Effects of rolling reduction on microstructural evolution and mechanical properties of W-0.5wt%ZrC alloys
Source abstract
Abstract
Abstract The effects of hot rolling reduction on microstructures and mechanical properties of W-0.5 wt%ZrC (WZC) materials were investigated. Four WZC specimens with rolling reductions of 46%, 69%, 77%, and 96% were prepared by multi-step rolling processes. Metallographic observation, SEM, EBSD, and TEM characterization were conducted to obtain information on the microstructures of the materials. The metallography and EBSD results indicate that W grains were refined to 0.4–0.5 μm in the 96%-rolled WZC01 specimen. In addition, Vickers microhardness measurements at room temperature (RT) and tensile tests at various temperatures from RT to 500 °C were conducted. The results indicate that hardness and strength increase with the increase in rolling reduction. The 96%-rolled 1-mm thick WZC plate exhibits an ultra-high tensile strength of 1450 MPa at 100 °C. The 77%-rolled 6-mm thick WZC bulk material demonstrates both high tensile strength with an ultimate tensile strength of 620 MPa and good ductility with a tensile elongation of 21% at 400 °C, which are superior to those of most reported bulk W materials. The relationships between microstructure, mechanical properties, and rolling reduction were investigated and discussed systematically.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fusion materials and technologies · Nuclear Materials and Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. Irradiation effect on deuterium behaviour in low-dose HFIR neutron-irradiated tungsten10.1088/0029-5515/55/1/013008 ↗
2. Assessment of tungsten for use in the ITER plasma facing components10.1016/S0022-3115(98)00285-2 ↗
3. Materials research for fusion10.1038/nphys3735 ↗
4. Development of a helium-cooled divertor concept: design-related requirements on materials and fabrication technology10.1016/j.jnucmat.2004.04.137 ↗
5. Development of nanostructured tungsten based materials resistant to recrystallization and/or radiation induced embrittlement10.2320/matertrans.MG201209 ↗
6. Development of a helium-cooled divertor: material choice and technological studies10.1016/j.jnucmat.2007.04.027 ↗
7. Recent progress in R&D on tungsten alloys for divertor structural and plasma facing materials10.1016/j.jnucmat.2013.02.074 ↗
8. Surface damage evolution during transient thermal shock of W-2%vol Y2O3 composite material in different surfaces10.1016/j.fusengdes.2019.01.010 ↗
9. The thermal stability of dispersion-strengthened tungsten as plasma-facing materials: a short review10.1007/s42864-019-00022-9 ↗
10. High thermal shock resistance of the hot rolled and swaged bulk W-ZrC alloys10.1016/j.jnucmat.2015.10.052 ↗
11. Fracture strength and microstructure of ODS tungsten alloys10.1016/j.ijrmhm.2010.05.009 ↗
12. Mechanical properties and microstructures of W-TiC and W-Y2O3 alloys fabricated by hot-pressing sintering10.1016/j.msea.2021.141496 ↗
13. Recent progresses on designing and manufacturing of bulk refractory alloys with high performances based on controlling interfaces10.1016/j.jmst.2020.02.046 ↗
14. Mechanical properties and thermal shock resistance of tungsten alloys strengthened by laser fragmentation-processed zirconium carbide nanoparticles10.1007/s42864-020-00071-5 ↗
15. Fabrication of high temperature oxides dispersion strengthened tungsten composites by spark plasma sintering process10.1016/j.ijrmhm.2009.03.003 ↗
16. The effect of yttrium oxide on the sintering behavior and hardness of tungsten10.1007/BF03027538 ↗
17. Mechanical properties of Y2O3-doped W-Ti alloys10.1016/j.jnucmat.2010.07.016 ↗
18. Microstructure and mechanical properties of a W-2wt.%Y2O3 composite produced by sintering and hot forging10.1016/j.jnucmat.2013.01.301 ↗
19. Spark plasma sintering of tungsten- yttrium oxide composites from chemically synthesized nanopowders and microstructural characterization10.1016/j.jnucmat.2011.03.007 ↗
