journal article·2017-01

Evaluation of hydrogen induced damage of steels by different test methods

G. Rosenberg, I. Sinaiova

Publisher page

Abstract

Abstract The deleterious effect of hydrogen on mechanical properties of microalloyed pipeline (X70) and structural (S355) hot rolled steel strips was evaluated by static tensile testing of smooth and notched specimens (flat specimens with a central hole) and Charpy V impact testing. Hydrogen induced changes of the fatigue crack growth behavior were also examined. Most of the tests were performed on specimens exposed to the ageing for 4-years as well as on specimens who were after four years of ageing electrolytically charged with hydrogen. The comparison of mechanical properties of both studied steels before and after hydrogen charging showed that the degradation effect of hydrogen may or may not be detected, depending on the conditions of testing. The effect of hydrogen on the development of local plastic strain during deformation and fracture process as well as plastic zone size around the holes, notches and cracks observed on surface specimens was studied by differential interference contrast in optical microscope. The most important result of this work was the finding that the plastic zone size at the tip of the growing fatigue crack observed on the surface of hydrogenated specimens was significantly larger than for nonhydrogenated specimens.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Nuclear Materials and Properties · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (100+)

Show source-provided references
1. H.J.Goldschmid, Interstitial Alloys, Butterworths, London, 1967, pp. 71-78.10.1007/978-1-4899-5880-8 ↗
2. Elements of Metallurgy And Engineering Alloys, in: F.C. Campbel (Ed.), ASM International, Materials Park, Ohio, ASM International, 2008, p. 154.
3. Comparative study of solubilities of hydrogen, nitrogen and carbon in α-iron10.1007/BF00547962 ↗
4. Effect of long-term service on the tensile properties and capability of pipeline steel 17GS to resist cleavage fracture10.1016/j.ijpvp.2004.02.015 ↗
5. High-cycle fatigue failure of low-carbon steel after long-term aging10.1134/S0020168510140190 ↗
6. Effect of natural aging on the microstructural regions, mechanical properties, corrosion resistance and fracture in welded joints on API5L X52 steel pipeline
7. Hydrogen-induced softening and hardening in high purity iron10.1016/0025-5416(82)90055-6 ↗
8. A critical review of the influence of hydrogen on the mechanical properties of medium-strength steels10.1515/corrrev-2013-0023 ↗
9. Effect of cathodic hydrogen-charging current density on mechanical properties of prestrained high strength steels10.1016/j.msea.2015.06.003 ↗
10. Role of microstructure, composition and hardness in resisting hydrogen embrittlement of fastener grade steels10.1016/j.corsci.2009.12.020 ↗
11. Characterization of hydrogen embrittlement in automotive advanced high strength steels10.1002/mawe.201100917 ↗
12. Effect of tempering and baking on the charpy impact energy of hydrogen-charged 4340 Steel10.1007/s11665-014-1268-1 ↗
13. Recent developments in the study of hydrogen embrittlement: Hydrogen effect on dislocation nucleation10.1016/j.actamat.2010.05.057 ↗
14. Hydrogen embrittlement and rock bolt stress corrosion cracking10.1016/j.engfailanal.2008.01.004 ↗
15. Hydrogen embrittlementin HSSs limits use in lightweight body
16. A quantitative analysis of hydrogen traping on hydrogen10.1007/BF02648348 ↗
17. Influence of experimental parameters on thermal desorption spectroscopy measurements during evaluation of hydrogen trapping10.1016/j.jnucmat.2013.07.006 ↗
18. Effects of tungsten on the hydrogen embrittlement behaviour of microalloyed steels10.1016/j.corsci.2014.01.042 ↗
19. Hydrogen embrittlement of high strength pipeline steels10.1016/j.corsci.2006.02.011 ↗
20. Effects of ferrite/pearlite alignment on the hydrogen permeation in a AISI 4130 steel10.1016/S0167-577X(96)00140-1 ↗
21. A comparative study of hydrogen induced cracking behavior in API 5L X60 and X70 pipeline steels10.1016/j.engfailanal.2013.04.028 ↗
22. M.Ishikawa, T.Shinomiya, S.Endo, Recent development in high strength line-pipe for sour environment, Proc. 22nd Int. Conf. on Offshore Mechanics and Arctic Engineering, Vol. 3, ASME, 2003, Cancun, Mexico, Paper No. OMAE2003-37065, June 8–13 2003, pp. 17-26.10.1115/OMAE2003-37065 ↗
23. R.P.Frohmberg, W. J.Barnett, A. R.Troiano, Delayed Failure and Hydrogen Embrittlement in Steel, Case Institute of Technology, WADC (Wright air development center) Technical Report 54-320, June 1954.10.21236/AD0038142 ↗
24. Hydrogen embrittlement interaction in cold-worked steel10.5006/1.3293573 ↗
25. Hydrogen embrittlement evaluation methods for ultra-high strength steel sheets for automobiles
26. M.S.B.Hope, Effect of Plastic Deformation and Microstructure on Hydrogen Diffusion in Steel (MSc thesis), NTNU, Norway, Trondheim, June 2015, Perm. link: 〈http://hdl.handle.net/11250/2350324〉.
