The role of Sn element on the deformation mechanism and precipitation behavior of the Al–Cu–Mg alloy
Source abstract
Abstract
Abstract The deformation mechanism and precipitation behavior of Al-5.8Cu-0.35 Mg-(0.3Sn) (wt.%) alloys were intensively investigated by microstructure characterizations and mechanical tests in this work. The experimental results showed that the added Sn elements can induce profound impacts on the alloys in three manners: (1) the formation of Mg2Sn particles with excellent thermal stability can create particle-stimulated nucleation effect to facilitate dynamic recrystallization during hot deformation. Furthermore, the fine Mg2Sn particles distributed at subgrain boundaries obviously inhibited the recrystallized grain growth during the solution treatment; (2) the suppression of natural aging was because there was insufficient releasing of vacancies from Sn-vacancy clusters at room temperature; (3) the accelerated artificial aging with lowered hardening effect was owing to both Sn-vacancy clusters inhibited the annihilation of quenching vacancies and reduced concentration of solute Mg consumed by the stable Mg2Sn particles. Finally, the underlying mechanisms were elucidated in combination microstructure features with mechanical responses in the alloys.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (62)
Show source-provided references
1. Effects of solution treatment on the microstructure and mechanical properties of Al–Cu–Mg–Ag alloy10.1016/j.matdes.2010.04.058 ↗
2. Effect of plastic deformation on the ageing behavior of an Al–Cu–Mg alloy with a high Cu/Mg ratio10.1016/j.msea.2018.09.017 ↗
3. Unique hybrid precipitate structures forming in an Al–Cu–Mg–Si alloy10.1016/j.jallcom.2020.153977 ↗
4. Improved structural homogeneity and mechanical properties of nanoparticles reinforced Al composites after orthogonal thermomechanical processes10.1016/j.jallcom.2018.07.083 ↗
5. A model of continuous dynamic recrystallization10.1016/S1359-6454(03)00078-8 ↗
6. Suwas · 2014
7. Effects of nanosized particles on microstructure and mechanical properties of an aged in-situ TiB2/Al–Cu–Li composite10.1016/j.msea.2018.11.032 ↗
8. Microstructure and texture evolution during annealing a cryogenic-SPD processed Al–alloy with a nanoscale lamellar HAGB grain structure10.1016/j.actamat.2009.04.010 ↗
9. Influence of particle stimulated nucleation on the recrystallization textures in cold deformed Al–alloys Part I-Experimental observations10.1016/S1359-6462(97)00315-1 ↗
10. Structural evolution and the Hall–Petch relationship in an Al–Mg–Li–Zr alloy with ultra-fine grain size10.1016/S1359-6454(97)00120-1 ↗
11. The effect of pre-deformation on the precipitation behavior of AlCuMg(Si) alloys with low Cu/Mg ratios10.1016/j.jallcom.2020.153831 ↗
12. Precipitation processes in Al–Cu–Mg–Sn and Al–Cu–Mg–Sn–Ag10.1016/j.matdes.2016.02.048 ↗
13. Transmission electron microscopy study of the evolution of precipitates in aged Al–Li–Cu alloys: the θ′ and T1 phases10.1016/S1359-6454(03)00253-2 ↗
14. Influence of Sc content on the microstructure and mechanical properties of cast Al–2Li–2Cu–0.5Mg–0.2Zr alloy10.1016/j.matchar.2018.05.046 ↗
15. Microstructure characteristics of an ultra-high strength extruded Al–4.7Cu–1Li–0.5Mg–0.1Zr–1Zn alloy during heat treatment10.1016/j.jallcom.2019.152216 ↗
16. The effect of Ge addition on Al–3.5Cu–0.4Mg (wt.%) alloy10.1016/j.scriptamat.2011.12.011 ↗
17. Solute clustering and solute nanostructures in an Al–3.5Cu–0.4Mg–0.2Ge alloy10.1016/j.actamat.2013.03.004 ↗
18. Quantitative study of the solute clustering and precipitation in a pre-stretched Al–Cu–Mg–Ag alloy10.1016/j.jallcom.2017.07.258 ↗
19. Effect of pre-straining on the aging behavior and mechanical properties of an Al–Cu–Mg–Ag alloy10.1016/j.msea.2014.11.094 ↗
20. Microstructure of two-phase Al–1.7at%Cu alloy deformed by equal-channel angular pressing10.1016/S1359-6454(00)00308-6 ↗
21. Quench sensitivity in a dispersoid-containing Al–Mg–Si Alloy10.1007/s11661-019-05130-2 ↗
22. Internal co-precipitation in aged Al–1.7Cu–0.3Mg–0.1Ge (at.%) alloy10.1016/j.actamat.2007.12.032 ↗
23. Precipitation strengthening of aluminum alloys by room-temperature cyclic plasticity10.1126/science.aav7086 ↗
