journal article·2017-08

The effect of heat-to-heat variations in metallurgy and hydrogen-metal interactions on the hydrogen embrittlement of Monel K-500

B.C. Rincon Troconis, Z.D. Harris, H. Ha, J.T. Burns, J.R. Scully

Publisher page

Abstract

Abstract The influence of heat-to-heat variations on the hydrogen embrittlement susceptibility of age-hardened Monel K-500 (UNS N05500) was evaluated through detailed characterization of metallurgical attributes and hydrogen interactions, coupled with notched tensile specimen embrittlement metrics. Four nominally peak-aged material heats of Monel K-500 were assessed using slow strain rate tensile (SSRT) testing while immersed in 0.6 M NaCl solution and exposed to cathodic polarization levels ranging from −0.850 to −1.1 V SCE . Despite each of the four heats meeting the US Federal Procurement Specification QQ-N-286G, the hydrogen embrittlement susceptibility was found to vary extensively between the tested material heats. Characterization of microstructural features, composition, and hydrogen-metal interactions were performed to facilitate correlation between material property and susceptibility trends. Results suggest that subtle differences in grain boundary chemistry and H uptake behavior may contribute to heat-to-heat variations in hydrogen embrittlement susceptibility of Monel K-500. Conversely, parameters including yield strength, hydrogen diffusivity, hydrogen production rate, grain boundary character, and grain size do not independently control the observed variations in susceptibility. Based on these experimental results, a macroscale framework for assessing the degradation in fracture stress as a function of applied potential is proposed and possible avenues for framework improvement are suggested.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Nuclear Materials and Properties · High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (93)

