Strengthening mechanism and effect of Al2O3 particle on high-temperature tensile properties and microstructure evolution of W–Al2O3 alloys
Source abstract
Abstract
The W–Al2O3 alloy rods were successfully fabricated by the powder metallurgy process and hot swaging. Subsequently, the high-temperature tensile tests were conducted to characterize the mechanical properties of the W–Al2O3 alloy. At 800 °C, the ultimate tensile strength of W-0.25 wt% Al2O3 alloy is 611.1 MPa, which is 18% higher than that of pure W. After tension, the microstructure evolution was evaluated using metallographic microscope and transmission electron microscopy. For the pure W undergoing deformation at 1000 °C, dynamic recrystallization occurs, leading to the sharp decrease of the strength. However, the microstructure of the W-0.25 wt% Al2O3 alloy contains a large number of sub-grain and low-angle grain boundaries, which does not significantly change in the temperature range of 800–1200 oC, and the work hardening plays a leading role during the high-temperature deformation process. Due to high hardness, the dispersed Al2O3 particles effectively prevent the dislocation movement, displaying a significant strengthening effect.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Metal and Thin Film Mechanics · Fusion materials and technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Determination of the DBTT of nanoscale ZrC doped W alloys through amplitude-dependent internal friction technique10.1016/j.msea.2018.01.055 ↗
2. Towards enhanced strength-ductility synergy via hierarchical design in steels: from the material genome perspective.10.1016/j.scib.2021.01.022 ↗
3. Controlled synthesis of high-quality W-Y2O3 composite powder precursor by ascertaining the synthesis mechanism behind the wet chemical method10.1016/j.jmst.2019.05.067 ↗
4. Gradient nanotwinned CrCoNi medium-entropy alloy with strength-ductility synergy10.1016/j.scriptamat.2021.114117 ↗
5. The effect of HfC content on mechanical properties HfC-W composites10.1016/j.ijrmhm.2014.01.012 ↗
6. Current status of nanostructured tungsten-based materials development
7. Effect of mechanical alloying process on microstructure and mechanical properties of ODS tungsten heavy alloys10.1016/j.jallcom.2006.08.284 ↗
8. Processing of fine-grained W materials without detrimental phases and their mechanical properties at 200-432K10.1016/j.msea.2007.03.079 ↗
9. An investigation of the microstructure and ductility of annealed cold-rolled tungsten10.1016/j.actamat.2018.10.002 ↗
10. Flow behavior and processing map for hot deformation of W-1.5ZrO2 alloy10.1016/j.jallcom.2019.06.179 ↗
11. Preparation, microstructure, and constitutive equation of W-0.25 wt% Al2O3 alloy10.1016/j.msea.2018.12.001 ↗
12. The effect of Y2O3 on the grain growth and densification of W matrix during low temperature sintering: experiments and modelling10.1016/j.matdes.2019.108080 ↗
13. Effects of swaging and annealing on the microstructure and mechanical properties of ZrC dispersion-strengthened tungsten10.1016/j.ijrmhm.2018.05.018 ↗
14. Superplastic deformation in W-0.5 wt.% TiC with approximately 0.1 μm grain size10.1016/j.msea.2007.05.009 ↗
15. W-2wt.%Y2O3 composite: microstructure and mechanical properties10.1016/j.msea.2012.01.011 ↗
16. Microstructure and preparation of an ultra-fine-grained W-Al2O3 composite via hydrothermal synthesis and spark plasma sintering10.1016/j.ijrmhm.2017.12.022 ↗
17. Compressive and wear resistance of nanometric alumina reinforced copper matrix composites10.1016/j.matdes.2011.10.021 ↗
18. Nanoscale Alumina-reinforced aluminum matrix composites: microstructure and mechanical properties10.4028/www.scientific.net/KEM.395.157 ↗
19. Establishment of processing map, microstructure and high-temperature tensile properties of W-0.25 wt% Al2O3 alloys10.1016/j.jallcom.2020.154751 ↗
20. Mechanical properties and microstructural change of W-Y2O3 alloy under helium irradiation
21. Evaluation of the intergranular crack growth resistance of ultrafine grained tungsten materials10.1016/j.actamat.2019.06.051 ↗