27. The role of dynamic strain-ageing in the environment assisted cracking observed in pressure vessel steels10.1111/j.1460-2695.1997.tb00396.x ↗
28. Tendency towards strain ageing and hydrogen embrittlement of high-strength steel Kh80 for main pipelines10.1007/s10556-008-9096-5 ↗
29. F.Y.Cheng, Strain ageing of high-strength steels in the northern area and the associated technical challenges in development of high-strength steel pipeline technologies, Proc. of 23rd Int. Offshore and Polar Engineering Conf., Alaska, USA, June 30–July 5, 2013
30. Effects of hydrogen on the fracture toughness of a X70 pipeline steel10.1016/j.corsci.2009.07.013 ↗
31. The effect of hydrogen concentration on fracture of pipeline steels in presence of a notch10.1016/j.engfracmech.2010.10.007 ↗
32. Microstructural aspects upon hydrogen environment embrittlement of various bcc steels10.1016/j.ijhydene.2009.10.092 ↗
33. Quantifying the hydrogen embrittlement of pipe steels for safety considerations10.1016/j.ijhydene.2012.05.143 ↗
34. A possible explanation for the contradictory results of hydrogen effects on macroscopic deformation10.1016/j.ijpvp.2012.08.001 ↗
35. The role of hydrogen in hardening/softening steel: Influence of the charging process10.1016/j.scriptamat.2015.05.017 ↗
36. Internal and surface damage of multiphase steels and pure iron after electrochemical hydrogen charging10.1016/j.corsci.2011.05.060 ↗
37. Determination of the hydrogen fugacity during electrolytic charging of steel10.1016/j.corsci.2014.06.033 ↗
38. Hydrogen, crack initiation, and delayed failure in steel
39. Combination of radiation and hydrogen damage of reactor pressure vessel materials10.1016/0308-0161(93)90057-Z ↗
40. Effect of hydrogen on plastic deformation near crack-tip of A537 steel in 3.5% NaCl solution
41. Hydrogen induced delayed plasticity and cracking10.1016/0036-9748(79)90204-7 ↗
42. W.Z.Chu, C.M.Hsiao, S. Q.Li, Mechanism of SCC and hydrogen-induced delayed cracking, Proc. D. François (Ed.), Proceedings of the 5th Int. Conf. on Fracture (ICF5), Cannes, France, 29 March–3 April 1981, Pergamon Press, 1982
43. Positron annihilation study on the distribution of defects in the plastic zone of a crack tip10.1016/0036-9748(82)90432-X ↗
44. The crack tip strain field of AISI 434010.1023/A:1004751420033 ↗
45. Wang · 2011 · 95
46. Hydrogen-enhanced dislocation emission, motion and nucleation of hydrogen-induced cracking for steel10.1007/BF02917169 ↗
47. Atomistic study of the competitive relationship between edge dislocation motion and hydrogen diffusion in alpha iron10.1557/jmr.2011.106 ↗
48. The influence of hydrogen charging[on[the notch tensile properties and fracture behavior of dissimilar weld joints of advanced Cr-Mo-V and Cr-Ni-Mo creep-resistant steels10.1016/j.engfailanal.2010.09.043 ↗
49. Hydrogenation conditions which do not result in formation of cracks during hydrogen charging process of steels10.21062/ujep/x.2016/a/1213-2489/MT/16/5/1129 ↗
50. The effect of internal hydrogen on surface slip localisation on polycrystalline AISI 316L stainless steel10.1016/j.msea.2010.05.062 ↗
