journal article·2019-05

Microstructural evolution and growth kinetics of interfacial compounds in TiAl/Ti3SiC2 diffusion bonding joints

Qi Wang, Guo-qing Chen, Kang Wang, Xue-song Fu, Wen-long Zhou

Publisher page

Abstract

Abstract TiAl intermetallic was direct diffusion bonded to Ti3SiC2 at 900 °C, 950 °C, and 1000 °C with a holding time ranging from 0.25 h to 64 h. The interfacial microstructural evolution, the growth kinetics and the mechanical properties of the bonded TiAl/Ti3SiC2 joints were systematically investigated. The build-up of interfacial compounds in the TiAl/Ti3SiC2 joints changed from γ+α2/γ/Ti5Si3/Ti3SiC2 to γ+α2/γ/TiAl2/Ti5Si3/Ti3SiC2, to γ+α2/γ/TiAl2/Ti5Si4/Ti5Si3/Ti3SiC2, and to γ+α2/γ/TiAl2/TiAl3+Ti5Si3/Ti5Si4/Ti5Si3/Ti3SiC2 as the holding time or bonding temperature increased. The formation sequence of interfacial phase at the joint was: Ti5Si3→Ti5Si4→TiAl2→TiAl3. The de-intercalation Si atoms from the Ti3SiC2 diffusing into the TiAl base alloy and reacting with the Ti was responsible for the formation of the interfacial reaction layers. The thicknesses of the interfacial reaction layers grew following the parabolic kinetic law, indicated their growth was controlled by the bulk diffusion. The bonding activation energy was 213 kJ/mol. The joint, bonded at 900 °C for 9 h, had the highest shear strength (about 53 MPa) with a γ+α2/γ/TiAl2/Ti5Si4/Ti5Si3/Ti3SiC2 interfacial microstructure and with a total thickness of 6 μm.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: MXene and MAX Phase Materials · Intermetallics and Advanced Alloy Properties · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. The MN+1AXN phases: a new class of solids10.1016/S0079-6786(00)00006-6 ↗
2. The morphology of oxides and oxidation behavior of Ti3SiC2-based composite at high-temperature10.1016/S0266-3538(02)00285-3 ↗
3. Synthesis and characterization of a remarkable ceramic: Ti3SiC210.1111/j.1151-2916.1996.tb08018.x ↗
4. Solid combustion synthesis of Ti3SiC210.1016/0955-2219(89)90022-8 ↗
5. Progress in research and development on MAX phases: a family of layered ternary compounds10.1179/1743280410Y.0000000001 ↗
6. Ti3SiC2 as a candidate material for lead cooled fast reactor10.1016/j.nucengdes.2010.07.038 ↗
7. Mechanical damping in porous Ti3SiC210.1016/j.actamat.2006.06.052 ↗
8. Ordered intermetallic alloys, part III: gamma titanium aluminides10.1007/BF03220745 ↗
9. High-temperature structural intermetallics10.1016/S1359-6454(99)00301-8 ↗
10. Gamma titanium aluminide alloys—an assessment within the competition of aerospace structural materials10.1016/S0921-5093(98)01158-7 ↗
11. Application of TiAl in a turbocharger for passenger vehicles10.1002/1527-2648(200105)3:5<307::AID-ADEM307>3.0.CO;2-3 ↗
12. Wrought TiAl blades10.1016/j.matpr.2015.05.024 ↗
13. Diffusion bonding of ceramics10.1007/BF00554019 ↗
14. Diffusion bonding of intermetallic compound tial10.2355/isijinternational.31.1260 ↗
15. Phase and morphology evolution in high-temperature Ti3SiC2-NiTi diffusion-bonded joints10.1016/j.scriptamat.2011.04.015 ↗
16. Joining of Ti3SiC2 with Ti–6Al–4V alloy10.1557/JMR.2002.0010 ↗
17. Diffusion bonding of TiAl intermetallic and Ti3AlC2 ceramic: interfacial microstructure and joining properties10.1016/j.matdes.2013.10.074 ↗
18. Interfacial study of NiTi–Ti3SiC2 solid state diffusion bonded joints10.1016/j.msea.2014.10.033 ↗
19. Evaluation on diffusion bonded joints of TiAl alloy to Ti3SiC2 ceramic with and without Ni interlayer: interfacial microstructure and mechanical properties10.1016/j.matdes.2014.01.029 ↗
