Effect of surface roughness and industrial heat treatments on the microstructure and mechanical properties of Ti6Al4V alloy manufactured by laser powder bed fusion in different built orientations
Source abstract
Abstract
The emergence of powder bed fusion in recent years has made it one of the most demanded additive manufacturing technologies for Ti6Al4V alloys in the biomedical and aerospace industries due to its ease of part fabrication with complex geometry. However, Ti6Al4V components require a post-processing treatment to optimize their mechanical properties for engineering applications. The present study offers an analysis of the effects of different industrial heat treatments (704 °C for 120 min, 740 °C for 130 min) on the microstructure and tensile properties of Ti6Al4V samples manufactured by laser powder bed fusion in different orientations (Z, 45°, XY and XZ). These heat treatments were selected to improve the mechanical properties of the as-built material and to obtain samples representative of real industrial applications. SEM observations illustrated that the α’ martensite grown in the columnar parent β-grains was converted into an α+β mixture after both heat treatments. EBSD showed that the newly formed α phase maintained, inside the parent β grains, the same orientation relationship as the as-built α′ martensite. However, on a macroscopic scale, the α phase exhibited no preferential orientation. The heat-treated samples, which exhibited approximately 10% lower ultimate tensile strength and yield strength than the as built samples but a 10–13% higher elongation, were practically isotropic in their mechanical response. What little anisotropy was left was mainly attributed to few elongated interlamellar pores. The sandblasting process was also investigated; it did not affect the static mechanical properties of the samples but it reduced the Ra values by 25%. Finally, Vickers microhardness vs. strength relationships were studied by considering the α-phase orientation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · Additive Manufacturing and 3D Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (71)
Show source-provided references
1. 2012
2. Simulation of layer-by-layer Selective Laser Melting process with an efficient remeshing technique10.1016/j.promfg.2019.06.167 ↗
3. The effect of SLM process parameters on density, hardness, tensile test and surface quality of Ti6Al4V
4. A study of the microstructural evolution during selective laser manufacturing of Ti-6Al-4V10.1016/j.actamat.2010.02.004 ↗
5. Effect of the building orientation on the mechanical properties and fracture modes of SLM Ti-6Al-4V10.1016/j.msea.2014.07.086 ↗
6. Donachie · 2000
7. Microstructure and mechanical behavior of Ti-6Al-4V produced by rapid-layer manufactured, for biomedical applications10.1016/j.jmbbm.2008.05.004 ↗
8. Qualification of Ti6AL4V ELI alloy produced by laser bed powder fusion for biomedical applications10.1007/s11837-017-2655-5 ↗
9. Selective laser melting of Ti-6Al-4V: the impact of post-processing on the tensile, fatigue and biological properties for medical implant applications10.3390/ma13122813 ↗
10. Laser deposition and deformation behavior of Ti-Nb-Zr-Ta alloys for orthopedic implants10.1016/j.jmbbm.2012.08.014 ↗
11. Effects of topographical surface modifications of electron beam melted Ti-6Al-4V titanium on human fetal osteoblasts10.1002/jbm.a.31540 ↗
12. Selective laser melting and electron beam melting of Ti6Al4V for orthopedic applications: a comparative study on the applied building direction10.3390/ma13235584 ↗
13. Boyer · 1994
14. A.E. Wilson-Heid, S. Qin, A.M. Beese, Anisotropic multiaxial plasticity model for laser powder bed fusion additively manufactured Ti-6Al-4V, Mater. Sci. Eng. 738, 90-97. https://doi.org/10.1016/j.msea.2018.09.077.10.1016/j.msea.2018.09.077 ↗
