Mechanical property of induction brazing TiAl-based intermetallics to steel 35CrMo using AgCuTi filler metal
Source abstract
Abstract
Abstract TiAl-based intermetallics joined by vacuum induction brazing using Ag–Cu35.2–Ti1.8 filler alloy at 850–970 °C for 1–10 min was investigated. The optimum brazing parameters are as follows: brazing temperature is 870–880 °C, brazing time is 4–6 min. The maximum tensile strength of the joint is 320 MPa for the specimen induction brazed at for 870 °C for 5 min, and at this time, the thickness of Al–Cu–Ti intermetallic compound layer is about one third of that of the whole interface. Interfacial microstructure of TiAl/Ag–Cu–Ti/35CrMo joint brazed at 870 °C for 5 min is instable at 400 °C. The instantaneous high temperature strength is 248 MPa at 400 °C, the fracture location of joint is mainly at Al–Cu–Ti intermetallic compound layer, the fracture pattern of brazed joint deviate from transcrystalline crack at room temperature into intergranular crack.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Advanced materials and composites · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. Chesnult · Met. Mater. · 1990 · 6 · 509
2. Westbrook · 1995 · vol. 2
3. Noda · Intermetallics · 1998 · 12 · 70910.1016/S0966-9795(98)00060-0 ↗
4. Narita · Intermetallics · 2000 · 4 · 37110.1016/S0966-9795(99)00117-X ↗
5. Yang · Met. Powder Rep. · 1997 · 12 · 42
6. Medda · Mater. Sci. Eng. A · 2003 · 11 · 2310.1016/S0921-5093(03)00566-5 ↗
7. David · Weld. J. Res. Suppl. · 1990 · 4 · 133s
8. P.L. Threadgill, W.A. Baeslack III, Proceedings of the International Symposium on Intermetallic Compounds, Sendai, Japan, 17–20 June 1991, pp. 1021–1025.
9. W.A. Baeslack III, Proceedings of the Symposium on Weldability of Materials, ASM Fall Meeting, Detroit, September 1990, pp. 247–2581.
10. Baeslack · Weld. J. Res. Suppl. · 1989 · 483s
11. Baeslack · Scripta Met. · 1988 · 22 · 115510.1016/S0036-9748(88)80122-4 ↗
12. He · Trans. Nonferr. Met. Soc. China · 2002 · 12 · 1069
13. N. Ridley, D.W. Livesey, M.T. Salehi, Proceedings of the International Conference on High Temperature Intermetallics, London, 30 April–1 May 1991, pp. 198–200.
14. He · Mater. Charact. · 2003 · 50 · 8710.1016/S1044-5803(03)00122-0 ↗
15. Shiue · Intermetallics · 2003 · 66110.1016/S0966-9795(03)00077-3 ↗
16. Shiue · Acta Mater. · 2003 · 199110.1016/S1359-6454(02)00606-7 ↗
17. Chan · Int. J. Refract. Met. Hard Mater. · 2004 · 2710.1016/j.ijrmhm.2003.11.002 ↗