Microstructure and mechanical properties of hybrid in-situ Ti2AlCw/ Mo2B5p reinforced TiAl alloy
Source abstract
Abstract
Abstract The Ti–48Al–6Nb alloy is reinforced by the addition of the AlMo/B4C inoculant powders after high-energy ball milling. The in-situ reactions in TiAl melt lead to the formation of Ti2AlC whiskers and Mo2B5 nanoparticles. Good interface matching between the in-situ phases and the TiAl alloy is observed, which is the key point leading to the uniform distribution of the in-situ phases in the TiAl matrix. On this basis, the grain size and lamellar width of the alloy are significantly refined. The compression and three-point bending tests show that both the strength and toughness are improved. Casting twinning between γ-TiAl lamellas is detected in this study, which could be attributed to the internal stress of the melt TiAl as it solidifies. Multiple strengthening and toughening mechanisms induced by the dual-scaled Ti2AlCw and Mo2B5p are the main reason for the improvement on the mechanical properties.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · MXene and MAX Phase Materials · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. Microstructural design and mechanical properties of a cast and heat-treated intermetallic multi-phase γ-TiAl based alloy10.1016/j.intermet.2013.09.010 ↗
2. Prior particle boundaries and microstructural homogenization of a β-solidifying γ-TiAl alloy fabricated from prealloyed powder10.1016/j.msea.2018.09.021 ↗
3. Effect of microstructure on fatigue and tensile properties of the gamma TiAl alloy Ti-46.5A1-3.0Nb-2.1Cr-0.2W10.1016/0921-5093(94)03263-7 ↗
4. Variations of microstructure and tensile property of γ-TiAl alloys with 0–0.5 at% C additives10.1016/j.msea.2017.06.019 ↗
5. Design, processing, microstructure, properties, and application of advanced intermetallic TiAl alloys10.1002/adem.201200231 ↗
6. Electron beam melted TiC/high Nb–TiAl nanocomposite: microstructure and mechanical property10.1016/j.msea.2021.141059 ↗
7. Fabrication of nano-TiC reinforced high Nb-TiAl nanocomposites by electron beam melting10.1016/j.matlet.2019.126856 ↗
8. X. F. Lu et al. Mechanical, tribological and electrochemical corrosion properties of in-situ synthesized Al2O3/TiAl composites. Intermetallics.
9. Influence of nano-Y2O3 addition on microstructure and tensile properties of high-Al TiAl alloys10.1016/j.msea.2020.139803 ↗
10. Laser-induced exothermic bonding of carbon fiber/Al composites and TiAl alloys10.1016/j.matdes.2017.04.044 ↗
11. Microstructure evolution and mechanical properties of TiAl binary alloys added with SiC fibers10.1016/j.intermet.2018.04.018 ↗
12. Effect of TiB2 addition on microstructure and fluidity of cast TiAl alloy10.1016/j.vacuum.2020.109210 ↗
13. Effect of scan line spacing on texture, phase and nanohardness of TiAl/TiB2 metal matrix composites fabricated by selective laser melting10.1016/j.jallcom.2017.09.053 ↗
14. Contribution of Orowan strengthening effect in particulate-reinforced metal matrix nanocomposites10.1016/j.msea.2006.10.184 ↗
15. Orowan strengthening and forest hardening superposition examined by dislocation dynamics simulations10.1016/j.actamat.2010.06.028 ↗
16. The improved mechanical properties of Al matrix composites reinforced with oriented β-Si3N4 whisker10.1016/j.jmst.2019.02.003 ↗
17. In situ synthesis of a gamma-Al2O3 whisker reinforced aluminium matrix composite by cold pressing and sintering10.1016/j.msea.2017.10.063 ↗
18. Effects of hot rolling deformation on the microstructure and tensile properties of an in situ-generated ZrB2 nanoparticle-reinforced AA6111 composite10.1016/j.msea.2018.06.107 ↗