15. Comparison of the microstructures and mechanical properties of Ti-6Al-4V fabricated by selective laser melting and electron beam melting10.1016/j.matdes.2015.12.135 ↗
16. Additive manufacturing of AlSi10Mg and Ti6Al4V lightweight Alloys via laser powder bed fusion: a review of heat treatment effects10.3390/ma15062047 ↗
17. Formation and control of martensite in Ti-6Al-4V alloy produced by selective laser melting10.1016/j.matdes.2016.06.117 ↗
18. Heat treatments of Ti6Al4V produced by selective laser melting: microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
19. Microstructure and fatigue performance of SLM-fabricated Ti6Al4V alloy after different stress-relief heat treatments10.1016/j.trpro.2019.07.005 ↗
20. Effect of subtransus heat treatment on the microstructure and mechanical properties of additively manufactured TI-6Al-4V alloy10.1016/j.jallcom.2017.11.263 ↗
21. Martensitic transformation in Ti-6Al-4V (ELI) alloy manufactured by 3D Printing10.1016/j.matchar.2018.09.042 ↗
22. As-fabricated and heat-treated microstructures of the Ti-6Al-4V alloy processed by selective laser melting10.1007/s11661-011-0731-y ↗
23. Fatigue performance evaluation of selective laser melted Ti-6Al-4V10.1016/j.msea.2014.01.041 ↗
24. The influence of heat accumulation on the surface roughness in powder-bed additive manufacturing
25. Effect of the microstructure and porosity of Ti-6Al-4V ELI alloy fabricated by electron beam melting (EBM)
26. The influence of as-built surface conditions on mechanical properties of Ti-6Al-4V additive manufacturing by selective electron beam melting10.1007/s11837-015-1768-y ↗
27. Chemical etching of titanium samples10.3311/PPme.7046 ↗
28. Measurement on the interlamellar spacing of perlite10.1016/0026-0800(84)90002-8 ↗
29. Texture analysis with MTEX – free and Open source software toolbox10.4028/www.scientific.net/SSP.160.63 ↗
30. Improvement of fatigue resistance and ductility of Ti6Al4V processed by Selective Laser Melting10.1016/j.jmatprotec.2015.01.025 ↗
31. Influence of selective laser melting scanning speed parameter on the surface morphology, surface roughness and micropores for manufactured Ti6Al4V parts10.1557/jmr.2020.84 ↗
32. Analysis of defect generation in Ti-6Al-4V parts made using powder bed fusion additive manufacturing processes
33. Ductility improvement due to martensite α’ decomposition in porous Ti-6Al-4V parts produced by sleective laser melting for orthopedic implants10.1016/j.jmbbm.2015.09.020 ↗
34. Role of martensite decomposition in tensile properties of selective laser melted Ti-6Al-4V10.1016/j.jallcom.2018.02.111 ↗
35. Effect of industrial heat treatment on the mechanical performance of Ti6Al4V processed by Selective Laser Melting10.3390/app10072280 ↗
36. Microstructures and mechanical propreties of Ti6Al4V parts fabricated by selective laser melting and electron beam melting10.1007/s11665-013-0658-0 ↗
37. Ti6Al4V additively manufactured by selective laser melting with superior mechanical properties10.1007/s11837-015-1297-8 ↗
38. Thermomechanical response of 3D laser-deposited Ti-6A6-4V alloy over a wide range of strain rates and temperatures10.1016/j.msea.2015.08.043 ↗
39. Research on selective laser melting of Ti6Al4V: surface morphologies, optimized processing zone, and ductility improvement mechanism10.3390/met8070471 ↗
40. Thermal process maps for predicting solidification microstructure in laser fabrication of thin-wall structures
41. Additive manufacturing of metals: a brief review of the characteristic microstructures and properties of steels, Ti-6Al4V and high entropy alloys10.1080/14686996.2017.1361305 ↗
42. Effect of build geometry on the β-grain structure and texture in additive manufacturing of Ti-6Al-4V by selective electron beam melting10.1016/j.matchar.2013.07.012 ↗
