Hydrogen isotope trapping in Al–Cu binary alloys
Source abstract
Abstract
The trapping mechanisms for hydrogen isotopes in Al-X Cu (0.0 at.% < X < 3.5 at.%) alloys were investigated using thermal desorption spectroscopy (TDS), electrical conductivity, and differential scanning calorimetry. Constant heating rate TDS was used to determine microstructural trap energies and occupancies. In addition to the trapping states in pure Al reported in the literature (interstitial lattice sites, dislocations, and vacancies), a trap site due to Al-Cu intermetallic precipitates is observed. The binding energy of this precipitate trap is ($18\pm3$) kJ$\cdot$mol$-1$ ($0.19 \pm 0.03$ eV). Typical occupancy of this trap is high; for Al-2.6 at.% Cu (a Cu composition comparable to that in AA2219) charged at 200°C with 130 MPa D$_2$ for 68 days, there is ca. there is $3.15\times10-7$ mol D bound to the precipitate trap per mol of Al, accounting for a third of the D in the charged sample.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fusion materials and technologies · Nuclear Physics and Applications · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Effects of deformation on hydrogen permeation in austenitic stainless steels10.1016/0001-6160(86)90123-9 ↗
2. Tritium barriers and tritium diffusion in fusion reactors
3. The solubility of hydrogen in liquid and solid aluminium
4. 19-Hydrogen embrittlement of aluminum and aluminum-based alloys
5. San Marchi · 2012
6. Hydrogen embrittlement and stress corrosion cracking of aluminum alloys
7. P.M. Ordin, Safety Standard for Hydrogen and Hydrogen Systems: Guidelines for Hydrogen System Design, Materials Selection, Operations, Storage and Transportation, NASA, 1997. 〈http://archive.org/details/nasa_techdoc_19970033338〉 (accessed 20.08.15).
8. Hydrogen in aluminum10.1016/S0925-8388(96)02968-4 ↗
9. The diffusion and trapping of hydrogen in high purity aluminum10.1016/S1359-6454(98)00333-4 ↗
10. Characterization of trapped hydrogen in exfoliation corroded aluminium alloy 202410.1016/S1359-6462(99)00292-4 ↗
11. Deuterium transport and trapping in aluminum alloys10.1007/BF02664813 ↗
12. Effect of implanted silicon on hydrogen behavior in aluminum and nickel10.1016/S0168-583X(99)00684-9 ↗
13. Effect of prior deformation and heat treatment on the corrosion-induced hydrogen trapping in aluminium alloy 202410.1016/j.corsci.2013.11.021 ↗
14. Hydrogen diffusion in aluminium at high temperatures10.1088/0305-4608/13/6/013 ↗
15. Hydrogen in aluminum: first-principles calculations of structure and thermodynamics10.1103/PhysRevB.69.144109 ↗
16. Hydrogen diffusivity in aluminium10.1080/09500838808214712 ↗
17. Behaviour of hydrogen in pure aluminium, Al–4 mass% Cu and Al-1 mass% Mg2Si alloys studied by tritium electron microautoradiography10.1007/BF00349974 ↗
18. Hydrogen trapping in an Al–2.1wt% Li alloy10.1007/BF00356133 ↗
19. Hydrogen trapping and repelling in an Al–6wt% Zn–2wt % Mg alloy10.1007/BF01119730 ↗
20. Tritium diffusion and trapping associated with lithium in Al–Li systems10.1016/0022-5088(88)90222-6 ↗
21. Statistical model of defects in Al–H system10.1103/PhysRevB.81.024105 ↗
22. Precipitates in Al–Cu alloys revisited: Atom-probe tomographic experiments and first-principles calculations of compositional evolution and interfacial segregation10.1016/j.actamat.2011.06.036 ↗
23. Analysis and thermodynamic prediction of hydrogen solution in solid and liquid multicomponent aluminum alloys
24. Internal friction in hydrogen-charged aluminium alloys10.1080/01418618108239416 ↗
25. The identification of hydrogen trapping states in an Al–Li–Cu–Zr alloy using thermal desorption spectroscopy10.1007/s11661-000-0064-8 ↗
26. Hydrogen solubility, diffusion and trapping in high purity aluminum and selected Al-base alloys10.4028/www.scientific.net/MSF.331-337.1583 ↗
27. Bulk diffusion-controlled thermal desorption spectroscopy with examples for hydrogen in iron
28. Combined thermal desorption spectroscopy, differential scanning calorimetry, scanning electron microscopy and X-ray diffraction study of hydrogen trapping in cold deformed TRIP steel10.1016/j.actamat.2012.01.026 ↗
29. 1993
30. Eaton · 2009
31. Molecular hydrogen formation on astrophysically relevant surfaces10.1086/307642 ↗
32. Reaction kinetics in differential thermal analysis10.1021/ac60131a045 ↗
33. Kinetics and mechanisms of precipitation in an Al–0.2wt% Sc alloy10.1016/j.msea.2005.02.015 ↗
34. Dependence of electrical resistivity on temperature and composition of Al–Cu alloys10.1179/1433075X11Y.0000000041 ↗
35. Electrical resistivity of ten selected binary alloy systems10.1063/1.555684 ↗
36. Precipitation behavior of an Al–Cu alloy during isothermal aging at low temperatures10.1016/j.matlet.2004.10.058 ↗
37. Cooling and heating rate dependence of precipitation in an Al–Cu alloy10.1016/0921-5093(92)90150-Y ↗