19. Fabrication and mechanical properties of WC nanoparticle dispersion-strengthened copper10.1016/j.msea.2021.141274 ↗
20. Strength-ductility trade-off via SiC nanoparticle dispersion in A356 aluminium matrix10.1016/j.msea.2019.138639 ↗
21. Microstructure and melting behavior of tin nanoparticles embedded in alumina matrix processed by ball milling10.1016/j.msea.2014.02.006 ↗
22. Effect of in situ grown carbon nanotubes on the structure and mechanical properties of unidirectional carbon/carbon composites10.1016/j.msea.2010.11.067 ↗
23. In-situ Al2O3-Al interface contribution towards the strength-ductility synergy of Al-CuO composite fabricated by solid-state reactive sintering10.1016/j.scriptamat.2021.113825 ↗
24. Good strength-plasticity compatibility in graphene nanoplatelets/Ti composites by strengthening the interface bonding via in-situ formed TiB whisker10.1016/j.ceramint.2020.09.241 ↗
25. Effects of lamellar boundary structural change on lamellar size hardening in TiAl alloy10.1016/j.actamat.2004.07.029 ↗
26. Effect of fully lamellar morphology on creep of a near γ-TiAl intermetallic10.1016/S0966-9795(98)00019-3 ↗
27. Effect of heating rate on the grain refinement of a TiAl alloy by cyclic heat treatment10.1016/S0921-5093(00)01774-3 ↗
28. Crystallographic aspects of deformation twinning and consequences for plastic deformation processes in γ-TiAl10.1016/S1359-6454(99)00385-7 ↗
29. Formation of deformation twins in TiAl10.1016/S1359-6454(01)00264-6 ↗
30. Recent progress in the development of gamma titanium aluminide alloys10.1002/1527-2648(200011)2:11<699::AID-ADEM699>3.0.CO;2-J ↗
31. Plastic deformation of single crystals of a DO19 compound with an off-stoichiometric composition (Ti-36.5 at.% Al) at room temperature10.1080/01418619308225357 ↗
32. Generalized planar fault energies and mechanical twinning in gamma TiAl alloys10.1016/j.scriptamat.2012.12.032 ↗
33. Self-thickening, cross-slip deformation twinning model10.1063/1.2911735 ↗
34. Phase transformation mechanisms involved in two-phase TiAl-based alloys I. lamellar structure formation10.1016/1359-6454(95)00167-4 ↗
35. The deformation and ageing of mild steel: III discussion of results10.1088/0370-1301/64/9/303 ↗
36. Effects of ultra-refine grain and micro-nano twins on mechanical properties of 51CrV4 spring steel10.1016/j.msea.2017.02.078 ↗
37. Ultrahigh strength and high electrical conductivity in copper10.1126/science.1092905 ↗
38. Nano-sized twins induce high rate sensitivity of flow stress in pure copper10.1016/j.actamat.2005.01.031 ↗
39. The interaction mechanism of screw dislocations with coherent twin boundaries in different face-centered cubic metals10.1016/j.scriptamat.2005.11.072 ↗
40. Interaction between non-screw lattice dislocation and coherent twin boundaries in face-centered cubic metals10.1016/j.actamat.2007.11.020 ↗
41. Deformation mechanisms, length scales and optimizing the mechanical properties of nanotwinned metals10.1016/j.actamat.2011.07.038 ↗
42. Novel design concepts for gamma-base titanium aluminide alloys10.1016/S0966-9795(00)00036-4 ↗
43. Current understanding of creep behaviour of near γ -titanium aluminides10.1179/imr.1995.40.5.197 ↗
44. Twin-boundary assisted crack tip plasticity and toughening in lamellar γ -TiAl10.1016/j.actamat.2021.116924 ↗
45. Kinetics of cyclically-induced mechanical twinning in γ -TiAl unveiled by a combination of acoustic emission, neutron diffraction and electron microscopy10.1016/j.actamat.2021.116921 ↗
46. Nanostructured high-strength molybdenum alloys with unprecedented tensile ductility10.1038/nmat3544 ↗
47. Properties and deformation behaviour of Mg-Y2O3 nanocomposites10.1016/j.actamat.2007.05.032 ↗