Effect of microstructure on work hardening behaviour of IN-617 alloy
Source abstract
Abstract
Abstract Work hardening behaviour of the IN-617 alloy under tensile loading was studied in the solution treated, aged, and cold worked conditions at room temperature (RT) and 700 °C. Double logarithmic plots of the true stress and logarithmic plastic strain of this alloy displayed upward concave shape similar to those of other austenitic superalloys. Five different relationships between the true stress and logarithmic plastic strain were analyzed to characterize the flow behaviour of this alloy. The relationship proposed by Ludwigson was found to have best fit with the experimental data. Three stages of the instantaneous work hardening rate (θ) were observed in the solution treated and the aged conditions whereas only stage I was exhibited in the cold worked condition of the alloy. Transmission electron microscopy (TEM) revealed traces of slip bands in the samples tested at RT and micro twins as well their interaction with dislocations and precipitation of new carbides was observed in the samples tested at 700 °C. There was typical ductile fracture with dimples in both the solution treated and aged conditions whereas there was faceted fracture in the cold worked condition both at RT and 700 °C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High Temperature Alloys and Creep · Metallurgy and Material Forming · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Qualification of Ni-based alloys for advanced ultra super critical plants10.1016/j.proeng.2013.03.245 ↗
2. Development of nickel alloys based on alloy 617 for components in 700°C power plants10.1016/j.proeng.2013.03.247 ↗
3. Materials issues for turbines for operation in ultra-supercritical steam
4. Materials for ultra-supercritical coal-fired power plant boilers10.1016/j.ijpvp.2006.08.006 ↗
5. Nickel-base superalloys for ultra-supercritical coal-fired power plants: fireside corrosion. Laboratory studies and power plant exposures10.1016/j.fuel.2012.11.081 ↗
6. Nickel-base alloy solutions for ultra super critical steam power plants10.1016/j.proeng.2013.03.246 ↗
7. Microstructure and phase stability of Inconel alloy 61710.1007/BF02643879 ↗
8. Inconel alloy 617 – new high temperature alloy
9. Precipitation behavior of Ni-Cr-22 Fe-18 Mo (Hastelloy-X) and Ni-Cr-22 Co-12 Mo (Inconel-617) after isothermal aging10.13182/NT84-A33462 ↗
10. Effects of thermal aging on the microstructure and mechanical properties of a commercial Ni-Cr-Co-Mo alloy (Inconel 617)10.1007/BF02659828 ↗
11. High temperature aging and corrosion study on alloy 617 and alloy 23010.1115/1.4002819 ↗
12. Microstructure of long-term aged IN617 Ni-base superalloy10.1007/s11661-008-9618-y ↗
13. Investigation of thermal aging effects on the tensile properties of Alloy 617 by in-situ synchrotron wide-angle X-ray scattering10.1016/j.msea.2015.10.098 ↗
14. Microstructure and high temperature mechanical properties of Inconel 617
15. High temperature indentation based property measurements of IN-61710.1016/j.ijplas.2017.05.007 ↗
16. Elevated temperature mechanical properties of Inconel 617 surface oxide using nano indentation10.1016/j.msea.2020.139539 ↗
17. Creep behaviour of as received, aged and cold worked Inconel 617 at 850oC and 950oC10.1016/j.jnucmat.2010.01.019 ↗
18. Effect of thermo-mechanical processing on microstructure and creep properties of the foils of alloy 61710.1016/j.jnucmat.2009.02.029 ↗
19. Wright · 2014
20. A study of tensile flow and work-hardening behavior of alloy 61710.1007/s11665-018-3345-3 ↗
21. Tensile deformation
22. Modified stress-strain relation for FCC metals and alloys10.1007/BF02813258 ↗
23. Ludwik · 1909 · 32
24. Plastic instability under plane stress10.1016/0022-5096(52)90002-1 ↗
25. A practical strain hardening function
26. Dynamic strain aging, deformation and fracture behaviour of the nickel base superalloy Inconel 61710.1016/j.msea.2018.10.123 ↗
27. Wright · 2006
28. Tensile flow and work-hardening behavior of a Ti-modified austenitic stainless steel10.1007/s11661-997-0092-8 ↗
29. Strain hardening behaviour of a nickel based superalloy supercast 247A
30. Tensile flow and work hardening behaviour of 9Cr–1Mo ferritic steel in the frame work of Voce relationship10.1016/j.msea.2011.05.026 ↗
31. Strain hardening behavior of a Fe–18Mn–0.6 C–1.5 Al TWIP steel10.1016/j.msea.2009.08.028 ↗
32. Work-hardening behaviour of nitrogen-alloyed austenitic stainless steels10.1016/0921-5093(91)90655-7 ↗
33. Low cycle fatigue, deformation and fracture behaviour of Inconel 617 alloy10.1016/j.msea.2019.138286 ↗
34. Effect of Ti/C ratio and prior cold work on the tensile properties of 15Cr-15Ni-2.2 Mo-Ti modified austenitic stainless steel
35. Effect of critical temperatures on microstructures and mechanical properties of Nb–Ti stabilized IF steel processed by multiaxial forging10.1016/j.matdes.2016.03.107 ↗