Effect of grain orientation on the compressive response of highly oriented MAX phase Ti3SiC2
Source abstract
Abstract
Abstract The MAX phases comprise of a group of layered ternary carbides that exhibit unique mechanical properties which bridge the gap between their metal and ceramic constituents. To study the effects of the global grain orientation, Ti, Si and TiC powders were hot pressed to synthesize highly oriented bulk Ti3SiC2. X-ray diffraction (XRD) was used to verify the grain orientation and a Lotgering factor of 0.87 with respect to the c-axis was obtained. Prepared Ti3SiC2 samples have been compressed in two orientations, loading along the c-axis ( ∥ c-axis) and perpendicular to the c-axis ( ⊥ c-axis) at 10 − 3 s − 1 using a standard load frame and at 10 2 s − 1 using a Kolsky (split-Hopkinson) bar. The average compressive strength along the ⊥ c-axis orientation was 761 MPa under quasi-static conditions and 987 MPa under dynamic loading, exhibiting a 30% increase on average. The ∥ c-axis orientation exhibited no rate dependence in compressive strength; however both orientations exhibited an increase of strain at failure under dynamic conditions by over 0.5%, on average. The orientation-dependent failure behavior at different strain rates were examined using high-speed imaging and 2D digital image correlation (DIC) during loading and via scanning electron microscopy (SEM) post-mortem. Results indicate that the ⊥ c-axis fracture surface exhibited a mixture of transgranular and intergranular cracks, kink bands and delaminations, whereas ∥ c-axis was limited to a combination of intergranular and transgranular cracks. Such fracture distinctions due to the availability (or lack thereof) for kink band formation appear to be responsible for the anisotropic compressive behavior.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: MXene and MAX Phase Materials · Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (64)
Show source-provided references
1. Barsoum · 2013
2. On the chemical diversity of the MAX phases10.1016/j.trechm.2019.02.016 ↗
3. Synthesis and characterization of a remarkable ceramic: Ti3SiC210.1111/j.1151-2916.1996.tb08018.x ↗
4. The MAX phases: unique new carbide and nitride materials: ternary ceramics turn out to be surprisingly soft and machinable, yet also heat-tolerant, strong and lightweight10.1511/2001.28.334 ↗
5. Progress in research and development on MAX phases: a family of layered ternary compounds10.1179/1743280410Y.0000000001 ↗
6. Elastic and mechanical properties of the MAX phases10.1146/annurev-matsci-062910-100448 ↗
7. The Mn+1AXn phases: materials science and thin-film processing10.1016/j.tsf.2009.07.184 ↗
8. Fully reversible, dislocation-based compressive deformation of Ti3SiC2 to 1 GPa10.1038/nmat814 ↗
9. Processing and mechanical properties of Ti3SiC2: II, effect of grain size and deformation temperature10.1111/j.1151-2916.1999.tb02167.x ↗
10. A comprehensive survey of M2AX phase elastic properties10.1088/0953-8984/21/30/305403 ↗
11. Dislocations, kink bands, and room-temperature plasticity of Ti3SiC210.1007/s11661-999-0172-z ↗
12. Room-temperature ductile carbides10.1007/s11661-999-0325-0 ↗
13. Ripplocations in van der Waals layers10.1021/nl5045082 ↗
14. Spherical nanoindentation, modeling and transmission electron microscopy evidence for ripplocations in Ti3SiC210.1016/j.actamat.2017.03.055 ↗
15. Deformation of layered solids: ripplocations not basal dislocations10.1016/j.scriptamat.2017.04.002 ↗
16. Evidence for bulk ripplocations in layered solids10.1038/srep33451 ↗
17. Ripplocations: a universal deformation mechanism in layered solids
18. Single crystal pillar microcompression tests of the MAX phases Ti2InC and Ti4AlN310.1016/j.scriptamat.2013.05.002 ↗
19. Shear fracture behavior of Ti3SiC2 induced by compression at temperatures below 1000ํC10.1016/j.msea.2005.07.041 ↗
20. Damage accumulation and hysteretic behavior of MAX phase materials10.1016/j.jmps.2011.03.012 ↗
21. On the relevance of kinking to reversible hysteresis in MAX phases10.1016/j.actamat.2014.01.045 ↗
22. Kinking nonlinear elastic deformation of Ti3AlC2, Ti2AlC, Ti3Al(C0.5,N0.5)2 and Ti2Al(C0.5,N0.5)10.1016/j.jallcom.2010.03.099 ↗
23. Microscale modeling of kinking nonlinear elastic solids10.1103/PhysRevB.71.134101 ↗
