Microstructural evolutions and mechanical properties of Mg-xY-2Nd-0.2Zn-0.5Zr (x = 0, 2, 4, 6 and 8) alloy under hot compression
Source abstract
Abstract
Abstract In this work, Mg-xY-2Nd-0.2Zn-0.5Zr (x = 0, 2, 4, 6 and 8, in weight percentage) alloys were subjected to hot compression at various temperatures from 420 °C to 510 °C. For briefness, the studied alloys were named as 0Y, 2Y, 4Y, 6Y and 8Y samples. During hot compression, dynamic recrystallization (DRX) happened and ultra-fine grains (UFGs) were generated in all samples. With the increase of Y content, the volume fraction of UFGs became lower. Based on the origins of work softening during hot compression, the samples could be classified into two groups. Low Y-containing group included 0Y, 2Y and 4Y samples, while high Y-containing group included 6Y and 8Y samples. Continuous DRX (cDRX), which was accompanied by deformation bands, induced the work softening of low Y-containing samples. Inversely, for high Y-containing samples, high-density dynamic precipitates consumed the stored energy and induced the work softening. The cDRX development was delayed, and discontinuous DRX (dDRX) happened at the dynamic precipitate sites at high strains. For the hot-compressed samples, during uniaxial tensile tests at room temperature, basal slip dominated low Y-containing samples while pyramidal slip dominated high Y-containing samples. The strong interactions between pyramidal dislocations and precipitates enhanced the strength of high Y-containing samples by sacrificing elongation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Metal and Thin Film Mechanics · Hydrogen Storage and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. Enhancement of tensile ductility and stretch formability of AZ31 magnesium alloy sheet processed by cross-wavy bending10.1016/j.jallcom.2013.06.185 ↗
2. Mechanical behavior and deformation mechanisms of AZ31 Mg alloy at liquid nitrogen temperature10.1016/j.matlet.2013.07.029 ↗
3. Microstructural development under interrupted hot deformation and the mechanical properties of a cast Mg-Gd-Y-Zr alloy10.1016/j.msea.2015.11.034 ↗
4. Effect of rare earth additions on microstructure and texture development of magnesium alloy sheets10.1016/j.scriptamat.2009.12.033 ↗
5. Effect of rare earth elements on deformation behavior of an extruded Mg-10Gd-3Y-0.5Zr alloy during compression10.1016/j.matdes.2012.10.040 ↗
6. Growth and morphology of β phase in an Mg -Y-Nd alloy10.1016/j.matlet.2004.05.032 ↗
7. Strength and ductility optimization of Mg-Y-Nd-Zr alloy by microstructural design10.1016/j.ijplas.2014.11.003 ↗
8. On the microstructural factors affecting creep resistance of die-cast Mg-La-rare earth (Nd, Y or Gd) alloys10.1016/j.msea.2016.08.046 ↗
9. Enhanced age hardening response and creep resistance of Mg-Gd alloys containing Zn10.1016/j.scriptamat.2005.07.004 ↗
10. Additive manufactured WE43 magnesium: a comparative study of the microstructure and mechanical properties with those of powder extruded and as-cast WE4310.1016/j.matchar.2018.11.011 ↗
11. Mechanical response, twinning, and texture evolution of WE43 magnesium-rare earth alloy as a function of strain rate: experiments and multi-level crystal plasticity modeling10.1016/j.ijplas.2019.04.019 ↗
12. The effect of precipitation hardening on the structure and mechanical and tribological properties of magnesium alloy WE5410.1016/j.vacuum.2017.02.015 ↗
13. Influence of solution and aging on the microstructures and mechanical properties of complex deformed WE93 alloy10.1016/j.matdes.2013.03.104 ↗
14. The effect of heterogeneous deformation on the hot deformation of WE54 magnesium alloy10.1016/j.matdes.2014.01.038 ↗
15. Twinning and texture randomization in Mg and Mg-Ce alloys10.1016/j.ijplas.2019.03.001 ↗
16. Ductility enhancement in Mg-0.2%Ce alloys10.1016/j.actamat.2018.09.023 ↗
17. Secondary phase precipitation and thermally stable microstructure refinement induced by ECAP on Mg-Y-Nd (WN43) alloy10.1016/j.matlet.2018.09.107 ↗
