journal article·2017-02

Fracture toughness of type 316LN stainless steel welded joints

Wenhua Gao, Kai Chen, Xianglong Guo, Lefu Zhang

Publisher page

Abstract

Abstract The fracture toughness of two types 316LN welded joints in different orientations at 300 K and 623 K in air was investigated. The tests were conducted using single specimen method, where J-R curves and fracture toughness values (J0.2) were obtained. Microstructure of the specimens were characterized before and after the test. Results show that 2GT welded joint exhibits higher toughness as compared to 5GT welded joint, and orientation has slight effect on the fracture toughness. Moreover, the fracture toughness drops remarkably with the increase of temperature.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fatigue and fracture mechanics · Hydrogen embrittlement and corrosion behaviors in metals · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Aging of cast duplex stainless steels in LWR systems10.1016/0029-5493(85)90069-X ↗
2. Flaw evaluation of thermally aged cast stainless steel in light-water reactor applications10.1016/S0308-0161(97)00007-0 ↗
3. Effect of nitrogen addition and test temperatures on elastic-plastic fracture toughness of SS316LN10.1016/j.proeng.2014.11.042 ↗
4. Environmentally assisted cracking of types 304L/316L/316NG stainless steel in 288 C water10.5006/1.3582044 ↗
5. Characterization of microstructure and local deformation in 316NG weld heat-affected zone and stress corrosion cracking in high temperature water10.1016/j.corsci.2011.02.009 ↗
6. H.P. Seifert, S. Ritter, Environmentally-Assisted Cracking in Austenitic Light Water Reactor Structural Materials – Final Report of the KORA-I Project, PSI Report No. 09–03, Paul Scherrer Institute, Villigen PSI, Switzerland, 2009.
7. A review of the effects of coolant environments on the fatigue life of LWR structural materials10.1115/1.3027496 ↗
8. ASTME1820-01 · 2001
9. Castro · 1974
10. Prediction of austenitic weld metal microstructure and properties
11. Weld defects in austenitic stainless steel sheet-effect of welding parameters
12. SCC crack growth rate of cold worked 316L stainless steel in PWR environment10.1016/j.jnucmat.2014.09.054 ↗
13. ASTM E1820-11 · 2011
14. A review of irradiation effects on LWR core internal materials–IASCC susceptibility and crack growth rates of austenitic stainless steels10.1016/j.jnucmat.2010.12.001 ↗
15. Abramson · Met. Trans. A · 1985 · 16 · 10110.1007/BF02656717 ↗
16. Srawley · Engng. Fract. Mech. · 1972 · 2 · 58710.1016/0013-7944(72)90069-0 ↗
17. RCC-MR, Design and Construction Rules for Mechanical Components of FBR Nuclear Islands AFCEN, Paris, France, 2002.
18. Fracture toughness of type 304 and 316 stainless steels and their welds10.1179/imr.1997.42.2.45 ↗
19. Application of the normalization method for the determination of J–R curves10.1016/j.msea.2004.01.067 ↗
20. Evaluation of quasistatic fracture toughness of a modified 9Cr-1Mo (P91) steel10.1016/j.msea.2007.06.021 ↗
21. Samuel · Int. J. Pre. Ves. Pip. · 1990 · 41 · 5910.1016/0308-0161(90)90077-U ↗
22. Hull · 1999
23. Fracture toughness of iso 3183×80M (API 5L X80) steel friction stir welds10.1016/j.engfracmech.2010.07.022 ↗
24. Fatigue crack propagation in API 5L X-70 pipeline steel longitudinal welded joints under constant and variable amplitudes10.1111/j.1460-2695.2010.01521.x ↗
25. Role of grain boundary engineering in the SCC behavior of ferritic–martensitic alloy HT-910.1016/j.jnucmat.2006.12.006 ↗
26. Tensile and stress corrosion cracking behavior of ferritic–martensitic steels in supercritical water10.1016/j.jnucmat.2009.09.012 ↗
27. Characterization of elastic-plastic fracture behavior of type 347 stainless steel piping materials. fatigue and fracture mechanics in pressure vessels and piping
28. JR fracture properties of SA508-1a ferritic steels and SA312-TP347 austenitic steels for pressurized water reactor's (PWR) primary coolant piping10.1016/S0029-5493(99)00061-8 ↗
29. Preferred orientation in the weld fusion zone
30. Influence of ageing on the quasistatic fracture toughness of an SS 316(N) weld at ambient and elevated temperatures10.1016/j.jnucmat.2010.11.001 ↗
31. Byun · J. Nucl. Mater. · 2010 · 407 · 7810.1016/j.jnucmat.2010.09.031 ↗
32. Capdevila · Mater. Sci. Technol. · 2013 · 29 · 117910.1179/1743284713Y.0000000215 ↗