51. Hydrogen effect on cyclic plasticity and crack growth in coarse-grained iron10.1016/j.msea.2011.07.036 ↗
52. Hydrogen embrittlement of metals10.1016/0025-5416(72)90109-7 ↗
53. M.Nagumo, Fundamentals of Hydrogen Embrittlement, Springer, Media Singapore, 2016, p. 103.10.1007/978-981-10-0161-1_6 ↗
54. Influence of hydrogen and low temperature on pipeline steels mechanical behaviour of two pipeline steels10.1016/j.engfracmech.2011.09.016 ↗
55. S.T. Rolfe, J.M. Barsom, Fracture and fatigue control in structures, Applications of Fracture Mechanics, Prince-Hall, Inc. Englewood Cliffs, New Jersey, 1977, pp. 208–231.
56. Hydrogen in stress corrosion cracking of X-70 pipeline steels in near-neutral pH solutions10.1007/s10853-006-3944-5 ↗
57. An extensive study of hydrogen-induced cracking susceptibility in an API X60 sour service pipeline steel10.1016/j.ijhydene.2016.01.031 ↗
58. Hydrogen-controlled cracking – an approach to threshold stress intensity10.1007/BF02667281 ↗
59. The role of stress state on hydrogen cracking in fe-si single crystals10.1016/0013-7944(90)90128-4 ↗
60. Consequence of the diffusive hydrogen contents on tensile properties of martensitic steel during the desorption at room temperature10.1016/j.msea.2014.01.039 ↗
61. Enhanced susceptibility to delayed fracture in pre-fatigued martensitic steel10.1016/S0921-5093(02)00403-3 ↗
62. Hydrogen thermal desorption relevant to delayed-fracture susceptibility of high-strength steels10.1007/s11661-001-0265-9 ↗
63. Lattice defects dominating hydrogen-related failure of metals10.1016/j.actamat.2008.06.031 ↗
64. G.Rosenberg, Effects of ageing on behavior of sheet steels fractured under dynamic loading conditions, Proc. of the Int. Conf. on Metallurgy and Materials, METAL 2003, 2003, Hradec nad Moravici, Czech Republic (In Slovak).May 20–22 2003
65. Influence of hydrogen and frequency on fatigue crack growth behavior of Cr-Mo steel10.1007/s10704-010-9560-z ↗
66. Effects of large amounts of hydrogen on the fatigue crack growth behavior of torsional prestrained carbon steel
67. Effects of hydrogen on fatigue crack growth and stretch zone of 0.08% C low carbone steel pipe10.1299/kikaia.74.1528 ↗
68. Hydrogen embrittlement mechanism in fatigue of austenitic stainless steels10.1007/s11661-008-9506-5 ↗
69. The failure criterion based on hydrogen distribution ahead of the fatigue crack tip10.3221/IGF-ESIS.24.13 ↗
70. Fatigue crack growth behaviour in austenitic stainless steels subjected to superficial and entire hydrogenation10.1016/j.msea.2012.03.101 ↗
71. Fractographic and numerical study of hydrogen–plasticity interactions near a crack tip10.1007/s10853-006-0364-5 ↗
72. Interaction of hydrogen with crack-tip plasticity: effects of constraint on void growth10.1016/j.msea.2003.09.052 ↗
73. Effect of hydrogen and microstructure on fatigue crack propagation in a medium carbon steel10.1016/0025-5416(83)90222-7 ↗
74. Campbel · 2008 · 249
75. Local yielding attending fatigue crack growth10.1007/BF02642452 ↗