20. W-2wt% Y2O3 composite: microstructure and mechanical properties10.1016/j.msea.2012.01.011 ↗
21. Mechanical properties and thermal shock performance of W-Y2O3 composite prepared by high-energy-rate forging10.1088/1402-4896/aa8f2d ↗
22. Effect of high temperature swaging and annealing on the mechanical properties and thermal conductivity of W-Y2O310.1016/j.jnucmat.2015.04.050 ↗
23. Nanostructured yttria dispersion strengthened tungsten synthesized by sol-gel method10.1016/j.jallcom.2015.10.059 ↗
24. Thermal shock behavior of fine grained W-Y2O3materials fabricated via two different manufacturing technologies10.1016/j.jnucmat.2015.12.042 ↗
25. Development of ultra- fine grained W- (0.25- 0.8)wt% TiC and its superior resistance to neutron and 3 MeV He-ion irradiations10.1016/j.jnucmat.2008.02.055 ↗
26. Development of nanostructured tungsten based materials resistant to recrystallization and/or radiation induced embrittlement10.2320/matertrans.MG201209 ↗
27. Current status of nanostructured tungsten- based materials development
28. Development of toughened, fine grained, recrystallized W-1.1%tic10.4028/www.scientific.net/MSF.1024.103 ↗
29. Microstructures, mechanical properties and deuterium blistering behavior of chemically prepared W–TiC alloys10.1007/s10894-017-0124-3 ↗
30. Effects of TiC content on microstructure, mechanical properties, and thermal conductivity of W-TiC alloys fabricated by a wet-chemical method10.1016/j.fusengdes.2017.07.026 ↗
31. The superior thermal stability and tensile properties of hot rolled W-HfC alloys10.1016/j.ijrmhm.2019.02.018 ↗
32. Microstructure and mechanical properties of nano-size zirconium carbide dispersion strengthened tungsten alloys fabricated by spark plasma sintering method10.1088/1009-0630/17/12/15 ↗
33. Extraordinary high ductility/strength of the interface designed bulk W-ZrC alloy plate at relatively low temperature10.1038/srep16014 ↗
34. Grain growth behavior and mechanical properties of zirconium micro-alloyed and nano-size zirconium carbide dispersion strengthened tungsten alloys10.1016/j.ijrmhm.2015.03.019 ↗
35. Mechanical properties and thermal stability of pure W and W-0.5wt%ZrC alloy manufactured with the same technology10.1016/j.msea.2017.12.112 ↗
36. Effects of swaging and annealing on the microstructure and mechanical properties of ZrC dispersion-strengthened tungsten10.1016/j.ijrmhm.2018.05.018 ↗
37. High thermal shock resistance of the hot rolled and swaged bulk W-ZrC alloys10.1016/j.jnucmat.2015.10.052 ↗
38. Recrystallization and thermal shock fatigue resistance of nanoscale ZrC dispersion strengthened W alloys as plasma-facing components in fusion devices10.1016/j.jnucmat.2017.09.022 ↗
39. Recent progress on the R&D of W-ZrC alloys for plasma facing components in fusion devices10.1016/j.nme.2018.07.002 ↗
40. Plastic deformation in advanced tungsten-based alloys for fusion applications studied by mechanical testing and TEM10.1016/j.ijrmhm.2020.105409 ↗
41. European materials development: results and perspective10.1016/j.fusengdes.2019.02.063 ↗
42. Preparation of pure tungsten via various rolling methods and their influence on macro-texture and mechanical properties10.1016/j.matdes.2017.04.021 ↗
43. Microstructure evolution of hot-rolled pure and doped tungsten under various rolling reductions10.1016/j.jnucmat.2020.152074 ↗
44. Hot ductility behavior of AD730™ nickel-base superalloy10.1016/j.msea.2019.138391 ↗
45. Microstructure and tensile properties of tungsten at elevated temperatures10.1016/j.jnucmat.2015.09.057 ↗
46. Effect of hot rolling and annealing on the mechanical properties and thermal conductivity of W-0.5 wt.% TaC alloys10.1016/j.ijrmhm.2015.12.004 ↗
47. Controlling factors for the brittle-to-ductile transition in tungsten single crystals10.1126/science.282.5392.1293 ↗
48. etc., Recent progress in research on tungsten materials for nuclear fusion applications in Europe10.1016/j.jnucmat.2012.08.018 ↗