High temperature superplasticity and deformation behavior of naturally aged Zn-Al alloys with different phase compositions
Source abstract
Abstract
Abstract Two Zn-Al alloys, eutectoid Zn-22Al and dilute Zn-0.3Al, were processed through equal-channel angular pressing (ECAP). The ECAP-processed alloys were subjected to long-term natural aging at room temperature for 120 days in order to investigate the effect of long-term natural aging on high-temperature superplasticity and the deformation behavior of these alloys. The grain size of the Zn-22Al alloy increased from 200 nm after ECAP to 400 nm after the natural aging process. The Zn-0.3Al alloy with a grain size of 1.3 µm after ECAP demonstrated a reasonably stable microstructure with the grain size of ~ 1.7 µm after long-term natural aging. The naturally aged ultrafine-grained (UFG) Zn-22Al alloy showed an excellent superplastic elongation of about 1800% at 200 °C. Grain boundary sliding was determined as the dominant deformation mechanism in this alloy. On the contrary, a considerably low elongation to failure of 230% was recorded in the naturally aged fine-grained (FG) Zn-0.3Al alloy at 150 °C, and dislocation creep was evaluated as the main deformation mechanism for this alloy. Detailed microstructural analyses showed that the FG Zn-0.3Al alloy was exposed to grain boundary corrosion during the natural aging process due to the presence of Al precipitates at grain boundaries whereas such formation was not observed in the UFG Zn-22% Al alloy. Grain boundary sliding was hindered by grain boundary corrosion and the cavity nucleation at the corroded grain boundaries caused a premature failure leading to such a low elongation in the Zn-0.3Al alloy.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Microstructure and mechanical properties · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (52)
Show source-provided references
1. Seventy-five years of superplasticity: historic developments and new opportunities10.1007/s10853-009-3780-5 ↗
2. Kaibyshev · 1992
3. Principles of equal-channel angular pressing as a processing tool for grain refinement10.1016/j.pmatsci.2006.02.003 ↗
4. Cook · 1968
5. Superplastic deformation of a fine-grained Zn–0.3 wt% Al alloy at room temperature10.1016/S0921-5093(00)01952-3 ↗
6. Effect of equal-channel angular pressing on room temperature superplasticity of quasi-single phase Zn–0.3Al alloy10.1016/j.msea.2015.07.041 ↗
7. A study on the superplasticity of Zn-Al alloy using dynamic materials model10.5228/KSPP.2009.18.4.317 ↗
8. Superplastic deformation behavior of Zn-0.3 wt% Al alloy fabricated by ECAP10.5228/KSPP.2009.18.6.448 ↗
9. Naziri · 1972
10. Superplasticity in a Zn-1.1 wt% A1 alloy, I. The influence of strain rate10.1007/BF01597631 ↗
11. Superplasticity in a coarse-grained Zn-1.1 wt% A1 alloy10.1007/BF01605414 ↗
12. Achieving room temperature superplasticity in Zn-5Al alloy at high strain rates by equal-channel angular extrusion10.1016/j.jallcom.2014.10.111 ↗
13. Improvement of room-temperature superplasticity in Zn–22 wt% Al alloy10.1016/j.msea.2007.07.100 ↗
14. Capability of superplastic forming in the seismic device using Zn–22Al eutectoid alloy10.1016/S1359-6462(03)00328-2 ↗
15. Significance of Si impurities on exceptional room-temperature superplasticityin a high-purity Zn-22%Al alloy10.1016/j.msea.2015.07.087 ↗
16. Superplasticity at room temperature in Zn-22Al alloy processed by equal-channel-angular extrusion10.2320/matertrans.45.1261 ↗
17. Mechanical characteristics of a Zn–22% Al alloy processed to very high strains by ECAP10.1016/j.msea.2006.05.044 ↗
18. Characterization of deformation processes in a Zn-22% Al alloy using atomic force microscopy10.1023/A:1021071228521 ↗
19. Achieving high strain rate superplasticity via severe plastic deformation processing10.1007/s10853-008-2909-2 ↗
20. Improvement of high strain rate and room temperature superplasticity in Zn–22Al alloy by two-step equal-channel angular pressing10.1016/j.msea.2014.09.114 ↗
21. Effect of different processes on lamellar-free ultrafine grain formation, room temperature superplasticity and fracture mode of Zn-22Al alloy10.1016/j.jallcom.2015.12.142 ↗
22. Microstructural characteristics and superplastic ductility in a Zn-22% Al alloy with submicrometer grain size10.1016/S0921-5093(97)00481-4 ↗
23. Grain boundary sliding in a superplastic zinc-aluminum alloy processed using severe plastic deformation10.2320/matertrans.ME200720 ↗
24. Developing superplasticity and a deformation mechanism map for the Zn–Al eutectoid alloy processed by high-pressure torsion10.1016/j.msea.2011.04.053 ↗
25. Factors influencing ductility in the superplastic Zn-22 pct AI eutectoid10.1007/BF02661575 ↗
26. Nieh · 1997
27. The significance of self-annealing in two-phase alloys processed by high-pressure torsion10.1088/1757-899X/63/1/012126 ↗
28. Effect of natural aging on RT and HSR superplasticity of ultrafine grained Zn-22Al alloy
29. The influence of Cd on the superplasticity of Zn-A1 alloys10.1007/BF01604797 ↗
30. O.A. Kaibyshev, Sverkhplastichnost' Promyshlennykh Splavov (Superplasticity of Commercial Alloys), Metallurgia, Moscow. (In Russian), 1984.