76. S.W.Nam, S.J.Kim, The role of hydrogen in creep of pure iron, V: Proc. M.G. Yan, S.H. Zhang, Z.M. Zheng (Eds.), Proceedings of the Fifth Int. Conf.,Mechanical Behaviour of Materials, Beijing, China, June 3–6 1987, Pergamon Press, 1988
77. Activation volume and density of mobile dislocations in hydrogen-charged iron10.1016/j.actamat.2013.05.007 ↗
78. Plastic zone and pileup around large indentations10.1007/BF02595628 ↗
79. The effect of hydrogen on plastic deformation of electroless nickel phosphorous amorphous coating10.1016/j.msea.2006.07.122 ↗
80. Hydrogen effects on dislocation activity in austenitic stainless steel10.1016/j.actamat.2006.02.007 ↗
81. Hydrogen effects on localized plasticity in sus310s stainless steel investigated by nanoindentation and atomic force microscopy10.1143/JJAP.48.08JB08 ↗
82. Stress-dependent hardening-to-softening transition of hydrogen effects in nanoindentation of a line-pipe steel10.1016/j.ijhydene.2013.11.060 ↗
83. Investigation of hydrogen-deformation interactions in β-21S titanium alloy using thermal desorption spectroscopy10.1016/j.jallcom.2006.10.026 ↗
84. Numerical analysis of hydrogen transport near a blunting crack tip10.1016/0022-5096(89)90002-1 ↗
85. Transient hydrogen diffusion analyses coupled with crack-tip plasticity under cyclic loading10.1016/j.ijpvp.2008.02.002 ↗
86. Fatigue and fracture of a bulk nanocrystalline nife alloy10.1007/s11661-008-9487-4 ↗
87. Hydrogen embrittlement of ferritic steels: Observations on deformation microstructure, nanoscale dimples and failure by nanovoiding10.1016/j.actamat.2012.06.014 ↗
88. Hydrogen-enhanced lattice defect formation and hydrogen embrittlement of cyclically prestressed tempered martensitic steel10.1016/j.actamat.2013.09.015 ↗
89. The interaction of dislocations and hydrogen-vacancy complexes and its importance for deformation-induced proto nano-voids formation in α-Fe10.1016/j.ijplas.2015.05.017 ↗
90. Interplay between hydrogen and vacancies in α-Fe10.1103/PhysRevB.87.174103 ↗
91. In situ TEM observation of nucleation and bluntness of nanocracks in thin crystals of 310 stainless steel10.1016/0956-7151(95)00122-C ↗
92. Hydrogen-inducing nanovoids in thin crystals of 310 stainless steel10.1023/A:1004426212522 ↗
93. J.A.Newman, Jr., W.T.Riddel, R.S.Piascik, Effects of Kmax on fatigue crack growth threshold in aluminium alloys, in: Thresholds, Endurance Limits, and Design, ASTM STP 1372, ASTM, 200010.1520/STP1372-EB ↗
94. A new mechanism in hydrogen-enhanced fatigue crack growth behavior of a 1900-MPa-class high-strength steel10.1007/s10704-012-9760-9 ↗
95. J.R.Rice, The mechanics of crack tip deformation and extension by fatigue, in: Proceedings of the Symposium on Fatigue Crack Growth, STP 415, ASTM, Philadelpbia, 1967, p. 283.10.1520/STP47234S ↗
96. Cyclic plastic deformation response at fatigue crack tips10.1016/j.ijpvp.2012.10.007 ↗
97. The effect of yield strength on overload affected crack growth rate behavior in steels
98. A kinetic trapping model for hydrogen-induced cracking10.1016/0001-6160(79)90059-2 ↗
99. Hydrogen in microalloyed steels10.1002/srin.200100110 ↗
100. Nucleation mechanism of stress corrosion cracking from notches10.1016/0013-7944(84)90026-2 ↗