Effect of non-equilibrium heat treatments on microstructure and tensile properties of an Al-Si-Cu alloy
Source abstract
Abstract
Abstract The influence of heat treatment on the morphology of s-Al 5 FeSi inclusions in Fe-rich Al-Si-Cu was investigated and the tensile properties were improved. Samples were sand casted and subjected to various T6 heat treatments. Metallographic samples were examined by optical microscopy as well as scanning electron microscopy (SEM) and the average length and area fraction of the Fe-rich phases were quantified with image analysis software. It was found that a minimum solution temperature at 520–525 °C and solution time of 1 h is required for a significant fragmentation and dissolution of the detrimental long-needle-like s-Al 5 FeSi inclusions. Solution time longer than 2 h leads to incipient melting of Cu-rich phases and coarsening of the eutectic Si. Tensile specimens were machined from the heat-treated samples and tensile tests performed. The highest ultimate tensile corresponds to the samples heat treated at 525 °C for 1.5 h. Fracture surface observations indicate a transgranular cleavage mechanism for the non-treated specimens, and massive s-Al 5 FeSi platelets were identified as main crack initiation sites. After heat treatment, a mixed fracture mode and dissolved s-Al 5 FeSi phases were observed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. P.D. Lee, T.C. Lindley, C.W.J. Cheong, G.R. Davis, J. Elliott, in: Proceedings of COM, Vancouver, BC, 2003. p. 457.
2. Aluminum industry and climate change – assessment and responses10.1007/s11837-010-0027-5 ↗
3. EAA/OEA Recycling Division, Aluminum recycling in Europe, European Aluminum 2007, 1, 51.
4. A micro-cell model of the effect of microstructure and defects on fatigue resistance in cast aluminum alloys10.1016/j.actamat.2004.07.035 ↗
5. Effect of Fe-content on fatigue crack initiation and propagation in a cast aluminum–silicon alloy (A356–T6)10.1016/S0921-5093(04)00964-5 ↗
6. Effect of Heat Treatment on Morphology of Fe-Rich Intermetallics in hypereutectic Al-Si-Cu-Ni Alloy with 1.26pct Fe10.1007/s11661-013-1937-y ↗
7. Dissolution of iron intermetallics in Al-Si alloys through nonequilibrium heat treatmen10.1007/BF02670687 ↗
8. Evolution of phases in a recycled Al-Si cast alloy during solution treatment
9. Infuelnce of Sr and Mn additions on intermetallic compound morphologies in Al-Si-Cu-Fe cast alloys10.2320/matertrans.44.2611 ↗
10. Y. Shimizu, Y. Awano, M. Nakamura, in: Paper presented at 96th Casting Congress 1992, Milwaukee, WI, AFS no. 92:135.
11. Dissolution and precipitation behaviour during continuous heating of Al–Mg–Si alloys in a wide range of heating rates10.3390/ma8052830 ↗
12. Continuous cooling precipitation diagram of cast aluminium alloy Al–7Si–0.3Mg10.1016/S1003-6326(14)63308-2 ↗
13. The quench sensitivity of cast Al-7Si-0.4Mg alloy10.1007/BF02595647 ↗
14. Microstructural aspects of the dissolution and melting of AI2Cu phase in AI-Si alloys during solution heat treatment10.1007/BF02651928 ↗
15. Porosity formation in AI-9 Wt Pct Si-3wt Pct Cu alloy systems: Metallographic observations10.1007/BF02648419 ↗