Abstract A medium-carbon Cr-Mo-V martensitic steel was quenched at a decreased temperature from 1200° to 900°C and tempered at an identical temperature of 700 °C, thus provided with an enhanced KISSC value. The effect of quenching temperature, Tq, on the sulfide stress cracking (SSC) behaviors was estimated via the double cantilever beam (DCB) and the electrochemical hydrogen permeation (EHP) tests, and the microstructure characterizations. The results indicate that, as the Tq decreased, the overall and local hydrogen concentration around the inclusions decreased, owing to the decreased solute atoms and dislocation density, therefore preventing the SSC initiation. Moreover, the martensitic microstructure were refined and the fraction of the high angle grain boundaries (HAGBs) increased with the decreased Tq, thus decreasing the SSC propagation rate by diverting more frequently the propagating direction and further hindering the SSC propagation. The overall SSC resistance of this martensitic steel was therefore significantly enhanced.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Effect of microstructure on the strength of 25CrMo48V martensitic steel tempered at different temperature and time10.1016/j.matdes.2011.11.026 ↗
2. Effect of martensitic morphology on mechanical properties of an as-quenched and tempered 25CrMo48V Steel10.1016/j.msea.2011.11.078 ↗
3. Effect of martensite morphology on impact toughness of ultra-high strength 25CrMo48V steel seamless tube quenched at different temperatures10.1016/S1006-706X(13)60058-8 ↗
4. Characterization of the microstructures and mechanical properties of 25CrMo48V martensitic steel tempered at different times10.1016/j.msea.2012.08.049 ↗
5. Development of 110-ksi grade OCTG with good resistance to sulfide-stress-corrosion cracking
6. B. Garrison, B.E. Urband, G. Prideco, S. Morey, Production and fit for service attributes of c125 high strength casing, in: NACE International. 〈https://www.onepetro.org/conference-paper/NACE-05090〉 (Accessed 28 August 2017), 2005.
7. A. Di Schino, G. Porcu, L. Scoppio, M. Longobardo, G.L. Turconi, Metallurgical design and development of c125 grade for mild sour service application, in: NACE International. 〈https://www.onepetro.org/conference-paper/NACE-06125?Sort=&start=0&q=Metallurgical+Design+and++Development++of++C125++Grade++for++Mild++Sour++Service++Application&from_year=&peer_reviewed=&published_between=&fromSearchResults=true&to_year=&rows=10#〉 (Accessed 16 December 2017), 2006.
8. The effects of processing variables on mechanical properties and sulfide stress cracking resistance of SAE 4135 steel modified with 0.75 percent Mo and 0.035 percent cb10.1115/1.3438976 ↗
9. The improvement of sulfide stress cracking resistance of 12% chromium stainless steels through heat treatment10.5006/0010-9312-33.7.231 ↗
10. T. Omura, T. Ohe, T. Abe, M. Ueda, P.I. Nice, J.W. Martin, Sulfide stress cracking (SSC) resistance limits for a 125 ksi grade high strength low alloy steel octg developed for mildly sour service, in: NACE International. 〈https://www.onepetro.org/conference-paper/NACE-10307〉 (Accessed 16 December 2017), 2010.
11. G.P. Echaniz, T.E. Perez, C. Pampillo, R.C. Newman, R.P.M. Procter, G.W. Lorimer, The Effect of microstructure on SSC resistance of low alloy carbon steels, in: NACE International. 〈https://www.onepetro.org/conference-paper/NACE-97050sort=&start=0&q=microstructure+SSC&from_year=&peer_reviewed=&published_between=&fromSearchResults=true&to_year=&rows=10#〉 (Accessed 21 August 2017), 1997.
12. G.L. Turconi, C. Gluseppe, E. Anelli, L. Scoppio, T.E. Perez, C. Morales, G. Echaniz, Improvement of resistance to SSC initiation and propagation of high strength OCTG through microstructure and precipitation control, in: NACE International. 〈https://www.onepetro.org/conference-paper/NACE-01077sort=&start=0&q=microstructure+SSC&from_year=&peer_reviewed=&published_between=&fromSearchResults=true&to_year=&rows=10#〉 (Accessed 21 August 2017), 2001.
13. Influence of microstructure on SSC susceptibility of low-alloy, high-strength oil country tubular goods10.5006/1.3577883 ↗
14. Some observations on the corrosion of carbon steel in sour gas environments: effects of H2S and H2S/CO2/CH4/C3H8 Mixtures10.5006/1.3584920 ↗
15. Effects of hydrogen on the properties of iron and steel10.1007/BF02654700 ↗
16. Hydrogen in trapping states innocuous to environmental degradation of high-strength steels10.2355/isijinternational.43.520 ↗
17. Function of Hydrogen in embrittlement of high-strength steels10.2355/isijinternational.41.590 ↗
18. Nature of hydrogen trapping sites in steels induced by plastic deformation10.1016/S0925-8388(99)00322-9 ↗
19. Relation between different inclusion-matrix interfaces in steels and the susceptibility to hydrogen embrittlement10.1007/BF01117917 ↗
20. A new nonmetallic inclusion rating method by positive use of hydrogen embrittlement phenomenon10.1007/s11661-012-1376-1 ↗
21. Hydrogen effects on fracture of high-strength steels with different micro-alloying : Corrosion Reviews, (2015). 〈https://www.degruyter.com/view/j/corrrev.2015.33.issue-6/corrrev-2015-0044/corrrev-2015-0044.xml〉(Accessed August 24, 2017).