18. Texture and microhardness of Mg-Rare Earth (Nd and Ce) alloys processed by high-pressure torsion10.1016/j.msea.2018.03.114 ↗
19. Microstructure, texture and mechanical properties of coarse-grained Mg-Gd-Y-Nd-Zr alloy processed by multidirectional forging10.1016/j.jallcom.2014.10.084 ↗
20. Dynamic recrystallization behaviors of a Mg-4Y-2Nd-0.2Zn-0.5Zr alloy and the resultant mechanical properties after hot compression10.1016/j.matdes.2016.02.072 ↗
21. Effect of heat treatment on dynamic recrystallization behaviors and mechanical properties of Mg-2.7Nd-0.5Zn-0.8Zr alloy10.1016/j.msea.2016.08.025 ↗
22. Precipitation response of the magnesium alloy WE43 in strained and unstrained conditions10.1016/j.jallcom.2014.09.179 ↗
23. Influence of aging pre-treatment on the compressive deformation of WE54 alloy10.1016/j.msea.2006.10.125 ↗
24. The maximum solubility of Y in α -Mg and composition ranges of Mg24Y5-x and Mg2Y1-x intermetallic phases in Mg-Y binary system10.1016/j.jallcom.2010.09.120 ↗
25. Diffusion of Nd in hcp Mg and interdiffusion coefficients in Mg–Nd system10.1016/j.scriptamat.2015.06.010 ↗
26. Influence of texture and grain size on work hardening and ductility in magnesium-based alloys processed by ECAP and rolling10.1016/j.actamat.2006.05.018 ↗
27. The effect of twinning on dynamic recrystallization behavior of Mg-Gd-Y alloy during hot compression10.1016/j.jallcom.2019.06.279 ↗
28. Identification of NdH2 particles in solution-treated Mg–2.5%Nd (wt.%) alloy10.1016/j.jallcom.2009.06.040 ↗
29. A taylor model based description of the proof stress of magnesium AZ31 during hot working10.1007/s11661-003-0146-5 ↗
30. Dynamic recrystallization and texture development during hot deformation of magnesium alloy AZ3110.1016/S1003-6326(08)60228-9 ↗
31. Dynamic evolution of new grains in magnesium alloy AZ31 during hot deformation10.2320/matertrans.44.197 ↗
32. Enhanced deformation mechanisms by anisotropic plasticity in polycrystalline Mg alloys at room temperature10.1007/s11661-005-0032-4 ↗
33. Effect of initial microstructure on the dynamic recrystallization behavior of Mg-Gd-Y-Zr alloy10.1016/j.msea.2012.07.021 ↗
34. Dynamic and post-dynamic recrystallization under hot, cold and severe plastic deformation conditions10.1016/j.pmatsci.2013.09.002 ↗
35. Enhanced mechanical properties of a hot-extruded AZ80 Mg alloy rod by pre-treatments and post-hot compression10.1016/j.jallcom.2017.12.296 ↗
36. Effect of β-Mg17Al12 phase on microstructure, texture and mechanical properties of AZ91 alloy processed by asymmetric hot rolling10.1016/j.msea.2018.09.086 ↗
37. Deformation mechanisms and recrystallization behavior of Mg-3Al-1Zn and Mg-1Gd alloys deformed by electroplastic-asymmetric rolling10.1016/j.msea.2018.09.041 ↗
38. Dynamic precipitation and dynamic recrystallization during hot deformation of a solutionized WE43 magnesium alloy10.1016/j.msea.2019.138076 ↗
39. Effects of initial texture on the three-dimensional creep anisotropic behaviors of dilute Mg-Y binary alloy sheets10.1016/j.msea.2019.138336 ↗
40. On the role of non-basal deformation mechanisms for the ductility of Mg and Mg-Y alloys10.1016/j.actamat.2010.08.031 ↗
41. Creep behaviors of hot compressed Mg-4Y-2Nd-0.2Zn-0.5Zr alloy with and without aging10.1016/j.msea.2017.10.014 ↗
42. Influence of pre-straining on creep behaviors of Mg-2Y alloy sheets10.1016/j.jallcom.2019.07.249 ↗
43. Precipitation and hardening in magnesium alloys10.1007/s11661-012-1217-2 ↗
44. Hardening precipitation in a Mg-4Y-3RE alloy10.1016/S1359-6454(03)00391-4 ↗
45. Precipitation in magnesium alloy WE54 during isothermal ageing at 250°C10.1016/S1359-6462(99)00084-6 ↗
46. The activity of non-basal slip systems and dynamic recovery at room temperature in fine-grained AZ31B magnesium alloys10.1016/S1359-6454(03)00005-3 ↗
47. Effect of precipitate shape on slip and twinning in magnesium alloys10.1016/j.actamat.2010.11.060 ↗