journal article·2020-05Open access

Influence of C content and annealing temperature on the microstructures and tensile properties of Fe–13Mn–8Al–(0.7, 1.2)C steels

Dong Han, Hua Ding, Degang Liu, Bernard Rolfe, Hossein Beladi

Abstract

Abstract In the present work, the Fe-13Mn-8Al-(0.7, 1.2)C steels were subjected to different post-cold rolling annealing treatments in a temperature range of 800–1000 °C for 15 min to investigate the microstructural evolution and the mechanical properties. Both steels annealed at 800 °C consisted of fine austenite and ferrite grains along with intergranular κ-carbides formed by eutectoid reaction, which contributed to the high strength but deteriorated ductility. With annealing temperature increasing, the volume fraction of ferrite and intergranular κ-carbides progressively decreased. Meanwhile, the precipitation of intragranular κ′-carbides enhanced the yield strength, whereas coarse austenite was harmful to both strength and elongation. The increase in C content increased the volume fraction of intergranular κ-carbides and austenite as well as retarded the austenite recrystallization, which further increased strength and strain hardening rate but deteriorate ductility. The deformation mechanism in austenite was massive planar slip. The microbands were widely observed in both steels at an annealing temperature above 900 °C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. Austenite growth and stability in medium Mn, medium Al Fe-C-Mn-Al steels10.1016/j.commatsci.2016.08.041 ↗
2. Effect of annealing temperature on microstructural modification and tensile properties in 0.35 C–3.5 Mn–5.8 Al lightweight steel10.1016/j.actamat.2013.04.038 ↗
3. Influence of Al content and precipitation state on the mechanical behavior of austenitic high-Mn low-density steels10.1016/j.scriptamat.2012.08.038 ↗
4. Microband-induced plasticity in a high Mn–Al–C light steel10.1016/j.msea.2008.05.042 ↗
5. Microstructures and mechanical properties of high-strength Fe-Mn-Al-C light-weight TRIPLEX steels10.1002/srin.200606440 ↗
6. Current state of Fe-Mn-Al-C low density steels10.1016/j.pmatsci.2017.05.002 ↗
7. Novel 1.5 GPa-strength with 50%-ductility by transformation-induced plasticity of non-recrystallized austenite in duplex steels10.1038/s41598-017-01514-9 ↗
8. Dramatic improvement of strain hardening and ductility to 95% in highly-deformable high-strength duplex lightweight steels10.1038/s41598-017-02183-4 ↗
9. Excellent combination of strength and ductility in an Fe–9Al–28Mn–1.8C alloy10.1016/j.scriptamat.2010.03.038 ↗
10. High strength and ductile low density austenitic FeMnAlC steels: simplex and alloys strengthened by nanoscale ordered carbides10.1179/1743284714Y.0000000515 ↗
11. Evolution of microstructure and mechanical properties during thermomechanical processing of a low-density multiphase steel for automotive application10.1016/j.actamat.2014.04.031 ↗
12. Effect of carbon content on cracking phenomenon occurring during cold rolling of three light-weight steel plates10.1007/s11661-010-0456-3 ↗
13. Deformation behavior of ferrite–austenite duplex lightweight Fe–Mn–Al–C steel10.1016/j.scriptamat.2011.12.026 ↗
14. Microstructural evolution and strain hardening behavior during plastic deformation of Fe–12Mn–8Al–0.8C steel10.1016/j.msea.2013.07.023 ↗
15. Tensile deformation of a duplex Fe–20Mn–9Al–0.6C steel having the reduced specific weight10.1016/j.msea.2011.03.045 ↗
16. Tensile deformation of a low density Fe–27Mn–12Al–0.8C duplex steel in association with ordered phases at ambient temperature10.1016/j.msea.2013.07.094 ↗
17. Stacking fault energy and plastic deformation of fully austenitic high manganese steels: effect of Al addition10.1016/j.msea.2010.02.058 ↗