20. Fabrication and characterization of NiTi/Ti3SiC2 and NiTi/Ti2AlC composites10.1016/j.jallcom.2014.04.224 ↗
21. Sliding speed and load dependence of tribological properties of Ti3SiC2/TiAl composite10.1080/10402004.2014.951748 ↗
22. Microstructure evolution, mechanical and tribological properties of Ti3(Al,Sn)C2/Al2O3 composites10.1016/j.jeurceramsoc.2018.01.029 ↗
23. Reaction synthesis of Ti3SiC2 phase in plasma sprayed coating10.1016/j.jallcom.2009.04.079 ↗
24. Improved mechanical properties of Al2O3 ceramic by in-suit generated Ti3SiC2 and TiC via hot pressing sintering10.1016/j.ceramint.2017.04.165 ↗
25. Study of the interfacial reaction between Ti3SiC2 particles and Al matrix10.1016/j.jallcom.2017.12.123 ↗
26. Rapid synthesis of ternary carbide Ti3SiC2 through pulse-discharge sintering technique from Ti/Si/TiC powders10.1007/s11661-002-0320-1 ↗
27. Bifurcation of the Kirkendall marker plane and the role of Ni and other impurities on the growth of Kirkendall voids in the Cu–Sn system10.1016/j.actamat.2017.03.068 ↗
28. Interdiffusion and the Kirkendall effect in binary systems
29. Intermetallic formation and mechanical properties of Ni-Ti diffusion couples10.1016/j.matdes.2017.05.055 ↗
30. First-principles study of Ti3AC2 (A=Si, Al) (001) surfaces10.1016/j.actamat.2007.04.033 ↗
31. General trend of the mechanical properties of the ternary carbides M3SiC2 (M=transitionmetal)10.1103/PhysRevB.74.054106 ↗
32. Decohesion of Ti3SiC2 induced by He impurities10.1016/j.matlet.2012.05.093 ↗
33. Role of nanolaminated crystal structure on the radiation damage tolerance of Ti3SiC2: theoretical investigation of native point defects10.1155/2013/831590 ↗
34. Interfacial reaction between Cu and Ti2SnC during processing of Cu-Ti2SnC composite10.3139/146.101181 ↗
35. A novel route to prepare a Ti3SnC2/Al2O3 composite10.1016/j.scriptamat.2017.01.013 ↗
36. Diffusion pattern in MSi2 and M5Si3 silicides in group VB (M = V, Nb, Ta) and VIB (M = Mo, W) refractory metal-silicon systems10.1080/14786435.2014.888103 ↗
37. Thermodynamic investigation on phase formation in the Al–Si rich region of Al–Si–Ti system10.1016/j.matdes.2016.03.144 ↗
38. Self-diffusion in γ-TiAl: an experimental study and atomistic calculations10.1016/S0966-9795(98)00117-4 ↗
39. Experimental investigation and thermodynamic calculation of the titanium-silicon-carbon system10.1111/j.1151-2916.2000.tb01170.x ↗
40. Degrees C isothermal section of the Al-Ti-Si ternary phase diagram10.1007/s11669-014-0325-7 ↗
41. The diffusion couple technique in phase diagram determination10.1016/S0925-8388(00)01487-0 ↗
42. Growth kinetics of planar binary diffusion couples: “Thin-film case” versus “bulk cases”10.1063/1.331028 ↗
43. Reactivity of Zircaloy-4 with Ti3SiC2 and Ti2AlC in the 1100–1300 °C temperature range10.1016/j.jnucmat.2015.02.006 ↗
44. Microstructure and mechanical behavior of reaction hot-pressed titanium silicide and titanium silicide-based alloys and composites10.1007/s11661-998-0086-1 ↗
45. Thermal expansion of the Ti5Si3 and Ti6Si2B phases investigated by high-temperature X-ray diffraction10.1016/j.intermet.2005.05.007 ↗
46. Thermal expansion of select Mn+1AXn (M=earlytransitionmetal, A=A group element, X=C or N) phases measured by high temperature x-ray diffraction and dilatometry10.1063/1.3021465 ↗
47. Elastic constants and thermal expansion of single crystal gamma-TiAl from 300 to 750 K10.1016/S0921-5093(97)00575-3 ↗
48. Microstructure and mechanical strength of diffusion-bonded Ti3SiC2/Ni joints10.1557/jmr.2006.0290 ↗
49. Direct diffusion bonding of Ti3SiC2 and Ti3AlC210.1016/j.materresbull.2008.12.002 ↗