journal article·2021-01

Influence of microstructure on cyclic deformation response and micromechanics of Ti–55531 alloy

Zilu Xu, Chaowen Huang, Changsheng Tan, Mingpan Wan, Yongqing Zhao, Junqing Ye, Weidong Zeng

Publisher page

Abstract

Abstract Cyclic deformation response and micromechanics in strain controlled low cycle fatigue of Ti–5Al–5Mo–5V–3Cr–1Zr (Ti–55531) alloy with bimodal microstructure (BM) and lamellar microstructure (LM) were comparatively investigated at ambient temperature. Results showed that cyclic hardening/softening behavior of Ti–55531 alloy was found to be significantly dependent on both the strain amplitude and microstructure. The cyclic softening rate of LM was always larger than that of BM at strain level below 1.0%; however, the opposite result was produced for strain amplitude above 1.0%. Dislocation features revealed that cyclic deformation of the alloy primarily relied on primary α (αp) and secondary α (αs) phases. At low strain levels, lasting hardening of BM was due to the interaction of multiple prismatic and basal slips, and pyramidal slip in αp particles, while slight softening of LM was owing to the activation of a few twins in lamellar αs. However, at high strain levels, dislocation annihilation and numerous twins were detected in both αp and αs phases in BM, which resulted in the larger cyclic softening rate of BM than that of LM. Evidently, besides dislocation annihilation, twinning was found to be another important softening mechanism, which was not revealed by other studies on Ti alloys.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Intermetallics and Advanced Alloy Properties · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (42)

