Effect of multi-stage aging treatments on the precipitation and mechanical properties of Al-Zn-Mg alloys
Source abstract
Abstract
Abstract The mechanical properties of Al-Zn-Mg alloys via multi-stage aging treatments were studied to explore the strength-toughness trade-off. The microstructures of aged alloys were characterized by scanning electron microscope (SEM) and transmission electron microscope (TEM). The results indicated that large numbers of GP zones and some part of η′ phases were formed during the low-temperature (90 °C) aging at the third-stage aging, which consumed considerable solid solubility. This prevents fast growth and coarsening of precipitates at the fourth-stage aging (150 °C). Finally, the mixed precipitation state of mainly η′ phases and some η phases formed. The grain boundary phase grew insignificantly, which is beneficial to decrease the strength gap between intragranular and grain-boundary. The intragranular equilibrium η phase is beneficial to pin the movement of dislocation, which avoids fracture caused by accumulation of dislocations around the large second-phase and on the grain boundaries. Although the strength of materials decreased slightly, the impact toughness of materials significantly increased due to the positive effect of the intragranular equilibrium η phase. Compared with the conventional retrogression and re-aging (RRA) treatment (120 °C/24 h + 185 °C/105min + 120 °C/12 h), the designed four-stage ageing treatment (FSA) (120 °C/24 h + 185 °C/105min + 90 °C/12 h + 150 °C/12 h) resulted in the decrease of tensile strength and yield strength by only 3% and 4%, respectively, but contributed to the increases of elongation and impact toughness by 15% and 17%, respectively.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Constitutive analysis of homogenized 7005 aluminum alloy at evaluated temperature for extrusion process10.1016/j.matdes.2014.10.045 ↗
2. Influence of heat treatment on the strength and fracture toughness of 7N01 aluminum alloy10.1016/j.jallcom.2016.03.228 ↗
3. Effect of composition on tensile properties and fracture toughness of Al-Zn-Mg alloy (A7N01S-T5) used in high speed trains10.1016/j.matdes.2015.11.107 ↗
4. Hot deformation behavior and constitutive equation of a new type Al-Zn-Mg-Er-Zr alloy during isothermal compression10.1016/j.msea.2015.10.122 ↗
5. Hot deformation behavior of as-quenched 7005 aluminum alloy10.1016/S1003-6326(14)63411-7 ↗
6. Correlations between stress corrosion cracking susceptibility and grain boundary microstructures for an Al-Zn-Mg alloy10.1016/j.corsci.2013.07.032 ↗
7. Influence of Al7Cu2Fe intermetallic particles on the localized corrosion of high strength aluminum alloys10.1016/j.matdes.2013.07.003 ↗
8. Influence of dual retrogression and re-aging temper on microstructure, strength and exfoliation corrosion behavior of Al-Zn-Mg-Cu alloy10.1016/S1003-6326(11)61248-X ↗
9. The effect of pre-ageing temperature and retrogression heating rate on the strength and corrosion behaviour of AA715010.1016/j.corsci.2011.08.042 ↗
10. Effect of heat treatment on strength, exfoliation corrosion and electrochemical behavior of 7085 aluminum alloy10.1016/j.matdes.2011.09.033 ↗
11. Microstructure and mechanical properties of high strength Al-Zn-Mg-Cu alloys used for oil drill pipes10.1016/S1003-6326(15)63994-2 ↗
12. Effects of retrogression heating rate on microstructures and mechanical properties of aluminum alloy 705010.1016/S1003-6326(09)60239-9 ↗
13. Improvement of strength and ductility of an Al-Zn-Mg alloy by controlling grain size and precipitate microstructure with Mn and Ag addition10.1016/j.msea.2013.05.025 ↗
14. Effect of heat treatment on stress corrosion cracking, fracture toughness and strength of 7085 aluminum alloy10.1016/S1003-6326(14)63351-3 ↗
15. Effect of solution treatment on the strength and fracture toughness of aluminum alloy 705010.1016/j.jallcom.2011.01.005 ↗
16. Evolution of precipitate microstructure during stress aging of an Al-Zn-Mg-Cu alloy10.1016/j.msea.2015.03.047 ↗
17. Early-stage precipitation in Al-Zn-Mg-Cu alloy (7050)10.1016/j.actamat.2004.06.025 ↗
18. Microstructural, mechanical and electrochemical behaviour of a 7017 Al-Zn-Mg alloy of different tempers10.1016/j.matchar.2015.03.025 ↗
19. Secondary ageing in an aluminium alloy 705010.1016/j.msea.2008.02.039 ↗
20. Influence of retrogression and re-aging treatment on corrosion behaviour of an Al-Zn-Mg-Cu alloy10.1016/j.matdes.2010.11.036 ↗
21. The effects of non-isothermal aging on the strength and corrosion behavior of Al-Zn-Mg-Cu alloy10.1016/j.jallcom.2016.04.208 ↗
22. Investigation of precipitation behaviour and related hardening in AA 7055 aluminium alloy10.1016/j.msea.2008.09.065 ↗
23. Influence of retrogression temperature and time on the mechanical properties and exfoliation corrosion behavior of aluminium alloy AA715010.1016/j.matchar.2009.06.007 ↗
24. Microstructure, mechanical properties and stress corrosion cracking of Al-Zn-Mg-Zr alloy sheet with trace amount of Sc10.1016/j.jallcom.2015.08.011 ↗
25. Effects of solution treatment on microstructural and mechanical properties of Al-Zn-Mg alloy by microalloying with Sc and Zr10.1016/j.jallcom.2016.01.016 ↗
26. Characterization of the mechanical properties changes in an Al-Zn-Mg alloy after a two-step ageing treatment at 70° and 135°C10.1016/j.matdes.2009.12.033 ↗
27. Investigation of mechanical and corrosion properties of an Al-Zn-Mg-Cu alloy under various ageing conditions and interface analysis of η′ precipitate10.1016/j.matdes.2015.06.183 ↗
28. Aging behavior and precipitate characterization of a high Zn-containing Al-Zn-Mg-Cu alloy with various tempers10.1016/j.matdes.2016.03.150 ↗
29. Effect of cooling aging on microstructure and mechanical properties of an Al-Zn-Mg-Cu alloy10.1016/j.matdes.2013.12.024 ↗