24. Solute-vacancy binding in aluminum10.1016/j.actamat.2007.06.039 ↗
25. Hardening of Al–Mg–Si alloys: effect of trace elements and prolonged natural aging10.1016/j.matdes.2016.06.014 ↗
26. Dislocation loops in quenched aluminium10.1080/14786435808237028 ↗
27. High temperature deformation behavior of Al–Cu–Mg alloys micro-alloyed with Sn10.1016/j.msea.2010.01.052 ↗
28. Nucleation and growth of θ′ precipitation in Sn-modified Al–Cu alloys: APFIM/TEM observations10.1016/0169-4332(94)00514-1 ↗
29. Shu · 2012
30. In situ natural ageing of Al–Cu–(Mg) alloys: the effect of in and Sn on the very early stages of decomposition10.1016/j.scriptamat.2019.04.031 ↗
31. Microstructure, mechanical properties and corrosion behavior of Al–Cu–Mg–Sn–Ga–In alloy10.1016/j.jallcom.2018.10.290 ↗
32. Effects of Mg2Sn intermetallic on the microstructure and tensile properties of Al–15%Mg2Si–X% Sn composite10.1557/jmr.2016.426 ↗
33. Prediction of hot deformation behavior of Al–5.9%Cu–0.5%Mg alloys with trace additions of Sn10.1007/s10853-011-5873-1 ↗
34. Aluminium alloys on the basis of Al-Cu-Mg, lead-free, intended for cutting10.4028/www.scientific.net/MSF.396-402.1641 ↗
35. Structures and tensile properties of Sc-containing 1445 Al–Li alloy sheet10.1016/j.jallcom.2018.03.032 ↗
36. Continuous dynamic recrystallization in an Al–Li–Mg–Sc alloy during equal-channel angular extrusion10.1016/j.msea.2005.01.053 ↗
37. Dynamic dissolution and texture evolution of an Al–Cu–Mg–Ag alloy during hot rolling10.1016/j.jallcom.2020.154254 ↗
38. Annealing response of binary Al–7Mg alloy deformed by equal channel angular pressing10.1016/j.msea.2013.08.039 ↗
39. Continuous dynamic recrystallization in an Al–Li–Mg–Sc alloy during equal-channel angular extrusion10.1016/j.msea.2005.01.053 ↗
40. The development of microstructure in Al–5%Mg during high temperature deformation10.1016/0001-6160(86)90171-9 ↗
41. A new etching technique for revealing the plastic deformation zone in an Al–Cu–Mg alloy10.1007/s10853-008-2544-y ↗
42. Strength, deformation, fracture behaviour and ductility of aluminium–lithium alloys10.1007/BF00585420 ↗
43. Effect of Sn and in on the natural ageing kinetics of Al–Mg–Si alloys
44. Synergy effect of Si addition and pre-straining on microstructure and properties of Al–Cu–Mg alloys with a medium Cu/Mg ratio10.1016/j.msea.2019.138429 ↗
45. A predictive mechanism for dynamic strain ageing in aluminium–magnesium alloys10.1038/nmat1765 ↗
46. Evolution of θ′ precipitate in aluminum alloy 2519A impacted by split Hopkinson bar
47. Vacancy-tuned precipitation pathways in Al–1.7Cu–0.025In–0.025Sb (at.%) alloy10.1016/j.actamat.2017.09.025 ↗
48. Ageing response of cold-rolled Al–Cu–Mg alloy10.1016/j.msea.2020.139148 ↗
49. The magic thicknesses of θ′ precipitates in Sn-microalloyed Al–Cu10.1016/j.actamat.2011.10.015 ↗
50. Size-dependent diffusion controls natural aging in aluminium alloys
51. Vacancy concentration in Al–Mg solid solutions10.1016/j.scriptamat.2007.03.014 ↗
52. The effect of silver on microstructural evolution in two 2 xxx series Al–alloys with a high Cu:Mg ratio during ageing to a T8 temper10.1016/j.msea.2008.03.014 ↗
53. Strengthening potential of the cubic precipitate in Al–Cu–Mg–Si alloys10.1007/BF00356599 ↗
54. Role of silicon in the formation of the (Al5Cu6Mg2) σ phase in Al–Cu–Mg alloys10.1023/A:1004767131956 ↗
55. Characterization of a cubic phase in an Al–Cu–Mg–Ag alloy10.1023/A:1018675029786 ↗
56. Effect of ageing time on strength and microstructures of an Al–Cu–Li–Zn–Mg–Mn–Zr alloy10.1016/j.msea.2008.08.001 ↗
57. The effect of long term creep exposure on the microstructure and properties of an underaged Al–Cu–Mg–Ag alloy10.1016/j.scriptamat.2004.02.001 ↗
58. The precipitate Ω phase in Al–Cu–Mg–Ag alloys10.1016/0001-6160(89)90005-9 ↗
59. Microstructural design of high-strength aluminum alloys10.1361/105497198770341734 ↗
60. Precipitation of the Ω phase in an Al–4.0Cu–0.5Mg alloy, scripta metal
61. Evolution of Ω phase in an Al–Cu–Mg–Ag alloy: a three-dimensional atom probe study10.1016/S1359-6454(98)00280-8 ↗
62. Precipitation of the Ω phase in 2024 and 2124 aluminium alloys10.1016/S1359-6462(99)00150-5 ↗