24. Macroscale constitutive modeling of kinking nonlinear elastic solids10.1016/j.msea.2005.11.043 ↗
25. Synthesis and characterization of Ti3SiC210.1111/j.1151-2916.2000.tb01281.x ↗
26. New phases' discovery in MAX family10.1016/j.ijrmhm.2012.10.011 ↗
27. Texture-engineered ceramics-property enhancements through crystallographic tailoring10.1557/jmr.2017.207 ↗
28. Toughening mechanisms in nanolayered MAX phase ceramics-A review10.3390/ma10040366 ↗
29. Topotactical reactions with ferrimagnetic oxides having hexagonal crystal structures—I10.1016/0022-1902(59)80070-1 ↗
30. Textured silicon nitride: processing and anisotropic properties10.1088/1468-6996/9/3/033001 ↗
31. Synthesis of high-purity, isotropic or textured Cr2AlC bulk ceramics by spark plasma sintering of pressure-less sintered powders10.1016/j.jeurceramsoc.2014.11.008 ↗
32. Physical and mechanical properties of highly textured polycrystalline Nb4AlC3 ceramic10.1088/1468-6996/12/4/044603 ↗
33. Fabrication of textured Nb4AlC3 ceramic by slip casting in a strong magnetic field and spark plasma sintering10.1111/j.1551-2916.2010.04096.x ↗
34. Shell-like nanolayered Nb4AlC3 ceramic with high strength and toughness10.1016/j.scriptamat.2010.12.045 ↗
35. In situ neutron diffraction evidence for fully reversible dislocation motion in highly textured polycrystalline Ti2AlC samples10.1016/j.actamat.2015.07.023 ↗
36. A new method to texture dense Mn+1AXn ceramics by spark plasma deformation10.1016/j.scriptamat.2015.08.023 ↗
37. Highly textured Ti2AlN ceramic prepared via thermal explosion followed by edge-free spark plasma sintering10.1016/j.scriptamat.2017.04.013 ↗
38. Fabrication of textured Ti3SiC2 by spark plasma sintering and their anisotropic mechanical properties10.2109/jcersj2.121.366 ↗
39. Effect of texture microstructure on tribological properties of tailored Ti3AlC2 ceramic10.1007/s40145-017-0224-6 ↗
40. Tailoring Ti3AlC2 ceramic with high anisotropic physical and mechanical properties10.1016/j.jeurceramsoc.2014.08.026 ↗
41. Tailoring Ti3SiC2 ceramic via a strong magnetic field alignment method followed by spark plasma sintering10.1111/j.1551-2916.2010.04186.x ↗
42. Fabrication of textured Ti3SiC2 ceramic by slip casting in a strong magnetic field and pressureless sintering10.2109/jcersj2.122.817 ↗
43. Electrophoretic deposition of Ti3SiC2 and texture development in a strong magnetic field10.1111/j.1551-2916.2012.05296.x ↗
44. Dynamic fracture behavior of a MAX phase Ti3SiC210.1016/j.engfracmech.2016.11.006 ↗
45. Clarkin · 2017
46. High strain-rate response and deformation mechanisms in polycrystalline Ti2AlC10.1016/j.msea.2014.01.032 ↗
47. The effect of grain size on deformation and failure of Ti2AlC MAX phase under thermo-mechanical loading10.1007/s11340-017-0264-4 ↗
48. Mechanical response of fine grained Ti2AlC under extreme thermo-mechanical loading conditions10.1016/j.msea.2016.01.106 ↗
49. Abnormal response of Ti3SiC2 to high strain-rate loading
50. NIH Image to ImageJ: 25 years of image analysis10.1038/nmeth.2089 ↗
51. Study of optimal subset size in digital image correlation of speckle pattern images10.1016/j.optlaseng.2007.01.012 ↗
52. Image Correlation for Shape, Motion and Deformation Measurements: Basic concepts
53. Drop on demand colloidal suspension inkjet patterning for DIC10.1007/s40799-018-0260-3 ↗
54. An investigation of the mechanical properties of materials at very high rates of loading10.1088/0370-1301/62/11/302 ↗
55. Dynamic compressive strength of silicon carbide under uniaxial compression10.1016/S0921-5093(01)01172-8 ↗
56. Ramesh · 2008 · vol. 1
57. The compressive failure of aluminum nitride considered as a model advanced ceramic10.1016/j.jmps.2011.02.003 ↗
58. Dynamic failure and inelastic deformation behavior of SiC ceramic under uniaxial compression10.1016/j.ceramint.2019.09.011 ↗
59. Hidden energy dissipation mechanism in nacre10.1557/jmr.2014.179 ↗
60. P. Lava, D. Debruyne, MatchID (2010).
61. ASTM · 2019 · vol. 19
62. Dynamic strength and fragmentation of hot-pressed silicon carbide under uniaxial compression10.1016/j.actamat.2003.09.036 ↗
63. Compressive failure of fibre-reinforced composites: buckling, kinking, and the role of the interphase10.1007/BF00361515 ↗
64. A micromechanical model for high strain rate behavior of ceramics