journal article·2021-05

Effect of surface nanocrystallization on fatigue properties of Ti–6Al–4V alloys with bimodal and lamellar structure

Conghui Zhang, Kun Hu, Min Zheng, Wenguang Zhu, Guodong Song

Publisher page

Abstract

Abstract High-energy shot peening (HESP) was employed to obtain a nanocrystalline surface layer in Ti–6Al–4V alloy with bimodal and lamellar structure. The microstructure and residual stress after HESP treatment were characterized by transmission electron microscope (TEM) and X-ray diffractometer (XRD), respectively. The fracture morphology of fatigue was analyzed by scanning electron microscope (SEM). The results showed that the average grain sizes of Ti–6Al–4V alloy with bimodal and lamellar structure were 18.9 nm and 17.1 nm at the topmost surface layer, respectively. The maximum compressive residual stress of the bimodal structure was −906MPa, which was higher than that of the lamellar structure (−859 MPa). The fatigue limits of the HESP-treated Ti–6Al–4V alloy with the bimodal and lamellar structure were increased by 13.5% and 32.8%, respectively. Finally, a Goodman equation was employed to calculate the local fatigue strength and analyze the residual stress-fatigue strength correlation. Highly defected substructure, reduced effective slip length and improved yield strength were important factors for the improvement of fatigue strength. The synergy effect of surface gradient nanostructure and compressive residual stress improved the fatigue limit of the HESP-treated Ti–6Al–4V alloy with bimodal and lamellar structure.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Surface Treatment and Residual Stress · Erosion and Abrasive Machining · High-Velocity Impact and Material Behavior

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Perspectives on titanium science and technology10.1016/j.actamat.2012.10.043 ↗
2. Peters · 2003
3. Investigation of local deformation behaviour of metallic materials and recent research trends: a review10.3365/KJMM.2018.56.9.635 ↗
4. Segregation mediated heterogeneous structure in a metastable β titanium alloy with a superior combination of strength and ductility
5. Ralph · 1972
6. Mechanical surface treatments on titanium, aluminum and magnesium alloys10.1016/S0921-5093(98)01168-X ↗
7. Overall evaluation of the effect of residual stress induced by shot peening in the improvement of fatigue fracture resistance for metallic materials10.3901/CJME.2015.0112.013 ↗
8. Fatigue properties of nanocrystallized surfaces obtained by high energy shot peening10.1016/j.proeng.2010.03.181 ↗
9. Effect of severe shot peening on microstructure and fatigue strength of cast iron10.1016/j.ijfatigue.2013.08.022 ↗
10. Surface nanocrystallization of 17-4 precipitation-hardening stainless steel subjected to ultrasonic surface rolling process10.1016/j.msea.2018.04.033 ↗
11. Enhancing torsion fatigue behaviour of a martensitic stainless steel by generating gradient nanograined layer via surface mechanical grinding treatment10.1179/1743284712Y.0000000192 ↗
12. Fatigue life improvement through surface nanostructuring of stainless steel by means of surface mechanical attrition treatment10.1016/j.scriptamat.2006.01.049 ↗
13. Effect of surface nanocrystallization on the corrosion behavior of Ti-6Al-4V titanium alloy10.1016/j.surfcoat.2013.02.052 ↗
14. Influence of the surface nanocrystallization on the gas nitriding of Ti-6Al-4V alloy10.1016/j.apsusc.2013.09.105 ↗
15. Nanocrystallization mechanism of beta phase in Ti-6Al-4V subjected to severe plastic deformation10.1016/j.msea.2016.05.088 ↗
16. Influence of shot peening on the fatigue life of Cu-Ni austempered ductile iron10.1016/j.msea.2012.02.092 ↗
17. Influence of severe shot peening on the surface state and ultra-high-cycle fatigue behavior of an AW 7075 aluminum alloy10.1007/s11665-017-2692-9 ↗
18. Effects of shot-peening and re-shot-peening on four-point bend fatigue behavior of Ti-6Al-4V10.1016/j.msea.2007.01.156 ↗
19. Effect of compressive residual stress introduced by cavitation peening and shot peening on the improvement of fatigue strength of stainless steel10.1016/j.jmatprotec.2020.116877 ↗
20. Fatigue performance of surface nanocrystallized TC4
21. On the influence of laser peening with different coverage areas on fatigue response and fracture behavior of Ti-6Al-4V alloy10.1016/j.engfracmech.2015.08.026 ↗
22. A micromechanical model to study the closure stress effect on fatigue life of Ti6Al4V subjected to laser shock peening10.1016/j.engfracmech.2018.08.004 ↗
23. Comparison of the fatigue and fracture of α + β and β titanium alloys10.1007/s11661-001-1031-8 ↗
24. Influence of microstructure on high-cycle fatigue of Ti-6Al-4V: bimodal vs. lamellar structures
25. Effect of microstructure on fatigue crack propagation rate of TC4-DT titanium alloy
26. High cycle fatigue fractograph of TC17 titanium alloy with equiaxed and basket-waved microstructure
27. Slip and fatigue crack formation processes in an α/β titanium alloy in relation to crystallographic texture on different scales10.1016/j.actamat.2008.04.036 ↗
28. On the mechanism of fatigue and dwell-fatigue crack initiation in Ti-6Al-4V10.1016/j.scriptamat.2020.03.031 ↗
29. On the influence of ultrasonic surface rolling process on surface integrity and fatigue performance of Ti-6Al-4V alloy10.1016/j.surfcoat.2019.04.080 ↗
30. Evolution of residual stress redistribution associated with localized surface microcracking in shot-peened medium-carbon steel during fatigue test10.1016/j.ijfatigue.2013.06.010 ↗
31. Room- temperature tensile plasticity of BT18y titanium alloy with equiaxed structure and fully lamellar structure
32. High cycle fatigue of isothermally forged Ti-6.5Al-2.2Mo-2.2Zr-1.8Sn-0.7W-0.2Si with different microstructures10.1016/j.jallcom.2016.07.277 ↗
33. Lütjering · 2007
34. Effect of shot peening on fatigue performance of Ti2AlNb intermetallic alloy10.1016/j.ijfatigue.2019.05.034 ↗
35. Fatigue crack growth of TC17 titanium alloy with three microstructures
36. Effect of ultrasonic shot peening on LCF behavior of the Ti–6Al–4V alloy10.1016/j.jallcom.2017.07.014 ↗
37. Effect of laser shock peening on microstructure and fatigue crack growth rate of AZ31B magnesium alloy10.1016/j.jallcom.2016.04.179 ↗
38. Subsurface crack initiation during fatigue as a result of residual stresses10.1111/j.1460-2695.1979.tb00388.x ↗
39. Improved fatigue behavior of low-carbon steel 20GL by applying ultrasonic impact treatment combined with the electric discharge surface alloying10.1016/j.msea.2016.02.036 ↗