Show source-provided references
1. The effect of machining and induced surface deformation on the fatigue performance of a high strength metastable β titanium alloy10.1016/j.ijfatigue.2019.02.033 ↗
2. Crack nucleation in β titanium alloys under high cycle fatigue conditions - a review
3. Perspectives on titanium science and technology10.1016/j.actamat.2012.10.043 ↗
4. The use of β titanium alloys in the aerospace industry10.1007/s11665-013-0728-3 ↗
5. Advanced materials and technology for A380 structure
6. On the microstructure evolution during isothermal low cycle fatigue of β-annealed Ti-6242S titanium alloy: internal damage mechanism, substructure development and early globularization10.1016/j.ijfatigue.2018.07.014 ↗
7. Committee · 1996
8. Strain controlled fatigue testing of the metastable β-titanium alloy Ti–6.8Mo–4.5Fe–1.5Al (Timetal LCB)10.1016/j.msea.2011.04.031 ↗
9. On the effect of deep-rolling and laser-peening on the stress-controlled low- and high-cycle fatigue behavior of Ti–6Al–4V at elevated temperatures up to 550°C10.1016/j.ijfatigue.2012.03.008 ↗
10. Cyclic deformation behavior of an α/β titanium alloy -I. micromechanisms of plasticity under various loading paths10.1016/S1359-6454(96)00406-5 ↗
11. Cyclic deformation behavior of an α/β titanium alloy -II. internal stress and micromechanic modelling10.1016/S1359-6454(96)00407-7 ↗
12. Low cycle fatigue behavior of an α + β titanium alloy: Ti624610.1016/0921-5093(93)90423-C ↗
13. Cyclic softening of the Ti-10V-2Fe-3Al titanium alloy10.1016/S0921-5093(96)10531-1 ↗
14. Cyclic deformation response and micromechanisms of Ti alloy Ti–5Al–5V–5Mo–3Cr–0.5Fe10.1016/j.msea.2011.08.045 ↗
15. 3-D observations of short fatigue crack interaction with lamellar and duplex microstructures in a two-phase titanium alloy10.1016/j.actamat.2010.11.015 ↗
16. Three-dimensional characterization of fatigue cracks in Ti-6246 using X-ray tomography and electron backscatter diffraction10.1016/j.actamat.2009.08.009 ↗
17. Effect of α-phase morphology on low-cycle fatigue behavior of TC21 alloy10.1016/j.ijfatigue.2015.01.010 ↗
18. Effect of duplex aging on microstructure and mechanical behavior of beta titanium alloy Ti–15V–3Cr–3Al–3Sn under unidirectional and cyclic loading conditions10.1016/j.ijfatigue.2014.12.005 ↗
19. The crack initiation behavior and the fatigue limit of Ti–5Al–5Mo–5V–1Cr–1Fe titanium alloy with basket-weave microstructure10.1016/j.jallcom.2015.01.077 ↗
20. Cyclic deformation response of β-annealed Ti-5Al-5V-5Mo-3Cr alloy under compressive loading conditions10.1007/s11661-011-0705-0 ↗
21. Effect of microstructure on tensile properties of Ti–5Al–5Mo–5V–3Cr–1Zr alloy10.1016/j.jallcom.2016.09.233 ↗
22. Static and fatigue characterization of the Ti5553 titanium alloy10.1111/ffe.12011 ↗
23. Effect of microstructure on torsion properties of Ti–5Al–5Mo–5V–3Cr–1Zr alloy10.1016/j.msea.2016.11.049 ↗
24. Twinning behavior in the Ti–5at.% Al single crystals during cyclic loading along [0001]10.1016/j.msea.2004.11.039 ↗
25. Cyclic deformation and microcrack initiation during stress controlled high cycle fatigue of a titanium alloy10.1016/j.msea.2017.11.019 ↗
26. Effect of microstructure on high cycle fatigue behavior of Ti–5Al–5Mo–5V–3Cr–1Zr titanium alloy10.1016/j.ijfatigue.2016.09.005 ↗
27. Source mechanism of non-basal ⟨c+a⟩ slip in Ti alloy10.1016/j.scriptamat.2013.03.009 ↗
28. Characterization of deformation in primary α phase and crack initiation and propagation of TC21 alloy using in-situ SEM experiments10.1016/j.msea.2018.03.123 ↗
29. High cycle fatigue behavior of Ti–5Al–5Mo–5V–3Cr–1Zr titanium alloy with lamellar microstructure10.1016/j.msea.2016.11.014 ↗
30. Crystallography of fatigue crack initiation and growth in fully lamellar Ti–6Al–4V10.1007/s11661-009-0064-2 ↗
31. Defect-interface interactions10.1016/j.pmatsci.2015.02.001 ↗
32. Study of twinning/detwinning behaviors of Ti by interrupted in situ tensile tests10.1016/j.actamat.2014.09.038 ↗
33. Tensile deformation and fracture of Ti–5Al–5V–5Mo–3Cr–1.5Zr–0.5Fe alloy at room temperature10.1016/j.msea.2013.08.055 ↗
34. Mechanical behavior and deformation mechanisms of Ti–2.5Cu alloy reinforced by nano-scale precipitates at 293 and 77 K10.1016/j.msea.2003.08.015 ↗
35. On the design of new β-metastable titanium alloys with improved work hardening rate thanks to simultaneous TRIP and TWIP effects10.1016/j.scriptamat.2012.01.049 ↗
36. Investigation of early stage deformation mechanisms in a metastable β titanium alloy showing combined twinning-induced plasticity and transformation-induced plasticity effects10.1016/j.actamat.2013.07.019 ↗
37. The onset of twinning in metals: a constitutive description10.1016/S1359-6454(01)00300-7 ↗
38. Flow stress for twinning of alpha copper alloys
39. Understanding common grain boundary twins in Mg alloys by a composite Schmid factor10.1016/j.ijplas.2019.07.018 ↗
40. Dislocation ↔ twin transmutations during interaction between prismatic slip and{10-11} twin in magnesium10.1016/j.actamat.2020.01.010 ↗
41. Influence of stacking fault energy and dislocation character on slip transfer at coherent twin boundaries studied by micropillar compression10.1016/j.actamat.2018.05.037 ↗
42. Uniaxial ratcheting and fatigue failure behaviors of hot-rolled AZ31B magnesium alloy under asymmetrical cyclic stress-controlled loadings10.1016/j.msea.2013.03.004 ↗