31. The shearing characteristics associated with equal-channel angular pressing10.1016/S0921-5093(98)00750-3 ↗
32. Creep at low stress levels in the superplastic Zn-22% Al eutectoid10.1016/0001-6160(75)90076-0 ↗
33. Achieving high superplasticity of a new Al–Mg–Sc–Zr alloy sheet prepared by a simple thermal–mechanical process10.1016/j.msea.2015.08.052 ↗
34. Excellent superplasticity and deformation mechanism of Al–Mg–Sc–Zr alloy processed via simple free forging10.1016/j.msea.2014.11.054 ↗
35. Hot tensile deformation and fracture behaviors of AZ31 magnesium alloy10.1016/j.matdes.2013.01.023 ↗
36. Fracture behavior of AZ31 magnesium alloy during low-stress high-temperature deformation10.1007/s13632-015-0189-1 ↗
37. An investigation of cavity development during superplastic flow in a zinc-aluminum alloy processed using severe plastic deformation10.2320/matertrans.MD201106 ↗
38. The mechanism of intergranular corrosion of dilute zinc aluminum alloys in hot water10.1016/0010-938X(76)90050-0 ↗
39. A unified approach to grain boundary sliding in creep and superplasticity10.1016/0956-7151(94)90322-0 ↗
40. Principles of superplasticity in ultrafine-grained materials10.1007/s10853-006-0954-2 ↗
41. The activation energies associated with superplastic flow10.1016/0001-6160(75)90153-4 ↗
42. Neck formation and cavitation in the superplastic Zn-22% Al eutectoid10.1007/BF00611474 ↗
43. Deformation mechanism maps for superplastic materials10.1016/0036-9748(76)90358-6 ↗
44. Superplastic deformation behavior in commercial and high purity Zn-22 pct AI10.1007/BF02645809 ↗
45. Achieving high strain rate superplasticity of an Al-Mg-Sc-Zr alloy by a new asymmetrical rolling technology10.1016/j.msea.2016.06.070 ↗
46. Superplastic behavior and microstructure evolution of a new Al-Mg-Sc-Zr alloy subjected to a simple thermomechanical processing10.1016/j.msea.2016.05.086 ↗
47. Low temperature quasi-superplasticity of ZK60 alloy prepared by reciprocating extrusion10.1016/S1003-6326(11)61168-0 ↗
48. Microstructural evolution and mechanical, and corrosion property evaluation of Cu–30Ni alloy formed by Direct Metal Deposition process10.1016/j.jallcom.2011.03.091 ↗
49. The development of internal cavitation in a superplastic zinc–aluminum alloy processed by ECAP10.1007/s10853-008-2771-2 ↗
50. Micrograin Superplasticity: characteristics and utilization10.3390/ma4061194 ↗
51. Effects of aging treatment on the intergranular corrosion behavior of Al–Cu–Mg–Ag alloy10.1016/j.jallcom.2015.03.174 ↗
52. Intergranular corrosion failure in Zn-Al alloy solenoid valve seats