43. The heat treatment influence on the microstructure and hardness of TC4 titanium alloy manufactured via selective laser melting10.3390/ma11081318 ↗
44. Internal stress of plate martensitic depending on aspect ratio via fcc-hcp martensitic transformation in metastable Austenitic stainless steels10.2320/matertrans.MT-MJ2019007 ↗
45. Phase transformation during cooling in α+β titanium alloys10.1016/S0921-5093(97)00802-2 ↗
46. Thermal stability of an ultrafine grained Ti-6Al-4V alloy during post-deformation annealing10.1016/j.msea.2017.03.082 ↗
47. Laser and electron beam additive manufacturing methods of fabricating titanium bone implants10.3390/app7070657 ↗
48. Microstructure static properties, and fatigue crack growth mechanisms in Ti-6Al-4V fabricated by additive manufacturing: LENS and EBM10.1016/j.engfailanal.2016.05.036 ↗
49. Selective laser melting produced Ti-6Al-4V: post-process heat treatments to achieve superior tensile properties10.3390/ma11010146 ↗
50. On the creep performance of the Ti-6Al-4V alloy processed by additive manufacturing
51. Martensitic transformation form β to α’ and α’’ phases in Ti-V alloys: a first-principles study10.1557/jmr.2017.276 ↗
52. Parent grain reconstruction from partially or fully transformed microstructure in MTEX10.1107/S1600576721011560 ↗
53. Microstructural characterization of binary microstructure pattern in selective laser-melted Ti-6Al-4V10.1007/s00170-019-04002-8 ↗
54. Texture and crystal orientation in Ti-6Al-4V build fabricated by shaped metal deposition10.1007/s11661-010-0255-x ↗
55. Estimates of the mechanical properties of laser powder bed fusion Ti-6Al-4V parts using finite element models10.1016/j.matdes.2019.107678 ↗
56. Selective laser melting of aluminium metal-matrix composites and the challenges
57. The effect of manufacturing defects on the fatigue behaviour of Ti-6Al-4V specimens fabricated using selective laser melting10.4028/www.scientific.net/AMR.891-892.1519 ↗
58. Influence of processing parameters on internal porosity and types of defects formed in Ti6Al4V lattice structure fabricated by selective laser melting10.1016/j.msea.2019.138387 ↗
59. Surface chemistry of Ti6Al4V components fabricated using selective laser melting for biomedical applications10.1016/j.msec.2016.05.054 ↗
60. Surface finish has a critical influence on biofilm formation and mammalian cell attachment to additively manufactured prosthetics10.1021/acsbiomaterials.7b00336 ↗
61. Systematic evaluation of selective fusion additive manufacturing based on thermal energy source applied in processing of titanium alloy specimens for medical applications10.1007/s00170-020-05797-7 ↗
62. Application of mechanical surface finishing processes for roughness reduction and fatigue improvement of additively manufactured Ti-6Al-4V parts10.1016/j.ijfatigue.2017.05.008 ↗
63. Hickey · 1961 · 26
64. Development of strength-hardness relationships in additively manufactured titanium alloys10.1016/j.msea.2017.03.102 ↗
65. On the size and orientation effect in additive manufactured Ti-6Al-4V10.1016/j.matdes.2019.108235 ↗
66. The role of initial α-phase orientation on tensile and strain hardening behavior of Ti-6Al-4V alloy10.1016/j.mtcomm.2017.10.018 ↗
67. Direct observations and analyses alpha phase of an alpha/beta Ti-alloy of dislocation substructures in the formed by nanoindentation10.1016/j.actamat.2005.07.030 ↗
68. Determination of hardness and elastic modulus inverse pole figures of a polycrystalline commercially pure titanium by coupling nanoindentation and EBSD techniques10.1016/j.msea.2014.06.098 ↗
69. The hardness and strength metals
70. Improved equation relating hardness to ultimate strength10.1007/BF02652880 ↗
71. Determination of yield strength from hardness measurements10.1007/BF02913433 ↗