journal article·2017-05

Evaluation of strength property variations across 9Cr-1Mo steel weld joints using automated ball indentation (ABI) technique

S. Nagaraju, J. GaneshKumar, P. Vasantharaja, M. Vasudevan, K. Laha

Publisher page

Abstract

Abstract The variations of strength properties across 9Cr-1Mo steel weld joints fabricated by different arc welding processes such as shielded metal arc welding (SMAW), tungsten inert gas (TIG) and activated tungsten inert gas (A-TIG) have been evaluated employing automatic ball indentation (ABI) technique. ABI tests were conducted at 298 K across various zones of the weld joints comprising of base metal, weld metal, heat affected zone (HAZ) and intercritical HAZ (ICHAZ) regions. The flow curves obtained from ABI tests were correlated with corresponding conventional tensile test results. In general, the tensile strength decreased systematically across the weld joint from weld metal to base metal. Inter critical HAZ exhibited the least strength implying that it is the weakest zone. The incomplete phase transformation in the ICHAZ during weld thermal cycle caused the softening. The A-TIG weld metal exhibited higher UTS and strain hardening values due to higher carbon in the martensite. The strain hardening exponent exhibited only slight variation across the various regions of the weld joints. A-TIG weld joint exhibited higher weld metal and HAZ strength, marginally higher UTS to YS ratio in the weld metal and HAZ compared to that of the other two processes. Hence, among the three welding processes chosen, A-TIG welding process is found to be superior in producing a 9Cr-1Mo steel weld joint with better strength properties.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Welding Techniques and Residual Stresses · Metal and Thin Film Mechanics · Advanced machining processes and optimization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Microstructural evolution of modified 9Cr-1Mo steel10.1007/BF02661098 ↗
2. LjubicaMilovic · 2017
3. Microstructures and mechanical properties of creep resistant steel for application at elevated temperatures10.1016/j.matdes.2012.10.057 ↗
4. Study of the simulated heat affected zone of creep resistant 9–12% advanced chromium steel10.1080/10426910802160544 ↗
5. Experimental and numerical evaluation of a steamline behaviour using local approach
6. Ferritic/martensitic steels for next-generation reactors10.1016/j.jnucmat.2007.05.005 ↗
7. R.W. Vanstone, Advanced (“700°C”) PF power plant, in:Proceedings of the 3rd Conference on ‘Advances in Materials Technology for Fossil Power Plants, The Institute Of Materials, University of Wales Swansea, London, 2001, pp. 7–14.
8. G.W. Cunningham, P. Patriarca, E.E. Hoffman, Ferritic steels as alternate structural materials for high-temperature applications, in: Proceedings International Conference ‘Ferritic steels for high temperature application’, ASM metals park, Ohio, 1983, pp. 3–6.
9. Vasudevan · 2007
10. V. Maduraimuthu, M. Vasudevan, V. Muthupondi, A.K. Bhaduri, T. Jayakumar, Study of the effect of activated flux on the microstructure and mechanical properties of mod. 9Cr-1Mo steel, Metall. Trans. B, 43(1), pp. 123–132.10.1007/s11663-011-9568-4 ↗
11. Effects of Activating flux on arc phenomena in gas tungsten welding10.1179/136217100101538461 ↗
12. Investigation in to arc constriction by active fluxes for tungsten inert gas welding10.1179/136217100101538191 ↗
13. Evaluation of TIG-flux welding on the characteristics of stainless steel10.1179/174329305X48329 ↗
14. Mechanisms giving increased weld depth due to a flux10.1088/0022-3727/38/18/018 ↗
15. Performance of activated TIG process in austenitic stainless steel welds10.1016/j.jmatprotec.2010.11.003 ↗
16. GTAW flux increases weld joint penetration
17. Effect of fluxes containing oxides on tungsten inert gas welding process10.1179/174329306X77047 ↗
18. TIG welding with single component fluxes10.1016/S0924-0136(99)00435-5 ↗
19. Effect of activated flux on the microstructure and mechanical properties of Plain 9Cr-1Mo steel weld joint10.1080/10426914.2011.610212 ↗
20. Characterization of gradients in mechanical properties of SA-533B steel welds using ball indentation10.1016/S0308-0161(99)00006-X ↗
21. Characterization of cast stainless steel weld pools by using ball indentation technique10.1016/j.msea.2009.02.007 ↗
22. Stress-strain characteristics of the heat affected zone in an HY-100 weldment as determined from microindentation testing10.1016/S1044-5803(96)00128-3 ↗
23. Determination of the mechanical properties of austenitic stainless steel weldments by using stress strain microprobe10.1016/j.msea.2006.03.041 ↗
24. Evaluation of variation of tensile strength across 316LN stainless steel weld joint using automated ball indentation technique10.1179/1878641315Y.0000000008 ↗
25. Evaluation of mechanical properties across micro alloyed HSLA steel weld joints using automated ball indentation10.1016/j.msea.2015.10.104 ↗
26. Nondestructive monitoring of structural materials using automated ball indentation (ABI) technique10.1016/j.nucengdes.2003.06.006 ↗
27. Ball indentation studies on the effect of aging on mechanical behavior of alloy 62510.1016/S0921-5093(98)01098-3 ↗
28. Nondestructive determination of tensile properties and fracture toughness of cold worked A36 steel10.1016/S0308-0161(98)00093-3 ↗
29. Evaluation of indentation tensile properties of Ti alloys by considering plastic constraint effect10.1016/j.msea.2011.03.052 ↗
30. Low temperature aging embrittlement of CF-8 stainless steel10.1016/S0921-5093(99)00140-9 ↗
31. Measurement of through-the-thickness variations of mechanical properties in SA508 Gr.3 pressure vessel steels using ball indentation test technique10.1016/S0308-0161(97)00114-2 ↗
32. Tabor · 1951
33. Non-destructive evaluation of deformation and fracture properties of materials using stress-strain microprobe
34. A numerical approach to spherical indentation techniques for material property evaluation10.1016/j.jmps.2005.04.007 ↗
35. Miannay · 2001
36. ASTM: Standard test methods for tension testing of metallic materials, Philadelphia, American Society for Testing and Materials. [ASTM E8], 2013.
37. F.M. Haggag, Field indentation microprobe for structuralintegrity evaluation, US patent, 1989, 4852397.
38. F.M. Haggag, J.A. Wang, M.A. Sokolov, K.L. Murthy, Use of portable/in situ stress-strain microprobe system to measure stress strain behavior and damage in metallic materials and structures, Philadelphia, American Society for Testing and Materials. [ASTM STP1318], 1997, pp. 85–98.10.1520/STP11894S ↗
39. Effect of multi pass TIG and activated TIG welding process on the thermo-mechanical behaviour of 316LN stainless steel weld joints10.1007/s11663-016-0600-6 ↗
40. Vasudevan · 2008
41. Type IV cracking susceptibility in weld joints of different grades of Cr-Mo ferritic steel10.1007/s11661-008-9724-x ↗