Show source-provided references
1. Precipitation in the Ni-Cu-base alloy Monel K-50010.1016/0025-5416(86)90236-3 ↗
2. Precipitation hardening in nickel-copper base alloy Monel K 50010.1007/BF02659495 ↗
3. Long-term corrosion behavior of materials in the marine atmosphere
4. A century of Monel metal: 1906–200610.1007/s11837-006-0077-x ↗
5. Effects of hydrogen on engineering properties of MONEL nickel-copper alloy K-50010.5006/0010-9312-28.2.57 ↗
6. Failures of nickel/copper bolts in subsea applications
7. Failure of Monel Ni-Cu-Al alloy K-500 bolts in seawater
8. G.A. Scott, Studbolting experience in the underwater environment of the North Sea, in: Proccedings of the 17th Offshore Technology Conference, 1985, pp. 269–280.10.4043/5050-MS ↗
9. Stress corrosion cracking and hydrogen embrittlement of high-strength nonmagnetic alloys in brine
10. Control of hydrogen embrittlement in deep gas wells
11. Scully · 1984
12. Hydrogen embrittlement of cathodically protected subsea bolting alloys
13. Measurement and modeling of hydrogen environment-assisted cracking in Monel K-50010.1007/s11661-014-2324-z ↗
14. R.E. Butler, Hydrogen embrittlement of high-strength alloys in marine environments, in: Eng. with Copper-Nickel Alloy., Metals Society, London, U.K., 1988, pp. 79–84.
15. Hydrogen asisted cracking of high strength alloys
16. Hydrogen embrittlement understood
17. Hydrogen embrittlement phenomena and mechanisms10.1515/corrrev-2012-0502 ↗
18. R. Otuska, T. Maruno, H. Tsuji, Correlation between hydrogen embrittlement and hydride formation in Ni-Cu and Pd-Ag alloys, in: Proceedings of the Int. Conf. Met. Corros., 1984, pp. 270–277.
19. Hydrogen-induced intergranular fracture of steels10.1016/S0013-7944(00)00124-7 ↗
20. Environment-assisted intergranular cracking: factors that promote crack path connectivity
21. Segregation to interfaces10.1179/imr.1977.22.1.262 ↗
22. Chapter 7: grain Boundary Segregation and Related Phenomena
23. The intergranular embrittlement of nickel by hydrogen: the effect of grain boundary segregation10.1007/BF02644118 ↗
24. Confirmation of sulfur embrittlement in nickel alloys10.1016/0036-9748(74)90394-9 ↗
25. Chapter 5: Compositional effects
26. Impurities and trace elements in nickel-base superalloys
27. Intergranular fracture of nickel: the effect of hydrogen-sulfur co-segregation10.1016/0001-6160(87)90127-1 ↗
28. A first-principles model for hydrogen uptake promoted by sulfur on Ni(111)10.1149/1.3536470 ↗
29. Influence of sulfur, phosphorus, and antimony segregation on the intergranular hydrogen embrittlement of nickel10.1007/BF02651619 ↗
30. The role of chemical bonding in grain boundary embrittlement10.1016/0001-6160(82)90226-7 ↗
31. Surface and grain-boundary segregation of sulfur and boron in nickel10.1016/0001-6160(88)90108-3 ↗
32. Effects of segregation on grain-boundary cohesion – a density-functional cluster model of boron and sulfur in nickel10.1103/PhysRevLett.58.234 ↗
33. The effects of boron impurity atoms on nickel E5 (012) grain boundary by first principles calculations
34. Embrittlement of a 5 Pct nickel high strength steel by impurities and their effects on hydrogen-induced cracking10.1007/BF02659919 ↗
35. A mechanistic theory of hydrogen embrittlement of steels10.1002/bbpc.19720760864 ↗
36. The role of hydrogen and other interstitials in the mechanical behavior of metals: (1959 Edward De Mille Campbell memorial lecture)10.1007/s13632-016-0319-4 ↗
37. The threshold stress intensity for hydrogen-induced crack growth10.1007/BF02643487 ↗
38. Gaseous hydrogen embrittlement of high strength steels10.1007/BF02667388 ↗
39. The effect of impurities and strength level on hydrogen induced cracking in a low alloy turbine steel10.1007/BF02644870 ↗
40. Strain gradient plasticity-based modeling of hydrogen environment assisted cracking10.1016/j.actamat.2016.07.022 ↗
41. Strain gradient plasticity modeling of hydrogen diffusion to the crack tip10.1016/j.ijhydene.2016.05.014 ↗
42. Intergranular fracture in 4340-type steels: effects of impurities and hydrogen10.1007/BF02646706 ↗
43. Hydrogen diffusion and trapping in a precipitation-hardened nickel–copper–aluminum alloy Monel K-500 (UNS N05500)10.1016/j.actamat.2013.02.007 ↗
44. Hydrogen permeation through iron and steel by electrochemical transfer—II. Influence of metallurgical factors on hydrogen permeation☆10.1016/0013-4686(67)80125-7 ↗
45. Hydrogen trap states in ultrahigh-strength AERMET 100 steel10.1007/s11661-004-0011-1 ↗