22. Effect of crystallographic orientations on the hydrogen-induced cracking resistance improvement of API 5L X70 pipeline steel under various thermomechanical processing10.1016/j.corsci.2016.05.003 ↗
23. The role of microstructure and grain orientations on intergranular cracking susceptibility of UNS 17400 martensitic stainless steel10.1016/j.engfailanal.2017.04.008 ↗
24. A. Di Schino, G. Porcu, L. Scoppio, M. Longobardo, G.L. Turconi, others, Metallurgical design and development of C125 grade for mild sour service application, NACE Corros. Pap. 〈https://www.researchgate.net/profile/Andrea_Di_Schino/publication/270684542_Metallurgical_design_and_development_of_C125_grade_for_mild_sour_service_application/links/54b2c7170cf2318f0f9539bc.pdf〉 (Accessed 27 February 2016).
25. The effect of austenitizing temperature on the microstructure and mechanical properties of as-quenched 4340 steel10.1007/BF02646340 ↗
26. Control of M23C6 carbides in 0.45C–13Cr martensitic stainless steel by means of three representative heat treatment parameters10.1016/S0921-5093(97)00491-7 ↗
27. The effect of heat treatment on mechanical properties and corrosion behavior of AISI420 martensitic stainless steel10.1016/j.jallcom.2010.12.174 ↗
28. A remarkable role of niobium precipitation in refining microstructure and improving toughness of A QT-treated 20CrMo47NbV steel with ultrahigh strength10.1016/j.msea.2014.06.040 ↗
29. A370−10 Standard test methods and definitions for mechanical testing of steel products, ASTM International. doi:10.1016/j.corsci.2016.05.003, 2010.10.1016/j.corsci.2016.05.003 ↗
30. NACE Standard. TM0177−2016, Labortory testing of metals for resistance to sulfide stress cracking and stress Corrosion cracking in H2S environments, NACE International, 2016.
31. A technique for the evaluation of hydrogen embrittlement characteristics of electroplating baths10.1149/1.2425894 ↗
32. Hydrogen permeation behavior in relation to microstructural evolution of low carbon bainitic steel weldments10.1016/j.corsci.2016.07.025 ↗
33. Determination of trapping parameters and the chemical diffusion coefficient from hydrogen permeation experiments10.1016/j.corsci.2014.01.002 ↗
34. Effect of microstructure and inclusions on hydrogen induced cracking susceptibility and hydrogen trapping efficiency of X120 pipeline steel10.1016/j.msea.2010.07.022 ↗
35. Electron backscattering diffraction study of acicular ferrite, bainite, and martensite steel microstructures10.1179/026708300773002636 ↗
36. The morphology and crystallography of lath martensite in Fe-C alloys10.1016/S1359-6454(02)00577-3 ↗
37. The retained austenite, twinned substructure and autotempered carbide in as-quenched low-carbon martensite
38. M. Masoumi, C.C. Silva, H.F.G. de Abreu, Effect of crystallographic orientations on the hydrogen-induced cracking resistance improvement of API 5L X70 pipeline steel under various thermomechanical processing, Corros. Sci. (n.d.). doi:10.1016/j.corsci.2016.05.003.10.1016/j.corsci.2016.05.003 ↗
39. In situ observations of silver-decoration evolution under hydrogen permeation: effects of grain boundary misorientation on hydrogen flux in pure iron10.1016/j.scriptamat.2016.10.027 ↗
40. The role of microstructure and grain orientations on intergranular cracking susceptibility of UNS 17400 martensitic stainless steel10.1016/j.engfailanal.2017.04.008 ↗
41. Trap theory of hydrogen embrittlement10.1016/0001-6160(80)90106-6 ↗
42. A study of internal hydrogen embrittlement of steels10.1016/S0921-5093(00)00793-0 ↗
43. Microstructural aspects upon hydrogen environment embrittlement of various bcc steels10.1016/j.ijhydene.2009.10.092 ↗
44. The role of retained austenite in hydrogen embrittlement of supermartensitic stainless steel10.1016/j.engfailanal.2013.07.025 ↗
45. Hydrogen trapping in ferritic steel weld metal10.1179/095066002225006548 ↗
46. The effect of heat treatment on mechanical properties and corrosion behavior of AISI420 martensitic stainless steel10.1016/j.jallcom.2010.12.174 ↗
47. Effect of microstructural refinement on the toughness of low carbon martensitic steel10.1016/j.scriptamat.2007.10.053 ↗
48. Hydrogen trapping in high strength martensitic steel after austenitized at different temperatures10.1016/j.ijhydene.2013.08.121 ↗
49. In situ electrochemical microcantilever bending test: a new insight into hydrogen enhanced cracking10.1016/j.scriptamat.2017.01.019 ↗
50. The microstructural evolution and impact toughness of nugget zone in friction stir welded X100 pipeline steel10.1016/j.jallcom.2016.03.299 ↗
51. In situ TEM study of the effect of M/A films at grain boundaries on crack propagation in an ultra-fine acicular ferrite pipeline steel10.1016/j.actamat.2005.09.015 ↗