorus. The elevated temperature intergranular cracking under tensile stress occurs finally due to the carbide-free grain boundary cracking following the decohesion of the grain boundary carbide interfaces.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High Temperature Alloys and Creep · Metallurgy and Material Forming · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Bailey · 1994
2. Balaguer · Weld. J · 1989 · 68 · 121
3. Nawrocki · Weld. J. · 2003 · 82 · 25
4. Nawrocki · Weld. J. · 2000 · 79 · 355
5. Hippsley · Acta Metall. · 1980 · 28 · 86910.1016/0001-6160(80)90104-2 ↗
6. Raj · Acta Metall. · 1975 · 23 · 65310.1016/0001-6160(75)90047-4 ↗
7. Chuang · Acta Metall. · 1979 · 27 · 26510.1016/0001-6160(79)90021-X ↗
8. Shin · Acta Metall. · 1984 · 32 · 153510.1016/0001-6160(84)90100-7 ↗
9. Misra · Acta Metall. · 1996 · 44 · 885
10. Bika · Acta Metall. · 1995 · 43 · 189510.1016/0956-7151(94)00388-X ↗
11. Hippsley · Acta Metall. · 1982 · 30 · 64110.1016/0001-6160(82)90113-4 ↗
12. Geng · Solid State Commun. · 2001 · 119 · 58510.1016/S0038-1098(01)00298-8 ↗
13. Lee · Metall. Trans. · 1984 · 15A · 141510.1007/BF02648571 ↗
14. Weng · Mater. Sci. Technol. · 1987 · 3 · 20710.1179/mst.1987.3.3.207 ↗
15. Van Der Brug · Acta Metall. · 1996 · 44 · 505
16. Raj · Acta Metall. · 1978 · 261 · 99510.1016/0001-6160(78)90050-0 ↗
17. Hull · Phil. Mag. A · 1959 · 4 · 67310.1080/14786435908243264 ↗
18. Speight · Met. Sci. · 1967 · 1 · 8310.1016/0036-9748(67)90021-X ↗
19. Hondros · Int. Metals Rev. · 1977 · 222 · 262
20. Lea · Phil. Mag. · 1977 · 35 · 21310.1080/14786437708235984 ↗
21. Rellick · Metall. Trans. · 1971 · 2 · 149210.1007/BF02662692 ↗
22. Seah · Acta Metall. · 1980 · 28 · 95510.1016/0001-6160(80)90112-1 ↗
23. Honda · Met. Sci. · 1968 · 2 · 17210.1179/030634568790443404 ↗
24. Rees · J. Iron Steel Inst. · 1951 · 157
25. Barrett · 1973
26. Weertman · 1971
27. Leslie · Metall. Trans. · 1972 · 3 · 510.1007/BF02680580 ↗
28. Conrad · 1961
29. Leslie · 1982
30. Speich · Metal. Trans. · 1972 · 3 · 203110.1007/BF02643211 ↗
31. Grant · 1954