46. Trapping of hydrogen to lattice defects in nickel10.1088/0965-0393/3/3/001 ↗
47. Deuterium concentration profiles in FeNiCo alloys electrochemically charged at room temperature10.1016/0001-6160(89)90286-1 ↗
48. Hydrogen transport in nickel-base alloys10.1007/BF02663432 ↗
49. QQ-N-286G, Nickel-Copper-Aluminum Alloy, Wrought (UNS N05500), 2000.
50. The effect of microstructural variation on the hydrogen environment-assisted cracking of Monel K-50010.1007/s11661-016-3486-7 ↗
51. R.D. Bayles, T. Lemieux, F. Martin, D. Lysogorski, T. Newbauer, W. Hyland, et al., Monel K-500 hydrogen embrittlement, in: Nav. Surf. Treament Cent. MR2010 Proceedings Present. 〈http://nstcenter.com/docs/PDFs/MR2010/Thurs-1-Presentations/10-Bayles.PDF〉.
52. Limitations of the slow strain rate test for stress-corrosion cracking testing10.5006/1.3315931 ↗
53. ASTM Standard G129, 2000 · 2013
54. The slow strain rate stress corrosion cracking test – a 50 year retrospective10.5006/2137 ↗
55. Kingery · 1976
56. An electrochemical technique to measure diffusible hydrogen in metals (Barnacle electrode)
57. The adsorption and diffusion of electrolytic hydrogen in palladium
58. ASTM Standard E1447, 2009 · 2016
59. The identification of hydrogen trapping states in an Al-Li-Cu-Zr alloy using thermal desorption spectroscopy10.1007/s11661-000-0064-8 ↗
60. Crank · Math. Diffus. · 1975
61. A study of hydrogen-trapping phenomena in AISI 5160 spring steel10.1016/0025-5416(84)90053-3 ↗
62. Intergranular sulfur and grain boundary plane in a nickel bicrystal10.1051/jphyscol:1990154 ↗
63. Sulfur segregation on nickel10.1016/0036-9748(85)90276-5 ↗
64. Effect of minor elements on hot workability of nickel-base super-alloys10.1179/030716979803276110 ↗
65. The control of sulfur content in nickel-base, single crystal superalloys and its effects on cyclic oxidation resistance
66. Debardaillo · 1976 · 95
67. Effects of hydrogen on the properties of iron and steel10.1007/BF02654700 ↗
68. Hydrogen detrapping from grain boundaries and dislocations in high purity iron10.1016/0956-7151(92)90436-I ↗
69. Analysis of hydrogen atom transport in a two-phase alloy10.1016/0921-5093(94)90488-X ↗
70. Grain boundary segregation in Ni and binary Ni alloys doped with sulfur10.1007/BF02644289 ↗
71. Solubility limit for sulphur in nickel between 637° and 1400°C10.1179/cmq.1970.9.4.525 ↗
72. In situ auger electron spectroscopy tensile fracture study of nickel alloys
73. Effect of zirconium on microstructure and mechanical properties of cast fine-grain CM 247 LC superalloy10.2320/matertrans.45.554 ↗
74. Kinetics of hydrogen evolution on nickel electrodes10.1016/0022-0728(90)87140-F ↗
75. On the kinetics of the hydrogen evolution reaction on nickel in alkaline solution – Part I. The mechanism10.1016/S0022-0728(01)00590-3 ↗
76. Mechanism of hydrogen evolution reaction on nickel in alkaline solutions by the degree of coverage10.1039/tf9605601820 ↗
77. The mechanism of hydrogen evolution at nickel cathodes in aqueous solutions10.1063/1.1700503 ↗
78. Electrochemical aspects of hydrogen in metals
79. Surface effects on hydrogen entry into metals
80. Science-based prognosis to manage structural alloy performance in hydrogen
81. Predicting the effect of applied potential on crack tip hydrogen concentration in low-alloy martensitic steels10.5006/1.3278484 ↗
82. Trap theory of hydrogen embrittlement10.1016/0001-6160(80)90106-6 ↗
83. Grain boundary engineering: historical perspective and future prospects10.1007/s10853-011-5393-z ↗
84. McLean · 1957
85. Effect of hydrogen on the fracture behavior of high strength steel during slow strain rate test10.1016/j.corsci.2007.03.038 ↗
86. Effect of hydrogen and stress concentration on the notch tensile strength of AISI 4135 steel10.1016/j.msea.2005.03.008 ↗
87. A critical-strain criterion for hydrogen embrittlement of cold-drawn, ultrafine pearlitic steel10.1007/s11661-002-0217-z ↗
88. Influence of dynamic straining on hydrogen embrittlement of UNS-G41300 and UNS-S31803 steels in a low H2S concentration environment10.1016/j.corsci.2004.07.033 ↗
89. Grain-boundary engineering markedly reduces susceptibility to intergranular hydrogen embrittlement in metallic materials10.1016/j.actamat.2009.05.012 ↗
90. An example of the effect of hydrogen trapping on hydrogen embrittlement10.1007/BF02648348 ↗
91. Measurement and modeling of hydrogen environment assisted cracking in a Ni-Cu-Al-Ti superalloy10.1007/s11661-015-3315-4 ↗
92. NACE Standard MR0175-1998 · 1998
93. ASTM E1447, 2009 · 2014