18. Control of inter/intra-granular κ-carbides and its influence on overall mechanical properties of a Fe-11Mn-10Al-1.25C low density steel10.1016/j.msea.2017.12.102 ↗
19. Microstructures and mechanical behavior of Fe-18Mn-10Al-(0.8-1.2)C steels
20. Recrystallization behavior in a low-density high-Mn high-Al austenitic steel undergone thin strip casting process10.1016/j.msea.2018.07.023 ↗
21. Deformation mechanisms in ultrahigh-strength and high-ductility nanostructured FeMnAlC alloy10.1016/j.jallcom.2013.10.153 ↗
22. Effect of aging on the microstructure and deformation behavior of austenite base lightweight Fe–28Mn–9Al–0.8C steel10.1016/j.scriptamat.2010.07.036 ↗
23. Modulated structure and magnetic properties of age-hardenable Fe-Mn-Al-C alloys10.1007/BF02656419 ↗
24. Influence of Al content on the strain-hardening behavior of aged low density Fe–Mn–Al–C steels with high Al content10.1016/j.msea.2015.05.002 ↗
25. Effect of annealing temperature on the microstructure and tensile properties of Fe–10Mn–10Al–0.7C low-density steel10.1016/j.matdes.2015.11.115 ↗
26. High-strength Fe-20Mn-Al-C-based alloys with low density10.2355/isijinternational.50.893 ↗
27. Microstructural developments and tensile properties of lean Fe-Mn-Al-C lightweight steels
28. On the eutectoid reaction in a quaternary Fe-C-Mn-Al alloy: austenite → ferrite + kappa-carbide + M23C6 carbide10.1007/s11661-013-2083-2 ↗
29. Thermo-Calc & DICTRA, computational tools for materials science10.1016/S0364-5916(02)00037-8 ↗
30. Novel ultra-high-strength (ferrite plus austenite) duplex lightweight steels achieved by fine dislocation substructures (Taylor lattices), grain refinement, and partial recrystallization10.1016/j.actamat.2015.06.024 ↗
31. Tensile deformation of a low density Fe-27Mn-12Al-0.8C duplex steel in association with ordered phases at ambient temperature10.1016/j.msea.2013.07.094 ↗
32. Microstructural evolution and strain hardening behavior during plastic deformation of Fe-12Mn-8Al-0.8C steel10.1016/j.msea.2013.07.023 ↗
33. 2013
34. Effect of carbon content on the recrystallization kinetics of Nb-steels10.1016/j.scriptamat.2007.02.029 ↗
35. Strengthening of FeMnAlC alloys during aging
36. Combined atom probe tomography and density functional theory investigation of the Al off-stoichiometry of κ-carbides in an austenitic Fe–Mn–Al–C low density steel10.1016/j.actamat.2016.01.007 ↗
37. Effect of alloying additions on the κ phase precipitation in austenitic Fe-Mn-Al-C alloys10.1016/0956-716X(94)90610-6 ↗
38. A simple method to produce austenite-based low-density Fe–20Mn–9Al–0.75C steel by a near-rapid solidification process10.1016/j.msea.2016.10.044 ↗
39. Tensile deformation behavior analysis of low density Fe–18Mn–10Al–xC steels10.1016/j.msea.2015.11.071 ↗
40. Ferrite effects in Fe-Mn-Al-C triplex steels10.1007/s11661-013-1990-6 ↗
41. Effects of aluminum content on cracking phenomenon occurring during cold rolling of three ferrite-based lightweight steel10.1016/j.actamat.2013.06.004 ↗
42. Correlation of microstructure and cracking phenomenon occurring during hot rolling of lightweight steel plates10.1007/s11661-009-0081-1 ↗
43. Fracture of brittle particles in a ductile matrix10.1007/BF00018353 ↗
44. Derivation and variation in composition-dependent stacking fault energy maps based on subregular solution model in high-manganese steels10.1007/s11661-009-0050-8 ↗
45. On the transitions of deformation modes of fully austenitic steels at room temperature10.1007/s12540-010-0001-3 ↗
46. Substructure induced twinning in low density steel10.1016/j.scriptamat.2016.10.001 ↗
47. A model for the grain size dependent work hardening of copper10.1016/j.scriptamat.2006.05.018 ↗