Tailoring microstructure and tensile properties of Mg-Si alloys varying solidification cooling rate and Si content
Source abstract
Abstract
Abstract Mg-Si alloys were investigated in terms of their microstructural characteristics and tensile properties, by varying solidification cooling rate and Si content. This type of investigation becomes essential since these alloys are considered potentially base alloys for new biocompatible and biodegradable materials that might be used to produce a variety of temporary implants. This because Silicon (Si) has been recognized as a vital mineral in the human body, aiding both the healing process and the development of the immune system. Despite these characteristics provided by Si, Mg-Si alloys typically have low ductility and tensile strength due to the presence of coarse Mg2Si particles. Therefore, efforts to understand and improve these properties are most welcome. In order to deepen the knowledge of these alloys, the present research analyzed three Mg-Si alloys: Mg-0.6 wt% Si, Mg-1.3 wt% Si and Mg-1.7 wt% Si regarding their microstructures and phase's morphologies produced in a broad range of solidification rates' samples and their corresponding tensile properties. The predominance of dendritic arrangement with the interdendritic region composed of the (Mg + Mg2Si) eutectic was noted for the Mg-0.6 wt% Si and Mg-1.7 wt% Si alloys. Eutectic cells prevailed for the Mg-1.3 wt% Si alloy, with cells varying from squarer and hexagonal to a more rounded shape with the decrease in cooling rate. Experimental influences of the microstructural parameters on the tensile properties have been verified. Except for the Mg-1.3 wt% Si alloy, the tensile properties of the other alloys were found to be roughly independent of the dendritic length scales in the verified ranges. In general, increased Si content led to a reduction in strength and ductility, probably due to the increase in the fraction of Mg2Si particles, which is an effective phase in the stress concentration during loading, shortening the break.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. In vitro and in vivo corrosion measurements of magnesium alloys10.1016/j.biomaterials.2005.07.037 ↗
2. In vivo corrosion behavior of Mg-Mn-Zn alloy for bone implant application10.1002/jbm.a.31273 ↗
3. Effect of magnesium ion on human osteoblast activity10.1590/1414-431x20165257 ↗
4. Updates on the research and development of absorbable metals for biomedical applications10.1007/s40204-018-0091-4 ↗
5. Microstructural evolution in Mg-Zn alloys during solidification: an experimental and simulation study10.1016/j.jcrysgro.2014.02.010 ↗
6. The current trends of Mg alloys in biomedical applications—a review10.1002/jbm.b.34290 ↗
7. Magnesium and its alloys as orthopedic biomaterials: a review10.1016/j.biomaterials.2005.10.003 ↗
8. Recent advances on the development of magnesium alloys for biodegradable implants10.1016/j.actbio.2014.07.005 ↗
9. Silicon
10. Silicon: the evolution of its use in biomaterials10.1016/j.actbio.2014.09.025 ↗
11. The nutritional essentiality of silicon10.1111/j.1753-4887.1982.tb05307.x ↗
12. Update on the possible nutritional importance of silicon10.1016/j.jtemb.2014.06.024 ↗
13. Patnaik · 2002
14. Quantitative analysis of interstitial Mg in Mg2Si studied by single crystal X-ray diffraction10.1016/j.jallcom.2014.07.137 ↗
15. A thermodynamic analysis of the Mg-Si system10.1361/105497100770339914 ↗
16. Phase equilibria and thermodynamics of the Mg-Si-Li system and remodeling of the Mg-Si system10.1007/s11669-004-0007-y ↗
17. 2010
18. Tensile strength , ductility and fracture of magnesium-silicon alloys10.1007/BF00357861 ↗
19. Combined ab initio, experimental, and CALPHAD approach for an improved thermodynamic evaluation of the Mg-Si system
20. Microstructural formation in a hypereutectic Mg-Si alloy10.1016/j.matchar.2005.07.009 ↗
21. Effect of Zn on the microstructure and mechanical properties of Mg – Si alloy10.1016/j.msea.2010.01.074 ↗
22. Garcia · 2007
23. Biodegradable metals10.1016/j.mser.2014.01.001 ↗
24. In vitro corrosion and biocompatibility of binary magnesium alloys10.1016/j.biomaterials.2008.10.021 ↗
25. Microstructures, corrosion and mechanical properties of Mg – Si alloys as biodegradable implant materials
26. Low frequency damping capacities and mechanical properties of Mg-Si alloys10.1016/j.msea.2006.10.099 ↗
27. Microstructure, mechanical properties and bio-corrosion properties of Mg-Si(-Ca, Zn) alloy for biomedical application10.1016/j.actbio.2009.11.024 ↗
28. Mechanical behavior of as-cast and extruded Mg-Si-Ni-Ca magnesium alloys10.1007/s11665-020-05229-3 ↗
29. Effects of Si content and Ca addition on thermal conductivity of As-Cast Mg-Si alloys10.3390/ma11122376 ↗
30. Effects of Si content and Ca modification on microstructure and thermal expansion property of Mg–Si alloys10.1016/j.matchemphys.2020.123260 ↗
31. Cashion · 1999
32. Samuels · 2003
33. 1999
34. Directional solidification of aluminium-copper alloys10.1016/S0921-5093(01)01649-5 ↗
35. Effect of silicon content on microstructure, mechanical and electrical properties of the directionally solidified Al–based quaternary alloys10.1016/j.jallcom.2016.10.010 ↗
36. 2021 · 30
37. Characterization of the Al-3wt.%Si alloy in unsteady-state horizontal directional solidification10.1590/S1516-14392013005000072 ↗
38. Growth orientations and morphologies of α-Mg dendrites in Mg-Zn alloys10.1016/j.scriptamat.2012.07.031 ↗
39. Dendritic evolution during coarsening of Mg-Zn alloys via 4D synchrotron tomography10.1016/j.actamat.2016.10.022 ↗
40. Mechanical properties, microstructural features, and correlations with solidification rates of Al–Cu–Si ultrafine eutectic alloys10.1002/adem.202001177 ↗
41. Microstructure and mechanical behavior of Al92Fe3Cr2X3 (X = Ce, Mn, Ti, and V) alloys processed by centrifugal force casting10.1016/j.jmrt.2018.12.022 ↗
42. Tiller · 1958
43. Microstructure of the Sn-Cu6Sn5 fibrous eutectic and its modification by segregation10.1016/S1359-6454(96)00060-2 ↗
44. Effects of solidification kinetics on microstructure formation in binary Sn-Cu solder alloys10.1016/j.actamat.2010.11.032 ↗
45. Thermal analysis during solidification of an Al–Cu eutectic alloy: interrelation of thermal parameters, microstructure and hardness10.1007/s10973-018-07992-x ↗
46. Structure and properties of rapidly solidified magnesium-silicon alloys10.1016/0025-5416(88)90177-2 ↗
47. Interconnection of Zn content, macrosegregation, dendritic growth, nature of intermetallics and hardness in directionally solidified Mg-Zn alloys10.1016/j.jallcom.2015.11.117 ↗