Synchronously improved fatigue strength and fatigue crack growth resistance in twinning-induced plasticity steels
Source abstract
Abstract
Abstract The tensile, high-cycle fatigue (HCF) and fatigue crack growth (FCG) rate tests of Fe-30Mn-0.9C and Fe-30Mn-0.3C twinning-induced plasticity (TWIP) steels were performed. Meanwhile, the corresponding surface damages, fatigue fracture morphologies and microstructure evolutions were also investigated. It is detected that both the fatigue strength and FCG resistance of Fe-30Mn-0.9C steel are higher than those of Fe-30Mn-0.3C steel, because Fe-30Mn-0.9C steel possesses higher yield strength, plasticity and slip planarity than Fe-30Mn-0.3C steel. Furthermore, it is proposed that, for the Fe-Mn-C TWIP steel, increasing the C content to enhance the short range order (SRO) would lead to the synchronous increment in the fatigue strength and FCG resistance. This study may have a certain guiding significance for the selection of materials to against fatigue fracture.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Fatigue and fracture mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (44)
Show source-provided references
1. Fatigue crack growth behavior of a coarse- and a fine-grained high manganese austenitic twin-induced plasticity steel10.1016/j.msea.2014.03.035 ↗
2. Low-cycle and extremely-low-cycle fatigue behaviors of high-Mn austenitic TRIP/TWIP alloys: property evaluation, damage mechanisms and life prediction10.1016/j.actamat.2015.11.015 ↗
3. Suresh · 1991
4. On some basic problems of fatigue research in engineering10.1016/S0142-1123(01)00040-8 ↗
5. Lee · 2005
6. General relation between tensile strength and fatigue strength of metallic materials10.1016/j.msea.2012.11.103 ↗
7. Relations between fatigue strength and other mechanical properties of metallic materials10.1111/ffe.12158 ↗
8. Near-threshold fatigue: a review10.1016/S0142-1123(99)00053-5 ↗
9. About the fatigue crack propagation threshold of metals as a design criterion-A review10.1016/j.engfracmech.2015.12.002 ↗
10. Microstructural evolution and mechanical properties of Cu-Al alloys subjected to equal channel angular pressing10.1016/j.actamat.2008.12.002 ↗
11. Effects of stacking fault energy on the thermal stability and mechanical properties of nanostructured Cu-Al alloys during thermal annealing10.1557/jmr.2010.39 ↗
12. Microscopic mechanisms contributing to the synchronous improvement of strength and plasticity (SISP) for TWIP copper alloys10.1038/srep09550 ↗
13. Strain rate effects on tensile deformation behaviors for Fe-22Mn-0.6C-(1.5Al) twinning-induced plasticity steel10.1016/j.msea.2014.04.043 ↗
14. On the relationship between the twin internal structure and the work-hardening rate of TWIP steels10.1016/j.scriptamat.2010.07.016 ↗
15. Influence of addition elements on the stacking-fault energy and mechanical properties of an austenitic Fe-Mn-C steel10.1016/j.msea.2006.12.170 ↗
16. High manganese austenitic twinning induced plasticity steels: a review of the microstructure properties relationships10.1016/j.cossms.2011.04.002 ↗
17. Fatigue behavior of four high-Mn twinning induced plasticity effect steels10.1007/s11661-010-0193-7 ↗
18. Improving the high-cycle fatigue lives of Fe-30Mn-0.9C twinning-induced plasticity steel through pre-straining10.1007/s11661-015-3010-5 ↗
19. High-cycle fatigue behavior of ultrafine-grained austenitic stainless and TWIP steels10.1016/j.msea.2010.05.035 ↗
20. Enhancing high-cycle fatigue properties of cold-drawn Fe-Mn-C TWIP steels10.1016/j.ijfatigue.2015.12.007 ↗
21. High-cycle fatigue properties and damage mechanisms of pre-strained Fe-30Mn-0.9C twinning-induced plasticity steel10.1016/j.msea.2016.10.043 ↗
22. Fatigue crack growth-Microstructure relationships in a high-manganese austenitic TWIP steel10.1016/j.msea.2009.12.012 ↗
23. Effect of chemical composition on work hardening of Fe-Mn-C TWIP steels10.1179/026708309X12535382371852 ↗
24. Extremely-low-cycle fatigue behaviors of Cu and Cu-Al alloys: damage mechanisms and life prediction10.1016/j.actamat.2014.10.002 ↗
25. Fatigue crack propagation in trip steels10.1007/BF02644242 ↗
26. Solute cluster size effect on the fatigue crack propagation resistance of an underaged Al-Cu-Mg alloy10.1016/j.ijfatigue.2015.11.023 ↗
27. Effect of microstructure on the fatigue crack growth behavior of Cu-Be-Co-Ni alloy10.1016/j.jallcom.2015.12.017 ↗
28. Influence of grain structure and crystallographic orientation on fatigue crack propagation behavior of 7050 alloy thick plate10.1016/j.ijfatigue.2014.03.009 ↗
29. Research on fatigue crack propagation behaviour of 4003 ferritic stainless steel based on infrared thermography10.1111/ffe.12352 ↗
30. Evolution of dislocations and twins in high cycle fatigue of a twinning-induced plasticity steel10.1016/j.msea.2015.09.017 ↗
31. Cyclic slip irreversibility and fatigue life: a microstructure-based analysis10.1016/j.actamat.2012.10.029 ↗
32. Improved fatigue properties of ultrafine-grained copper under cyclic torsion loading10.1016/j.actamat.2013.06.032 ↗
33. Fundamental factors on formation mechanism of dislocation arrangements in cyclically deformed fcc single crystals10.1016/j.pmatsci.2010.12.001 ↗
34. On the origin of planar slip in fcc alloys10.1016/0001-6160(89)90143-0 ↗
35. Dislocation emission and fatigue crack growth threshold10.1016/0956-7151(91)90304-J ↗
36. A transgranular fatigue-crack growth-model based on restricted slip reversibility10.1007/BF02668205 ↗
37. Effect of aging treatments on the kinetics of fatigue crack growth in 7010 aluminum alloy10.1016/j.msea.2006.07.063 ↗
38. Microstructure and fatigue crack growth in a γ-Fe-Ni-Al alloy10.1016/0001-6160(76)90104-8 ↗
39. Influence of precipitates on low-cycle fatigue and crack growth behavior in an ultrafine-grained aluminum alloy10.1016/j.actamat.2014.07.061 ↗
40. Predicting fatigue resistance of nano-twinned materials: part II-Effective threshold stress intensity factor range10.1016/j.ijfatigue.2014.06.006 ↗
41. Effect of laser peening and shot peening on fatigue striations during FCGR study of Ti6Al4V10.1016/j.ijfatigue.2016.08.005 ↗
42. Relationship of the spacing of the fatigue striations to the range in the stress intensity factor10.1007/BF01150631 ↗
43. Comparison of work hardening and deformation twinning evolution in Fe-22Mn-0.6C (1.5Al) twinning-induced plasticity steels10.1016/j.scriptamat.2013.02.060 ↗
44. Modelling of TWIP effect on work-hardening10.1016/S0921-5093(00)02019-0 ↗