Experimental investigation into the crack propagation in multiphase tantalum carbide ceramics
Source abstract
Abstract
Abstract Tantalum carbide ceramics with high volume fractions of the ζ-Ta4C3 phase have been shown to exhibit high fracture strength and toughness as compared to those in absence of this phase. In this work, we investigated how microcracks propagated in this these high toughness ceramics using Knoop and Vickers microindentation. The Knoop indentations demonstrated that cracking preferentially occurred parallel to the lath structure in ζ-Ta4C3; however shorter cracks did form between the laths when a sufficient driving force was present. The resulting crack path was tortuous providing direct evidence for toughening through crack deflection; however, the microscale nature of the work cannot rule out crack bridging as a toughening mechanism as well. Plasticity is also observed under the indents, but is likely a result of the high confining pressures that occurred during indentation allowing for plastic flow.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. Fahrenholtz · 2010
2. Ultra high temperature ceramic composites
3. Phase constitution and mechanical properties of carbides in the Ta–C system10.1111/j.1551-2916.2009.03201.x ↗
4. Microstructure and mechanical properties of spark plasma sintered Tac0.7 ceramics10.1111/j.1551-2916.2010.03908.x ↗
5. Microstructural formations and phase transformation pathways in hot isostatically pressed tantalum carbides10.1016/j.actamat.2011.09.036 ↗
6. Effect of processing induced particle alignment on the fracture toughness and fracture behavior of multiphase dental ceramics10.1016/j.dental.2009.03.013 ↗
7. Toughening and strengthening mechanism of zirconia-alumina multiphase ceramics10.4028/www.scientific.net/KEM.249.167 ↗
8. Studies on the strengthening of silicon carbide-based multiphase ceramics I: the SiC-TiC system10.1016/0921-5093(89)90621-7 ↗
9. Damage tolerance and R-curve behavior of Al2O3–ZrO2–Nb multiphase composites with synergistic toughening mechanism10.1557/JMR.2008.0075 ↗
10. Microstructures and toughening behaviors of lined Al2O3-ZrO2 multiphase ceramics in Shs composite pipes10.4028/www.scientific.net/MSF.423-425.177 ↗
11. Al-B-C phase development and effects on mechanical properties of B4C/Al-derived composites10.1111/j.1151-2916.1995.tb08801.x ↗
12. Ashby · 1992
13. Relationship between microstructure, toughening mechanisms, and fracture toughness of reinforced silicon nitride ceramics10.1111/j.1151-2916.1995.tb08031.x ↗
14. E.K. Storms, The tantalum-tantalum carbide system, in: The Refractory Carbides, Academic Press, 1967.10.1016/B978-1-4832-3070-2.50004-5 ↗
15. Structure of non-stoichiometric TaC10.1016/0025-5416(75)90174-3 ↗
16. Variations in tantalum carbide microstructures with changing carbon content10.1111/j.1744-7402.2012.02761.x ↗
17. z–Ta4C3−x: a high fracture toughness carbide with rising-crack-growth-resistance (R-curve) behavior10.1111/jace.13635 ↗
18. A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
19. Indentation fracture: principles and applications10.1007/BF00823224 ↗
20. Fracture toughness anisotropy of sodium β-alumina10.1111/j.1151-2916.1983.tb10573.x ↗
21. Nanocrystalline hydroxyapatite with simultaneous enhancements in hardness and toughness10.1016/j.biomaterials.2009.08.048 ↗
22. Anisotropy in room temperature microhardness and fracture of CaWO 4 scheelite10.1016/j.actamat.2004.08.022 ↗
23. Knoop hardness and fracture anisotropy of calcite10.1007/BF00609168 ↗
24. Anisotropic hardness and fracture toughness of highly aligned YBa2Cu3O7–δ10.1063/1.351090 ↗
25. Use of the notched beam test for evaluation of fracture energies of ceramics10.1111/j.1151-2916.1974.tb10843.x ↗
26. Use of notched beams to measure the toughness of ceramics
27. Fracture toughness using the SEVNB method: preliminary results10.1002/9780470294444.ch18 ↗
28. S. Dionne, T. Lang, J. Li, Examination of fatigue crack origins in aircraft turbine blades using serial sectioning techniques. in: Proceedings of the 12th International Conference on Fracture. International Congress on Fracture, 2009.
29. 3d microstructural characterization of nickel superalloys via serial-sectioning using a dual beam fib-sem10.1016/j.scriptamat.2006.02.039 ↗
30. 00-035-0801 TaC, in ICDD Database, International Centre for Diffraction Data, 2009.
31. Atomic and vacancy ordering in carbide z-Ta4C3−X (0.28⩽X⩽0.40) and phase equilibria in the Ta–C system10.1016/j.jssc.2007.09.015 ↗
32. Lutterotti, L., S. Matthies, and H. R. Wenk. MAUD (material analysis using diffraction): a user friendly Java program for Rietveld texture analysis and more, in: Proceeding of the Twelfth International Conference on Textures of Materials (ICOTOM-12), NRC Research Press Ottowa, Canada, vol. 1, 1999.
33. Ab initio investigations of the phase stability in tantalum carbides10.1016/j.actamat.2014.07.070 ↗
34. Influence of carbon vacancy formation on the elastic constants and hardening mechanisms in transition metal carbides10.1016/j.jeurceramsoc.2014.08.021 ↗
35. Microstructure and mechanical properties of the spark plasma sintered Ta2c ceramics10.1016/j.ceramint.2012.02.055 ↗
36. Mechanisms of fatigue-crack propagation in ductile and brittle solids10.1023/A:1018655917051 ↗
37. Small fatigue cracks: a statement of the problem and potential solutions10.1016/0025-5416(86)90217-X ↗
38. Measurement of the thermal properties of zirconium and tantalum carbides at high temperatures (up to and above the melting point)10.1007/s11018-011-9828-3 ↗
39. Thermal properties of tantalum monocarbide and tungsten monocarbide
40. Synthesis and characterization of Ti3alc210.1111/j.1151-2916.2000.tb01281.x ↗
41. Fatigue-crack growth and fracture properties of coarse and fine-grained Ti3SiC210.1016/S1359-6462(99)00427-3 ↗
42. Damage mechanisms around hardness indentations in Ti3SiC210.1111/j.1151-2916.1997.tb02861.x ↗
43. First-principles study on surface stability of tantalum carbides10.1016/j.susc.2015.09.003 ↗
44. Elevated-temperature deformation mechanisms in Ta2C: an experimental study10.1016/j.actamat.2013.01.043 ↗
45. Dislocation nucleation from a crack tip: an analysis based on the Peierls concept10.1016/S0022-5096(05)80012-2 ↗
46. Crack tip dislocation nucleation in FCC solids10.1103/PhysRevLett.82.1700 ↗
47. The dislocation structure of crack tip plastic zones in a cobalt base superalloy10.1016/S0167-577X(98)00031-7 ↗
48. Hvem study of crack-tip dislocations in Si crystals prepared by FIB and twin-blade cutting method10.1093/jmicro/dfh052 ↗
49. Dynamic emission of screw dislocations from a propagating crack tip10.1063/1.364260 ↗
50. On the toughening of brittle materials by grain bridging: promoting intergranular fracture through grain angle, strength, and toughness10.1016/j.jmps.2007.12.006 ↗
51. Graphene nanoplatelets reinforced tantalum carbide consolidated by spark plasma sintering10.1016/j.msea.2013.06.006 ↗