Load partitioning between ferrite/martensite and dispersed nanoparticles of a 9Cr ferritic/martensitic (F/M) ODS steel at high temperatures
Source abstract
Abstract
Abstract In this study, a high-energy synchrotron radiation X-ray technique was used to investigate the tensile deformation processes of a 9Cr-ODS ferritic/martensitic (F/M) steel at different temperatures. Two minor phases within the 9Cr-ODS F/M steel matrix were identified as Y2Ti2O7 and TiN by the high-energy X-ray diffraction, and confirmed by the analysis using energy dispersive X-ray spectroscopy (EDS) of scanning transmission electron microscope (STEM). The lattice strains of the matrix and particles were measured through the entire tensile deformation process. During the tensile tests, the lattice strains of the ferrite/martensite and the particles (TiN and Y2Ti2O7) showed a strong temperature dependence, decreasing with increasing temperature. Analysis of the internal stress at three temperatures showed that the load partitioning between the ferrite/martensite and the particles (TiN and Y2Ti2O7) was initiated during sample yielding and reached to a peak during sample necking. At three studied temperatures, the internal stress of minor phases (Y2Ti2O7 and TiN) was about 2 times that of F/M matrix at yielding position, while the internal stress of Y2Ti2O7 and TiN reached about 4.5–6 times and 3–3.5 times that of the F/M matrix at necking position, respectively. It indicates that the strengthening of the matrix is due to minor phases (Y2Ti2O7 and TiN), especially Y2Ti2O7 particles. Although the internal stresses of all phases decreased with increasing temperature from RT to 600 °C, the ratio of internal stresses of each phase at necking position stayed in a stable range (internal stresses of Y2Ti2O7 and TiN were about 4.5–6 times and 3–3.5 times of that of F/M matrix, respectively). The difference between internal stress of the F/M matrix and the applied stress at 600 °C is slightly lower than those at RT and 300 °C, indicating that the nanoparticles still have good strengthening effect at 600 °C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fusion materials and technologies · Metal and Thin Film Mechanics · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Odette · Annu. Rev. Mater. Res. · 2008 · 38 · 47110.1146/annurev.matsci.38.060407.130315 ↗
2. Ukai · J. Nucl. Sci. Technol. · 2002 · 39 · 87210.1080/18811248.2002.9715271 ↗
3. Kim · Nucl. Eng. Technol. · 2008 · 40 · 30510.5516/NET.2008.40.4.305 ↗
4. Yamashita · J. Nucl. Mater. · 2007 · 367 · 20210.1016/j.jnucmat.2007.03.145 ↗
5. Lindau · Fusion Eng. Des. · 2005 · 75 · 98910.1016/j.fusengdes.2005.06.186 ↗
6. Klimiankou · J. Cryst. Growth · 2003 · 249 · 38110.1016/S0022-0248(02)02134-6 ↗
7. Ohnuma · Acta Mater. · 2009 · 57 · 557110.1016/j.actamat.2009.07.054 ↗
8. Heintze · J. Nucl. Mater. · 2012 · 428 · 13910.1016/j.jnucmat.2011.08.053 ↗
9. Miller · Mater. Sci. Eng. A · 2003 · 353 · 14010.1016/S0921-5093(02)00680-9 ↗
10. Williams · J. Nucl. Mater. · 2010 · 400 · 3710.1016/j.jnucmat.2010.02.007 ↗
11. Klimiankou · J. Nucl. Mater. · 2004 · 329 · 34710.1016/j.jnucmat.2004.04.083 ↗
12. Mo · J. Nucl. Mater. · 2014 · 455 · 37610.1016/j.jnucmat.2014.06.060 ↗
13. Miao · Mater. Charact. · 2015 · 105
14. Pan · J. Nucl. Mater. · 2010 · 398 · 22010.1016/j.jnucmat.2009.10.035 ↗
15. Pan · J. Nucl. Mater. · 2010 · 407 · 1010.1016/j.jnucmat.2010.07.003 ↗
16. Hedström · Acta Mater. · 2010 · 58 · 73410.1016/j.actamat.2009.09.053 ↗
17. Hedström · Metall. Mater. Trans. A · 2009 · 40 · 103910.1007/s11661-009-9807-3 ↗
18. Young · Acta Mater. · 2007 · 55 · 199910.1016/j.actamat.2006.11.004 ↗
19. Alvarez · Acta Mater. · 2012 · 60 · 689210.1016/j.actamat.2012.07.029 ↗
20. Qu · Acta Mater. · 2013 · 61 · 32110.1016/j.actamat.2012.09.062 ↗
21. Stock · J. Struct. Biol. · 2008 · 161 · 14410.1016/j.jsb.2007.10.001 ↗
22. Deymier-Black · J. Mech. Behav. Biomed. Mater. · 2013 · 21 · 1710.1016/j.jmbbm.2013.01.016 ↗
23. Singhal · Mater. Sci. Eng. C · 2013 · 33 · 146710.1016/j.msec.2012.12.069 ↗
24. Singhal · Adv. Eng. Mater. · 2013 · 15 · 23810.1002/adem.201200204 ↗
25. Zhang · J. Nucl. Mater. · 2014
26. Zhang · Fusion Eng. Des. · 2014 · 89 · 28010.1016/j.fusengdes.2014.01.067 ↗
27. Liss · Mater. Sci. Eng. A · 2010 · 528 · 1110.1016/j.msea.2010.06.017 ↗
28. Ramar · J. Nucl. Mater. · 2008 · 382 · 21010.1016/j.jnucmat.2008.08.009 ↗
29. R.E. Reed-Hill, R. Abbaschian, Brooks/Cole Engineering Division, (1973).
30. Mo · J. Nucl. Mater. · 2013 · 441 · 69510.1016/j.jnucmat.2013.03.083 ↗
31. Mariappan · J. Nucl. Mater. · 2013 · 435 · 20710.1016/j.jnucmat.2012.12.049 ↗
32. Kaona · BMC Public Health · 2004 · 4 · 6810.1186/1471-2458-4-68 ↗
33. Nye · 1985
34. Luan · 2011
35. Steneteg · Phys. Rev. B · 2013 · 87 · 09411410.1103/PhysRevB.87.094114 ↗
36. He · Scr. Mater. · 2011 · 64 · 54810.1016/j.scriptamat.2010.11.042 ↗
37. Zhang · Surf. Coat. Technol. · 2001 · 142 · 12510.1016/S0257-8972(01)01221-X ↗
38. Kim · J. Appl. Phys. · 1992 · 72 · 180510.1063/1.351651 ↗
39. Meng · Thin Solid Films · 1995 · 271 · 10810.1016/0040-6090(95)06875-9 ↗
40. Andrievskii · 1989
41. Weisser · Acta Mater. · 2011 · 59 · 444810.1016/j.actamat.2011.03.068 ↗
42. E. Orowan, in: Proceedings of the Symposium on Internal Stresses in Metals and Alloys, Institute of Metals, London, (1948).
43. Herrick · Scr. Metall. · 1988 · 22 · 187910.1016/S0036-9748(88)80230-8 ↗