journal article·2019-04

Mechanisms of fatigue crack propagation in a Q&P-processed steel

Kristin Hockauf, Martin Franz-Xaver Wagner, Bohuslav Mašek, Thomas Lampke

Publisher page

Abstract

Abstract The fatigue crack propagation (FCP) behavior of a quenched and partitioned (Q&P), low-alloyed CSiCrMn steel containing 12% of retained austenite is investigated in ΔK-controlled tests at different R-ratios and compared with its quenched and tempered (QT) counterpart, containing 4% of retained austenite. Characteristic features of the crack wake and FCP surfaces are examined by scanning electron microscopy and related to the presence or absence of martensitic transformation. Comparing the FCP behavior of the Q&P condition with its QT counterpart, the fatigue threshold ΔKth is higher, and fatigue crack growth rates in the Paris-regime are lower, for Q&P. With an increase of ΔK, Paris-lines intersect and, at high ΔK, the fatigue crack growth resistance of the Q&P condition becomes inferior. Such FCG behavior is attributed to the amount and stability of retained austenite: at low ΔK, contributions of the martensitic transformation are negligible, and thus a higher fraction of retained austenite accounts for an increased FCG resistance. With increasing ΔK, an increasing percentage of retained austenite in the cyclic plastic zone at the crack tip is transformed, providing brittle pathways for fast crack propagation and thus lowering FCG resistance. Analysing the crack surface, cleavage-like intergranular crack propagation can be directly related to martensitic transformation: in the threshold region, FCP occurs predominantly in a transgranular mode and the percentage of cleavage planes increases as ΔK increases. This study is the first one that examines the FCP behavior in a Q&P-processed steel and one of very few which deal with the near-threshold FCP behavior in TRIP steels.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Fatigue and fracture mechanics · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Microstructure and tensile properties in dual phase and TRIP steels10.1002/srin.200405831 ↗
2. A numerical and experimental investigation into hot stamping of boron alloyed heat treated steels10.1002/srin.200806320 ↗
3. A study of microstructure, transformation mechanisms and correlation between microstructure and mechanical properties of a low alloyed TRIP steel10.1016/j.actamat.2004.02.044 ↗
4. Microstructure-based constitutive modeling of TRIP steel: prediction of ductility and failure modes under different loading conditions10.1016/j.actamat.2009.02.020 ↗
5. Carbon partitioning into austenite after martensite transformation10.1016/S1359-6454(03)00059-4 ↗
6. Mechanism exploration of an ultrahigh strength steel by quenching–partitioning–tempering process10.1016/j.msea.2011.08.050 ↗
7. Characterization of microstructure obtained by quenching and partitioning process in low alloy martensitic steel10.1016/j.msea.2010.02.020 ↗
8. Properties of advanced experimental CMnSiMo steel achieved by QP process10.1016/j.proeng.2011.04.491 ↗
9. Influence of metastable retained austenite on macro and micromechanical properties of steel processed by the Q&P process10.1016/j.jallcom.2013.12.028 ↗
10. Enhanced ductility and toughness in an ultrahigh-strength Mn–Si–Cr–C steel: the great potential of ultrafine filmy retained austenite10.1016/j.actamat.2014.05.055 ↗
11. Microstructure-mechanical properties relationships for quenching and partitioning (Q&P) processed steel10.1016/j.actamat.2016.04.048 ↗
12. Microstructure-mechanical properties relationships for quenching and partitioning (Q&P) processed steel10.1016/j.actamat.2016.04.048 ↗
13. Role of microstructure in the low cycle fatigue of multi-phase steels10.1016/j.msea.2011.11.071 ↗
14. Influence of ferrite fraction within martensite matrix on fatigue crack propagation: an experimental verification with dual phase steel10.1016/j.msea.2012.05.085 ↗
15. Deformation-induced martensite formation during cyclic deformation of metastable austenitic steel: influence of temperature and carbon content10.1016/j.msea.2006.12.211 ↗
16. Factors influencing the austenite stability during tensile testing of quenching and partitioning steel determined via in-situ electron backscatter diffraction10.1016/j.msea.2015.04.075 ↗
17. Effect of microstructure on fatigue behavior of advanced high strength steels produced by quenching and partitioning and the role of retained austenite10.1016/j.msea.2015.06.034 ↗
18. Strain-induced martensitic transformation in fatigue crack tip zone for a high strength steel10.1016/j.matchar.2005.02.004 ↗
19. Martensitic transformation at a propagating crack10.1016/0001-6160(78)90211-0 ↗
20. Fatigue crack growth in TRIP steel under positive R-ratios10.1016/j.engfracmech.2007.01.019 ↗
21. Effect of retained austenite on the fracture toughness of quenching and partitioning (Q&P)-Treated sheet steels10.1007/s11661-013-2113-0 ↗
22. Development of a high strength high toughness ausferritic steel10.1016/j.msea.2009.02.013 ↗
23. Properties of advanced experimental CMnSiMo steel achieved by QP process10.1016/j.proeng.2011.04.491 ↗
24. Optimization of Q-P Process parameters with regard to final microstructures and properties
25. Effect of quenching and partitioning temperatures in the Q-P process on the properties of AHSS with various amounts of manganese and silicon10.4028/www.scientific.net/MSF.706-709.2734 ↗
26. Corrosion characteristics of a quenching and partitioning steel determined by electrochemical impedance spectroscopy10.1088/1757-899X/373/1/012003 ↗
27. DIN 50125, Testing of metallic materials - Tensile test pieces. Beuth Verlag GmbH, Germany.
28. ASTM E399, Standard Test Method for Linear-Elastic Plane-Strain Fracture Toughness KIc of Metallic Materials. ASTM International.
29. EBSD analysis of relationship between microstructural features and toughness of a medium-carbon quenching and partitioning bainitic steel10.1007/s11665-017-3052-5 ↗
30. In situ TEM study of the effect of M/A films at grain boundaries on crack propagation in an ultra-fine acicular ferrite pipeline steel10.1016/j.actamat.2005.09.015 ↗
31. Krupp · 2007
32. Crack growth in ultrafine-grained AA6063 produced by equal-channel angular pressing10.1007/s10853-008-2725-8 ↗
33. Microstructure and fatigue crack growth in a γ-Fe-Ni-Al alloy10.1016/0001-6160(76)90104-8 ↗
34. The low-cycle fatigue, deformation and final fracture behaviour of an austenitic stainless steel10.1016/j.msea.2005.09.081 ↗
35. Fatigue crack propagation in martensitic and austenitic steels10.1007/BF02644521 ↗
36. Influence of precipitates on low-cycle fatigue and crack growth behavior in an ultrafine-grained aluminum alloy10.1016/j.actamat.2014.07.061 ↗
37. Effects of microstructure on fatigue crack propagation and crack closure behavior in aluminum alloy 715010.1016/0025-5416(85)90276-9 ↗